Abstract
When carbon steel corrodes in anaerobic carbonated water, and the steel surface area to liquid volume is high, the concentration of ferrous and bicarbonate ions increases rapidly even though the corrosion rate is low. Such solutions with high bicarbonate concentration and a near neutral pH are believed to induce stress corrosion cracking of high-strength carbon steels. This work was conducted to investigate the solid precipitation in siderite supersaturated solutions. It was also an objective to measure the corrosion rate of high-strength carbon steel in solutions with high bicarbonate concentration at pH close to neutral. Preloading the solutions with ferrous ions and bicarbonate made it possible to measure desupersaturation and corrosion rate as function of time. The initial siderite supersaturation was more than 1,000 in the desupersaturation experiments. Despite this, the nucleation and growth of siderite was so slow that the solutions remained supersaturated for 100 h to 500 h at 10°C to 25°C. The ferrous ion concentration decreased from 1,200 mg/kg to 100 mg/kg in less than 24 h at 40°C, but did not reach equilibrium within 250 h. The precipitate was siderite at 5°C to 25°C. At 40°C, the solid was a mixture of siderite and chuckanovite in low salinity water and siderite with dissolved Ca2+ in artificial seawater. The corrosion rate of carbon steel at pH 6.7 to 7.2 at 25°C decreased to less than 0.01 mm/y in 5 h. Siderite precipitated and grew to a thin protective layer at the steel surface. Even though the solutions were highly supersaturated with respect to siderite throughout the experiments, the carbonate layer at the steel surface did not grow to more 5 μm thickness during 250 h to 400 h. The investigated steels were armor wires for flexible pipes. They have an oxide layer at the surface which is an inherent result of the manufacturing process. The presence of these oxides did not impede the formation of protective siderite layer.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
*LabCorr/PEMM/COPPE, Federal University of Rio de Janeiro-UFRJ, P.O. box 68505, Zip Code 21941-599, Rio de Janeiro/RJ, Brazil.
**Institute for Energy Technology, P.O. Box 40, NO-2027 Kjeller, Norway.
References (58)
Show source-provided references
1. Remita · Electrochim. Acta · 2007 · 52 · 771510.1016/j.electacta.2006.12.088 ↗
2. Corrosion Rates of Carbon Steel in Confined Environments10.5006/C2012-01495 ↗
3. Corrosion Testing of Steel Armour Wires in Flexible Pipes–A Parametric Study10.5006/C2015-05829 ↗
4. Experimental and Theoretical Investigation of the Uniform Corrosion in the Annulus of Offshore Flexible Pipelines10.5006/C2008-08538 ↗
5. Nešić · Corros. Sci. · 2007 · 49 · 430810.1016/j.corsci.2007.06.006 ↗
6. Remita · J. Electrochem. Soc. · 2008 · 155 · C4110.1149/1.2801349 ↗
7. Corrosion of Mild Steel in an Aqueous CO2 Environment–Basic Electrochemical Mechanisms Revisited10.5006/C2015-05671 ↗
8. Kahyarian · J. Nat. Gas Sci. Eng. · 2016 · 29 · 53010.1016/j.jngse.2015.12.052 ↗
9. Ekawati · Corrosion · 2017 · 73 · 115710.5006/2143 ↗
10. National Energy Board Canada, “Public Inquiry Concerning Stress Corrosion Cracking on Canadian Oil and Gas Pipelines” National Energy Board Canada, November1996, available athttp://publications.gc.ca/site/eng/418383/publication.html.
11. Chen · Corrosion · 2016 · 72 · 96210.5006/1967 ↗
12. Recommended Practices for Managing Near-Neutral pH Stress Corrosion Cracking
13. Effects of O2 and CO2 of Near-Neutral pH Stress Corrosion Crack Propagation10.5006/C2000-00356 ↗
14. Chen · Corrosion · 2002 · 58 · 26710.5006/1.3279878 ↗
15. Gu · Corrosion · 1999 · 55 · 31210.5006/1.3283993 ↗
16. Near-Neutral pH SCC in Pipelines: Effects of Pressure Fluctuations on Crack Propagation10.5006/C1998-98257 ↗
17. On the Beneficial Influence of a Very Low Supply of H2S on the Hydrogen Embrittlement Resistance of Carbon Steel Wires in Flexible Pipe Annulus10.4043/19950-MS ↗
18. New Anti H2S Layer for Flexible Pipes10.4043/21371-MS ↗
19. Sun · Corros. Sci. · 2009 · 51 · 127310.1016/j.corsci.2009.03.009 ↗
20. Berntsen · Corrosion · 2013 · 69 · 60110.5006/0553 ↗
21. Hassan SK · Corros. Sci. · 2017 · 126 · 2610.1016/j.corsci.2017.05.026 ↗
22. Sun · Corros. Sci. · 2009 · 51 · 127310.1016/j.corsci.2009.03.009 ↗
23. Burkle · Electrochim. Acta · 2017 · 255 · 12710.1016/j.electacta.2017.09.138 ↗
24. Sun · Corrosion · 2008 · 64 · 33410.5006/1.3278477 ↗
25. Braum · Talanta · 1991 · 38 · 20510.1016/0039-9140(91)80131-I ↗
26. Mechanism of Protective Layer Formation During CO2 Corrosion of Carbon Steel
27. Ferreira · Quim. Nova · 2016 · 39 · 1027
28. López · Appl. Surf. Sci. · 2007 · 207 · 6910.1016/S0169-4332(02)01218-7 ↗
29. Crolet · Corros. Sci. · 1998 · 54 · 19410.5006/1.3284844 ↗
30. Dugstad · Corrosion · 2001 · 57 · 36910.5006/1.3290361 ↗
31. Effect of Environmental Factor and Microstructure on Morphology of Corrosion Products in CO2 Environments10.5006/C1999-99013 ↗
32. How Ferrous Carbonate Kinetics Impacts Oilfield Corrosion10.2118/21025-MS ↗
33. Liu · Appl. Surf. Sci. · 2015 · 351 · 61010.1016/j.apsusc.2015.06.006 ↗
34. Mora-Mendoza · Corros. Sci. · 2002 · 44 · 122310.1016/S0010-938X(01)00141-X ↗
35. Stress Corrosion Cracking of Pipeline Steel in Near-Neutral pH Environments10.5006/C2006-06175 ↗
36. Recent Developments in Characterizing the Mechanism of Near Neutral pH SCC10.5006/C2005-05161 ↗
37. Bueno · Eng. Fail. Anal. · 2014 · 36 · 42310.1016/j.engfailanal.2013.11.012 ↗
38. Parkins · Corros. Sci. · 1997 · 39 · 15910.1016/S0010-938X(96)00116-3 ↗
39. Standard Practice for the Preparation of Substitute Ocean Water
40. Jensen · Appl. Geochem. · 2002 · 17 · 50310.1016/S0883-2927(01)00118-4 ↗
41. Construction and Verification of Pourbaix Diagrams for CO2 Corrosion of Mild Steel Valid up to 250°C10.5006/C2012-01418 ↗
42. De Marco · J. Electrochem. Soc. · 2005 · 152 · B38910.1149/1.2007227 ↗
43. Schlegel · Environ. Sci. Technol. · 2010 · 44 · 150310.1021/es9021987 ↗
44. Pandarinathan · Corros. Sci. · 2014 · 85 · 2610.1016/j.corsci.2014.03.032 ↗
45. Jiang · Earth Planet. Sci. Lett. · 2019 · 506 · 23110.1016/j.epsl.2018.11.010 ↗
46. Bénézeth · Chem. Geol. · 2009 · 265 · 310.1016/j.chemgeo.2009.03.015 ↗
47. Al-Hassan · Corrosion · 1998 · 54 · 48010.5006/1.3284876 ↗
48. Gadala · Metall. Mater. Trans. A · 2015 · 46A · 310410.1007/s11661-015-2891-7 ↗
49. Rogowska · Corros. Eng. Sci. Technol. · 2016 · 51 · 2510.1179/1743278215Y.0000000029 ↗
50. Ingham · Faraday Discuss. · 2015 · 180 · 17110.1039/C4FD00218K ↗
51. Qu · Eur. J. Miner. · 2011 · 23 · 75910.1127/0935-1221/2011/0023-2134 ↗
52. Yu · Chem. Commun. · 2004 · 21 · 241410.1039/b406839d ↗
53. Figueiredo · Cryst. Res. Technol. · 2015 · 50 · 35410.1002/crat.201400420 ↗
54. Xia · Corrosion · 1989 · 45 · 63610.5006/1.3579317 ↗
55. Parkins · Brit. Corros. J. · 1979 · 14 · 510.1179/000705979798276086 ↗
56. Liu · Corros. Sci. · 2012 · 55 · 5410.1016/j.corsci.2011.10.002 ↗
57. Di Liberto · Mater. Sci. · 1997 · 33 · 41110.1007/BF02537540 ↗
58. Bogdanov · AIMS Mater. Sci. · 2019 · 6 · 106510.3934/matersci.2019.6.1065 ↗