Corrosion Behavior of Binary Titanium Aluminide Intermetallics
Source abstract
Abstract
The corrosion behavior of arc-melted binary titanium aluminide intermetallics TiAl, Ti3Al, and TiAl3 in aqueous sodium sulfate (Na2SO4) and sodium chloride (NaCl) solutions was measured and compared to that of pure Ti and Al. Effects of electrolyte composition (e.g., sulfate [0.25 M SO42-], chloride [0.1 to 1.0 M Cl-], and pH [3 to 10]) were examined. Anodic polarization of titanium aluminides in aqueous SO42− solutions was similar (showing passive behavior), but no pitting or pitting potential (Epit) was observed. In aqueous NaCl, however, titanium aluminides were susceptible to pitting, and Epit decreased with increasing Al content (i.e., Ti3Al had the highest Epit and, therefore, a greater resistance to pitting, followed by TiAl and TiAl3). For TiAl, Epit was slightly dependent upon pH or Cl− concentration. Pit morphology and Epit values were quite different for TiAl compared to Ti3Al. TiAl showed numerous small pits, whereas Ti3Al exhibited fewer but larger and deeper pits. The larger pit density for TiAl was associated with Al-rich interdendrite regions. One interesting feature of the anodic polarization curves for Ti3Al was a small anodic peak frequently observed at ~ 1.4 VSCE to 1.8 VSCE. Results suggested this peak was associated with pit initiation, since pitting initiated concurrently with the peak or immediately afterward.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Quasicrystal Structures and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
*Department of Metallurgical and Materials Engineering, University of Alabama, Tuscaloosa, AL, 35487-0202.
References (30)
Show source-provided references
1. Intermetallic Alloys Based on Gamma Titanium Aluminide10.1007/BF03220267 ↗
2. Ordered Intermetallic Alloys, Part II: Silicides, Trialuminides, and Others10.1007/BF03223307 ↗
3. Ti Aluminide Foils for Metal-Matrix Composites
4. Ordered Intermetallic Alloys, Part III: Gamma-Titanium Aluminides10.1007/BF03220745 ↗
5. Producing Titanium Aluminide Foils from Plasma-Sprayed Preforms10.1007/BF03222383 ↗
6. The Mechanical Properties of Titanium Aluminides Near Ti-25% Al-25% Nb
7. Oxidation Characteristics of Ti-33% Al-6% Nb-1.4% Ta
8. Thin Coatings for Protecting Titanium Aluminides in High-Temperature Oxidation Environments
9. Oxidation Behavior of Gamma-Titanium Aluminide Alloys
10. Zhang · Scrip. Metall. · 1992 · 27 · 1,36110.1016/0956-716X(92)90084-R ↗
11. Environmental Effects in Titanium Aluminide Alloys
12. Takasugi · J. Mater. Res. · 1992 · 7 · 15910.1557/JMR.1992.2739 ↗
13. Recent Advances in Gamma-Titanium Aluminide Alloys
14. Koch · MP · 1993 · 32 · 54
15. A Review: Pitting Attack of Titanium Alloys
16. Q. Gan , “Anodic Behavior of Gamma-Titanium Aluminide and Its Pitting Corrosion in Aqueous Solution” (Master's thesis, University of Alabama, 1995).
17. Scully · 1990 · 208
18. Corrosion Behavior of Advanced Intermetallic Aluminides
19. Francois · Thin Solid Films · 1993 · 223 · 22310.1016/0040-6090(93)90525-T ↗
20. De Becdelievre · Electrochim. Acta · 1988 · 33 · 1,06710.1016/0013-4686(88)80196-8 ↗
21. Casillas · J. Electrochem. Soc. · 1993 · 140 · L14210.1149/1.2220897 ↗
22. Armstrong · Surf. Sci. · 1977 · 67 · 45110.1016/0039-6028(77)90007-3 ↗
23. The Passivity of Metals and Passivating Films
24. The Breakdown of Passivity on Titanium, Zirconium, and Tantalum in Halide Media
25. Hall · J. Phys. Chem. · 1953 · 57 · 26210.1021/j150504a002 ↗
26. J.C. Nelson , “Stress Generation in Thin Anodic Films on Titanium, Aluminum, and Nickel” (Ph.D. thesis, University of Minnesota, 1990), p. 29.
27. Leckie · Corrosion · 1967 · 23 · 18710.5006/0010-9312-23.7.187 ↗
28. Titanium Dioxide (TiO2) and Strontium Titanate (SrTiO3)
29. Möllers · J. Electrochem. Soc. · 1974 · 121 · 1,16010.1149/1.2402004 ↗
30. Szklarska-Smialowska · 1986 · 342