journal article·1999-07-01

Role of Microstructures on Stress Corrosion Cracking of Pipeline Steels in Carbonate-Bicarbonate Solution

H. Asahi, T. Kushida, M. Kimura, H. Fukai, S. Okano

Corrosion· Volume 55· Issue 7
Publisher page

Abstract

Stress corrosion cracking (SCC) on the external surface of pipelines contributes to the major failure of pipelines. The great majority of SCC is intergranular and occurs in a carbonate-bicarbonate environment. Metallurgical factors affecting SCC are still vague and therefore have been studied. Uniform microstructures, not mixed structures, are favorable for suppressing SCC. Low-C steels produced in a process such as thermomechanical-controlled processing are less susceptible to SCC. The presence of locally soft micro-structures decreases resistance to SCC (mixed structure and decarburized structure). However, SCC resistance is high on hard layers, like grit-blasted surfaces.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

*Nippon Steel Corporation, Steel Research Laboratories, 20-1, Shintomi, Futtsu-shi, Chiba-ken, Japan 293.

**Sumitomo Metal Industries, Ltd., Corporate Research and Development Laboratories, 1-8, Fuso-cho, Amagasaki-shi, Hyogo-ken, Japan 660.

***Kawasaki Steel Corporation, Technical Research Laboratories, 1-1, Kawasaki-cho, Handa-shi, Aichi-ken, Japan 475.

****NKK Corporation, Materials and Processing Research Center, 1, Kokan-cho, Fukuyama-shi, Hiroshima-ken, Japan 721.

*****Kobe Steel, Ltd., Kakogawa Works, 1, Kanazawa-cho, Kakogawa-shi, Hyogo-ken, Japan 675-0.

References (20)

Show source-provided references
1. Natural Gas Pipeline Stress Corrosion Cracking: A Failure Analysis
2. Gas Pipeline Failures: Australian Experience10.1179/000705985798272786 ↗
3. Corrosion Cracking of Gas-Carrying Pipelines — Does Cathodic Protection Contribute?
4. Major Field Study Compares Pipeline Stress Corrosion Cracking with Coatings
5. Pipeline Failure Update — Conclusion: Stress Corrosion Cracking, Bacteria top Items in Pipe Service Failures
6. Catastrophes of Large Diameter Pipelines: The Role of Hydrogen Fields
7. Fracture Propagation Assessment of 34th Gas Line
8. Stress Corrosion Cracking of C-Mn Steels in Environments Containing Carbon Dioxide
9. Stress Corrosion Cracking of Carbon Steel in Carbonate Solutions10.5006/0010-9312-28.8.313 ↗
10. Stress Corrosion Cracking of Pipelines — Its Control or Prevention
11. Effects of Alloying Additions to Ferritic Steels Upon Stress Corrosion Cracking Resistance10.5006/1.3577554 ↗
12. On the External Stress Corrosion Cracking of Line Pipe Steels
13. SCC Threshold Stress in Line Pipe Steels
14. Study on Material Factors that Influence the Susceptibility of Line Pipe Steels to External Stress Corrosion Cracking10.2355/tetsutohagane1955.69.11_1471 ↗
15. J.A. Beavers, R.N. Parkins, G.H. Koch, W.E. Berry, “Test Method for Defining Susceptibility of Line Pipe Steels to Stress Corrosion Cracking,”. AGA NG-18 report, paper no. 146 (Arlington, VA: AGA, 1985).
16. Surface Roughness — Definitions and Designation
17. On the External Stress Corrosion Cracking of Line Pipe Steels
18. Stress Corrosion Cracking Characteristics of a Range of Pipeline Steels in Carbonate-Bicarbonate Solutions10.5006/1.3316023 ↗
19. Some Effects of Surface Condition on the Stress Corrosion Cracking on Line Pipe Steel
20. An Overview — Prevention and Control of Stress Corrosion Cracking