journal article·2013-07-09

Enhanced Corrosion Resistance and Micro-Hardness of Titanium with Electroless Deposition Ni-W-Cr-P Coating

Long Che, Min Xiao, Hang Xu, Bin Wang, Yong Jin

Publisher page

Abstract

In the present study, Ni-W-Cr-P quaternary alloy coatings were prepared on titanium-based alloys by electroless deposition. The morphology, crystal structure, microhardness, and corrosion resistance of samples were studied by scanning electron microscope (SEM), X-ray diffractometer (XRD), microhardness tester, and electrochemical analyzer. The results show that the microstructure of these alloy films changes with the increase of annealing temperature. As-deposited alloy layers belong to nickel-based mischcrystal structure, and its crystallinity was enhanced to 200°C and 300°C, gradually; the new phase Ni3P began to appear at 400°C, completely crystallized at 600°C; Cr1.12Ni2.88 and Ni3Ti phases were present at 700°C; Ni and Ni3P phases were totally decomposed at 800°C, and Cr4Ni15W, Cr2Ni3, Ni17W3, Cr, Cr3P, and Ni2P generated. Because of the different structures after annealing, microhardness and corrosion resistance of the alloy coatings possess a relevant change. The Ni–W–Cr–P alloy coatings heated at 600°C exhibit better microhardness and corrosion resistance than those of samples at other annealing temperature. The related mechanisms of those results were also discussed, briefly.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · High Entropy Alloys Studies · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Palumbo G. · Materials & Design · 2012 · 40 · 4310.1016/j.matdes.2012.03.031 ↗
2. 10.1080/10426914.2011.58549910.1080/10426914.2011.585499 ↗
3. Kurt B. · Materials Science and Technology · 2009 · 25 · 55610.1179/174328408X311107 ↗
4. 10.1016/S1359-6462(01)01041-710.1016/S1359-6462(01)01041-7 ↗
5. Ozyurek D. · High Temperature Materials and Processes · 2011 · 30 · 17510.1515/htmp.2011.026 ↗
6. Byeli A.V. · Journal of the Mechanical Behavior of Biomedical Materials · 2012 · 6 · 8910.1016/j.jmbbm.2011.05.034 ↗
7. 10.1081/AMP-20004160210.1081/AMP-200041602 ↗
8. 10.1080/1539445090299657710.1080/15394450902996577 ↗
9. 10.1016/0143-7496(95)91627-I10.1016/0143-7496(95)91627-I ↗
10. Yang L.H. · Journal of Alloys and Compounds · 2009 · 467 · 56210.1016/j.jallcom.2007.12.041 ↗
11. 10.1016/j.jallcom.2008.05.07910.1016/j.jallcom.2008.05.079 ↗
12. 10.1016/j.surfcoat.2009.09.07410.1016/j.surfcoat.2009.09.074 ↗
13. Xu X.Q. · Applied Surface Science · 2012 · 258 · 880210.1016/j.apsusc.2012.05.094 ↗
14. Liao Y. · Materialwissenschaft Und Werkstofftechnik · 2011 · 42 · 83310.1002/mawe.201100850 ↗
15. Ayfer K. · Materials Letters · 2012 · 76 · 1110.1016/j.matlet.2012.02.037 ↗
16. Jin Y. · Transactions of Materials and Heat Treatment · 2012 · 33 · 146