Effect of pH and Chloride Contents on Stress Corrosion Cracking of Austenitic Stainless Steels at Room Temperature
Source abstract
Abstract
Constant elongation rate tests and constant load, subcritical crack growth tests were used to investigate the stress corrosion cracking (SCC) susceptibility of metastable (type 301 [UNS(1) S30100]) and stable (type 310S [UNS S30108]) austenitic stainless steels in H2SO4/NaCl aqueous solutions at 25°C. For annealed type 301, at each pH value there was a critical concentration of Cl− ions required to initiate SCC at 25°C. Using the constant extension rate test with notched specimens, the relation between pH and [Cl−] can be expressed as for SCC immunity: pH>6.9log [Cl−]+0.7 By using a sharper, fatigue precrack and a constant load, the critical concentrations of Cl− ions for SCC immunity and active dissolution to occur at 25° can be expressed as: for SCC immunity: pH>5log [Cl−]+3for active dissolution: pH<1.6log [Cl−]+0.3 SCC occurred at intermediate values of pH and [Cl−]. For type 310S, constant extension rate test results were insensitive to the environment, and the constant load test caused SCC to occur only in more acidic solutions than for type 301. The results for type 310S are summarized by: for SCC immunity: pH>3.9[Cl−]−1.7
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
*Chung Shan Institute of Science and Technology, Box 90008-8-3, Lung-Tan, Taiwan, ROC.
**Department of Materials Science and Engineering, University of Illinois, Urbana, IL 61801.
References (20)
Show source-provided references
1. Acello · Corrosion · 1962 · 18 · 28610.5006/0010-9312-18.8.286 ↗
2. Harston · Corrosion · 1969 · 25 · 49310.5006/0010-9312-25.12.493 ↗
3. Bianchi · Corrosion Science · 1973 · 13 · 16510.1016/0010-938X(73)90012-7 ↗
4. Truman · Corrosion Science · 1977 · 17 · 73710.1016/0010-938X(77)90069-5 ↗
5. Takano · Trans. Japan Inst. Metals · 1977 · 18 · 78010.2320/matertrans1960.18.780 ↗
6. Torchio · Corrosion Science · 1980 · 20 · 55510.1016/0010-938X(80)90071-2 ↗
7. Meyburg · Corrosion Science · 1983 · 23 · 94310.1016/0010-938X(83)90022-7 ↗
8. Frignani · Corrosion Science · 1984 · 24 · 91710.1016/0010-938X(84)90112-4 ↗
9. Davies · Corrosion Science · 1984 · 24 · 95310.1016/0010-938X(84)90116-1 ↗
10. Maier · Corrosion Science · 1985 · 25 · 1510.1016/0010-938X(85)90085-X ↗
11. Zucchi · Corrosion Science · 1988 · 28 · 6910.1016/0010-938X(88)90008-X ↗
12. Gragnolino · Corrosion · 1982 · 38 · 40610.5006/1.3577354 ↗
13. Perng · Acta Metallurgica · 1986 · 34 · 177110.1016/0001-6160(86)90123-9 ↗
14. Angel · J. Iron and Steel Inst. · 1954 · 177 · 165
15. Heger · 1966 · 122
16. Buhl · 1979 · 333
17. Hertzberg · 1983 · 291
18. Puiggali · Corrosion Science · 1987 · 17 · 58510.1016/0010-938X(87)90032-1 ↗
19. Stalder · Corrosion · 1977 · 33 · 6710.5006/0010-9312-33.2.67 ↗
20. Nishimura · Corrosion · 1989 · 45 · 30810.5006/1.3577859 ↗