C.V.D. Coating of Alumina Reinforcing Particles to Improve the Wear Resistance of H.S.S. Based Composites

C. Jouanny-Tresy, M. Vardavoulias, M. Jeandin

Publisher page

Abstract

Abstract C.V.D. coating of the reinforcing ceramic particles used in particulate metal matrix composites allows the control of reactivity at the particle/matrix interface. Wear resistant high speed steel-based composites containing uncoated A1203, uncoated TiC and C.V.D. coated A1203 were liquid phase sintered, then characterized using “pin-on-disc” wear testing. TiC or TiN C.V.D. coatings of A1203 were tested to determine die increase in reactivity of the particles with the liquid phases formed during sintering. This resulted in a porosity decrease at the particle/matrix interface in addition to a better ceramic/metal cohesion due to improved wettability. Reactivity and wettability were studied using differential thermal analysis, electron microprobe analysis, transmission electron microscopy, and image analysis. Results from pin-on-disc wear testing illustrated the role of the C.V.D. coating on the wear behavior of the studied materials. Lower wear rates were obtained with the composites containing TiC or TiN-coated Al203. These results showed that there is a relation between wettability of ceramic particles by the metallic phases and wear resistance of the composites.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. 10.1016/0010-4361(76)90234-210.1016/0010-4361(76)90234-2 ↗
2. Friedrich E. · 1992 · 3 · 85
3. 10.4028/www.scientific.net/KEM.56-57.16510.4028/www.scientific.net/KEM.56-57.165 ↗
4. Y.H. Teng and J.D. Boyd ,Proceedings of the Conference on Fabrication of Particulate Reinforced Metal Composites, J. Masounave and F.G. Hamel , eds. ASM , pp. 125 – 134 , ( 1990 ) .
5. 10.1016/0040-6090(77)90107-910.1016/0040-6090(77)90107-9 ↗
6. Vincent , H. , C. Vincent , J. L. Ponthenier , H. Mourichoux , and J. Bouix ,Proceedings of ECCM3, A.R. Bunsell et al., eds. Bordeaux, France , pp. 257 – 264 , ( 1989 ).10.1007/978-94-009-1123-9_35 ↗
7. Yang M.Y. · Advanced Ceramic Materials · 1988 · 3 · 34110.1111/j.1551-2916.1988.tb00231.x ↗
8. Kramer B. M. · United States Patent · 1988
9. Coleman D. S. · Powder Metallurgy · 1989 · 32 · 3510.1179/pom.1989.32.1.35 ↗
10. 10.1007/BF0117403210.1007/BF01174032 ↗
11. 10.1016/0257-8972(91)90060-A10.1016/0257-8972(91)90060-A ↗
12. Stiglich Jr J. J. · 1991 · 37
13. Thümmler F. · Powder Metallurgy International · 1991 · 23 · 285
14. Eustathopoulos N. · Materials Science and Engineering · 1991 · 135 · 8310.1016/0921-5093(91)90541-T ↗
15. Jouanny‐Tresy , C. , P. Von Rosentiel, M. Jeandin , and M. Durand ,Proceedings of EUROMAT '91, Institute of Metals Publication, Vol. 2 , Cambridge , U.K. , p. 265 , ( 1991 ).
16. Hoyle G. · 1988
17. Bolton J. · Powder Metallurgy · 1990 · 33 · 2610.1179/pom.1990.33.2.126 ↗
18. 10.1007/BF0114321410.1007/BF01143214 ↗
19. Michorius M. M. · European Patent · 1991
20. 10.1063/1.218594710.1063/1.2185947 ↗
21. 10.1016/0021-9797(82)90319-810.1016/0021-9797(82)90319-8 ↗
22. Marmur A. · 1992 · 39 · 13
23. 10.1007/BF0266668810.1007/BF02666688 ↗
24. 10.1007/BF0265393210.1007/BF02653932 ↗
25. 10.1007/BF0264788810.1007/BF02647888 ↗
26. 10.1007/BF0036503510.1007/BF00365035 ↗
27. 10.1016/0956-716X(93)90513-R10.1016/0956-716X(93)90513-R ↗
28. Martins , I. M. , M. M. Oliveira , and H. Carvalhinhos ,Proceedings of PM' 92, J.M. Capus and R.M. German , eds. MPIF and APMI, San Francisco , Vol. 6 , pp. 213 – 222 , ( 1992 ).
29. Dupré A.Théorie mécanique de la chaleur, Gauthier Villars, Paris , France , 1869 , p. 369 .
30. 10.1016/0043-1648(93)90329-K10.1016/0043-1648(93)90329-K ↗