journal article·2018-12-10

Surface characteristics and erosion phenomena in WEDM of alumina composites

Meinam Annebushan Singh, Deba Kumar Sarma, Ondrej Hanzel, Jaroslav Sedláček, Pavol Šajgalík

Publisher page

Abstract

Reinforcing the ceramic materials with a conducting filler allows the net electrical properties to increase. This makes the composites machinable by electrical discharge process. Present work identifies the influence of multi-walled carbon nanotubes (MWCNT) as conducting fillers toward the machined surface profile. Alumina composites with 5 and 10 vol. % MWCNTs are fabricated and machined by wire electrical discharge machining process. The spalling effect is found to be more dominant at lower MWCNT concentrations in the composites. Cracks, porosity, and oxidization of the surface materials are the main defects observed during the machining process. Also, a more intense cracks and porous behavior is observed at lower concentration of MWCNT (5 vol. %). A closer analysis of machined surface edges yielded some phenomena of mechanical erosion and chipping due to physical contact. This situation is brought forward by low electrical conductivity and high brittleness of the composites. The Energy Dispersive X-Ray (EDX) analysis confers toward actual dissociation and melting of the carbon nanotubes even at low concentration of MWCNTs (5 vol. %) though not readily visible.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Machining and Optimization Techniques · Advanced machining processes and optimization · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering, National Institute of Technology Meghalaya, Shillong, India

Institute of Inorganic Chemistry, Slovak Academy of Sciences, Bratislava, Slovakia

Funding

Slovak Research and Development Agency

References (20)

Show source-provided references
1. 10.1016/j.ceramint.2014.06.09510.1016/j.ceramint.2014.06.095 ↗
2. 10.1081/MST-12003424010.1081/MST-120034240 ↗
3. 10.1155/2015/58495210.1155/2015/584952 ↗
4. 10.1007/s00170-017-0751-x10.1007/s00170-017-0751-x ↗
5. 10.1080/10426914.2017.127930110.1080/10426914.2017.1279301 ↗
6. 10.1080/10426914.2014.89298310.1080/10426914.2014.892983 ↗
7. 10.1016/j.jmatprotec.2004.02.01310.1016/j.jmatprotec.2004.02.013 ↗
8. 10.1080/1042691090276931910.1080/10426910902769319 ↗
9. 10.1016/j.cirp.2008.03.08910.1016/j.cirp.2008.03.089 ↗
10. 10.1080/1042691090276928510.1080/10426910902769285 ↗
11. 10.1111/j.1744-7402.2012.02756.x10.1111/j.1744-7402.2012.02756.x ↗
12. 10.1111/j.1551-2916.2011.04419.x10.1111/j.1551-2916.2011.04419.x ↗
13. 10.1080/10426914.2015.105894710.1080/10426914.2015.1058947 ↗
14. 10.1007/s10853-016-0346-110.1007/s10853-016-0346-1 ↗
15. 10.1016/S1369-7021(11)70214-010.1016/S1369-7021(11)70214-0 ↗
16. 10.1007/s40684-016-0032-410.1007/s40684-016-0032-4 ↗
17. 10.1016/j.ceramint.2015.12.12010.1016/j.ceramint.2015.12.120 ↗
18. 10.1016/j.jeurceramsoc.2017.03.05810.1016/j.jeurceramsoc.2017.03.058 ↗
19. 10.1016/j.ceramint.2017.10.17410.1016/j.ceramint.2017.10.174 ↗
20. 10.1016/j.jeurceramsoc.2014.01.02010.1016/j.jeurceramsoc.2014.01.020 ↗