journal article·2019-01-01

Effect of Major Intermetallic Particles on Localized Corrosion of AA2060-T8

Yakun Zhu, G.S. Frankel

Corrosion· Volume 75· Issue 1
Publisher page

Abstract

The localized corrosion of AA2060-T8 and the role of two major types of intermetallic particles (IMPs), heterogeneous Al-Cu-Fe-Mn and S-phase (Al2CuMg), were studied using scanning Kelvin probe force microscopy (SKPFM) and scanning electron microscopy (SEM) coupled with energy dispersive spectroscopy (EDS). Topography and Volta potential maps were collected to determine the corrosion morphology around, and the relative nobility of, the same IMPs before and after sequential exposure to NaCl solution. Chemical compositions and the correlation to SKPFM maps of the representative IMPs and corroded structure were identified using SEM-EDS. These results provide insight into the electrochemical behavior and corrosion mechanism of the Al-Cu-Fe-Mn and S-phase IMPs and associated effects on localized corrosion of AA2060-T8 compared to the legacy AA2024-T3.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

*Fontana Corrosion Center, The Ohio State University Columbus, Ohio 43210.

References (55)

Show source-provided references
1. Liddicoat · Nat. Commun. · 2010 · 1 · 6310.1038/ncomms1062 ↗
2. Hirsch · Acta Mater. · 2013 · 61 · 81810.1016/j.actamat.2012.10.044 ↗
3. “Aerostructural Design and Its Application to Aluminum–Lithium Alloys,”10.1016/B978-0-12-401698-9.00002-1 ↗
4. Wang · Int. Mater. Rev. · 2005 · 50 · 19310.1179/174328005X14357 ↗
5. Häusler · Materials · 2017 · 10 · 11710.3390/ma10020117 ↗
6. Lin · Mater. Sci. Eng. A · 2013 · 565 · 42010.1016/j.msea.2012.12.058 ↗
7. Birbilis · J. Electrochem. Soc. · 2005 · 152 · B14010.1149/1.1869984 ↗
8. Birbilis · J. Electrochem. Soc. · 2008 · 155 · C11710.1149/1.2829897 ↗
9. Ma · Mater. Chem. Phys. · 2015 · 161 · 20110.1016/j.matchemphys.2015.05.037 ↗
10. Ma · Corros. Sci. · 2016 · 107 · 4110.1016/j.corsci.2016.02.018 ↗
11. Foley · Corrosion · 1986 · 42 · 27710.5006/1.3584905 ↗
12. Buchheit · J. Electrochem. Soc. · 1995 · 142 · 399410.1149/1.2048447 ↗
13. Frankel · Mater. Today · 2008 · 11 · 3810.1016/S1369-7021(08)70206-2 ↗
14. Zhang · Corrosion · 2017 · 73 · 98810.5006/2418 ↗
15. Buchheit · Corrosion · 1990 · 46 · 61010.5006/1.3585156 ↗
16. Buchheit · J. Electrochem. Soc. · 1997 · 144 · 262110.1149/1.1837874 ↗
17. Schmutz · J. Electrochem. Soc. · 1998 · 145 · 228510.1149/1.1838633 ↗
18. Schmutz · J. Electrochem. Soc. · 1998 · 145 · 229510.1149/1.1838634 ↗
19. Hughes Anthony · 2015 · 1
20. Vukmirovic · J. Electrochem. Soc. · 2002 · 149 · B42810.1149/1.1498258 ↗
21. Lacroix · J. Electrochem. Soc. · 2008 · 155 · C13110.1149/1.2833315 ↗
22. Zhu · Metall. Mater. Trans. A · 2012 · 43 · 493310.1007/s11661-012-1354-7 ↗
23. Yi · J. Alloys Compd. · 2018 · 740 · 46110.1016/j.jallcom.2017.12.329 ↗
24. Boag · Corros. Sci. · 2009 · 51 · 156510.1016/j.corsci.2009.05.001 ↗
25. Lacroix · J.Electrochem. Soc. · 2008 · 155 · C810.1149/1.2799089 ↗
26. Muster · J. Electrochem. Soc. · 2006 · 153 · B47410.1149/1.2349356 ↗
27. Blanc · Corros. Sci. · 1997 · 39 · 49510.1016/S0010-938X(97)86099-4 ↗
28. Ilevbare · Corrosion · 2001 · 57 · 48010.5006/1.3290371 ↗
29. Ilevbare · J. Electrochem. Soc. · 2001 · 148 · B19610.1149/1.1360206 ↗
30. Malladi · Corros. Sci. · 2013 · 69 · 22110.1016/j.corsci.2012.12.006 ↗
31. Parvizi · Corros. Sci. · 2017 · 116 · 9810.1016/j.corsci.2016.12.006 ↗
32. Malladi · Chem. Commun. · 2013 · 49 · 1085910.1039/c3cc46673f ↗
33. Decreus · Acta Mater. · 2013 · 61 · 220710.1016/j.actamat.2012.12.041 ↗
34. Dinsdale · Calphad · 1991 · 15 · 31710.1016/0364-5916(91)90030-N ↗
35. Gable · Calphad · 2008 · 32 · 25610.1016/j.calphad.2007.08.003 ↗
36. Gayle · Scr. Metall. Mater. · 1990 · 24 · 7910.1016/0956-716X(90)90570-7 ↗
37. Kertz · Metall. Mater. Trans. A · 2001 · 32 · 256110.1007/s11661-001-0046-5 ↗
38. Liu · Mater. Corros. · 2017 · 68 · 6510.1002/maco.201609090 ↗
39. “Deconstructing DB ASTM G85-A2 Testing Environment with In-Situ Measurements,”
40. “International Alloy Designations and Chemical Composition Limits for Wrought Aluminum and Wrought Aluminum Alloys
41. Boag · Corros. Sci · 2011 · 53 · 1710.1016/j.corsci.2010.09.009 ↗
42. Guillaumin · Corros. Sci · 1998 · 41 · 42110.1016/S0010-938X(98)00116-4 ↗
43. Ilevbare · J. Electrochem. Soc. · 2004 · 151 · B45310.1149/1.1764780 ↗
44. Schneider · J. Electrochem. Soc. · 2004 · 151 · B46510.1149/1.1764781 ↗
45. Liu · Acta Mater. · 2007 · 55 · 35310.1016/j.actamat.2006.08.025 ↗
46. Yi · Metall. Mater. Trans. A · 2014 · 45 · 485110.1007/s11661-014-2473-0 ↗
47. Yi · Corrosion · 2016 · 72 · 17710.5006/1918 ↗
48. “Corrosion and Potentiostatic Polarization of an Al-Cu-Li Alloy Under Tensile Stress,”
49. Liu · J. Mater. Sci. · 2012 · 47 · 429010.1007/s10853-012-6279-4 ↗
50. Ma · Corros. Sci. · 2013 · 66 · 29210.1016/j.corsci.2012.09.032 ↗
51. Dimitrov · J. Electrochem. Soc. · 2000 · 147 · 328310.1149/1.1393896 ↗
52. “High Strength Al-Alloys: Microstructure, Corrosion and Principles of Protection,”
53. Mokaddem · Electrochim. Acta · 2010 · 55 · 377910.1016/j.electacta.2010.01.079 ↗
54. Danaie · Corros. Sci. · 2014 · 83 · 29910.1016/j.corsci.2014.02.030 ↗
55. Kim · J. Appl. Electrochem. · 2013 · 43 · 50710.1007/s10800-013-0534-5 ↗