journal article·1990-12

Influence of the high temperature corrosion by different gaseous environments on the bending strength of Silicon carbide materials

R. Förthmann, A. Naoumidis

Materials and Corrosion· Volume 41· Issue 12
Publisher page

Abstract

Abstract Starting from silicon carbide tube and plate materials from industrial production, a series of corrosion tests was performed at temperatures between 1100 and 1400°C in different atmospheres containing water vapour, hydrogen, sulfur dioxide, hydrogen sulfide, and hydrogen chloride. Corrosion layers were characterized concerning their structure and morphology, but main emphasis was given to measurements on the change of the silicon carbide bending strength after gas corrosion. Important results of this work are the very different corrosion behaviour of various silicon carbide materials under the same corrosion conditions depending on stoichiometry, structure, sintering aids, and distribution of free silicon phase, the significant increase in the bending strength of SiCiC tube material with homogeneous silicon phase distribution after corrosion in hot water vapour in the presence of nitrogen, the decrease in bending strength in dry hydrogen/nitrogen atmospheres, the resistance of silicon carbide materials against sulfurous atmospheres at temperatures near 1400°C, and the attack on SiSiC by HCl depending on the HCl concentration and the oxygen partial pressure.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Cohrt H. · 1987 · 137
2. Siliciumcarbid als oxidationsbeständiger Hochtemperaturwerkstoff/Oxidations‐ und Heißkorrosionsverhalten
3. 10.1111/j.1151-2916.1988.tb05793.x10.1111/j.1151-2916.1988.tb05793.x ↗
4. F. CostaOliveira: “Corrosion of silicon nitride in H2S/H2O/H2gas mixtures at 1200–1300°C” Proceed. of the 1stEuropean Ceramic Society Conference Maastricht June19–23 1989.
5. 10.1111/j.1151-2916.1981.tb10297.x10.1111/j.1151-2916.1981.tb10297.x ↗
6. 10.1016/0022-3093(84)90138-810.1016/0022-3093(84)90138-8 ↗
7. 10.3891/acta.chem.scand.18-159610.3891/acta.chem.scand.18-1596 ↗
8. 10.1038/191701a010.1038/191701a0 ↗
9. R.Förthmann E.Gyarmati A.Naoumidis: “Corrosion of silicon carbide ceramics at high temperatures in water vaporcontaining atmospheres” Proceed. VIII Yugoslav‐German Meeting on Material Science and Development “Ceramics and Metals” Brdo pri Kranju May 18–21 1987 / Jül‐Spez‐446 (1988).
10. J.Li P.Eveno A. M.Huntz: “Oxidation of SiC” Werkst. Korros. dieses Heft S.716–725.10.1002/maco.19900411212 ↗