Cathodic Induction of Hydrogen Blistering on Carbon Steel in Alkaline Sour Environment
Source abstract
Abstract
Abstract Hydrogen blistering was electrochemically induced on mild steel immersed in alkaline sour solution by cathodic reduction to study the onset of blistering. Test solution attempted to emulate that associated with water formed in catalytic cracking units of oil refinery plants with cyanide ions. Chronoamperometry method allowed blister diameter and density be tuned by potential pulses and testing time. A theoretical formula was used to calculate critical radius before blistering onset, assuming a depth for hydrogen implantation. A reasonable correlation was found between these measurements and those experimentally determined. The critical radius for blistering initiation seems to be ascribed to a stress higher than the yield stress of material. Blistering rupture displayed material tearing so that a ductile fracture appears to be a consequence of the aerostatic pressure of molecular hydrogen.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. “Present Day Knowledge of the Effect of Elemental Sulfur on Corrosion in Sour Gas Systems,”
2. Elboujdaini · Corrosion · 2006 · 62 · 2910.5006/1.3278248 ↗
3. Skei · Corrosion · 1953 · 9 · 16310.5006/0010-9312-9.5.163 ↗
4. Chu · Corrosion · 1999 · 55 · 89210.5006/1.3284046 ↗
5. Chu · Corrosion · 2000 · 56 · 104610.5006/1.3294381 ↗
6. Panagopoulos · Corros. Sci · 1988 · 40 · 183710.1016/S0010-938X(98)00080-8 ↗
7. Lunarska · Corrosion · 1996 · 52 · 14310.5006/1.3292105 ↗
8. Doherty · Corros. Sci · 2008 · 50 · 275510.1016/j.corsci.2008.03.020 ↗
9. Freud · Appl. Phys. Lett · 1997 · 70 · 351910.1063/1.119219 ↗
10. MacDonald · Corros. Sci · 1978 · 18 · 41110.1016/S0010-938X(78)80037-7 ↗
11. Smith · Br. Corros. J · 1975 · 10 · 13610.1179/000705975798320701 ↗
12. Wilhelm · Corrosion · 1994 · 50 · 15210.5006/1.3293504 ↗
13. Yamakawa · Corrosion · 1999 · 55 · 2410.5006/1.3283961 ↗
14. Ehmke · Hydrocarb. Process · 1981 · 60 · 149
15. Hagi · Mater. Trans., JIM · 1997 · 38 · 97010.2320/matertrans1989.38.970 ↗
16. Hemmingsen · Corrosion · 1992 · 48 · 47510.5006/1.3315963 ↗
17. Park · J. App. Phys · 2005 · 97 · 07431110.1063/1.1885183 ↗
18. “Wet H2S and CN− Corrosion Control Through On-Site Polysulfide Generation,”
19. Galicia · Electrochim. Acta · 2005 · 50 · 445110.1016/j.electacta.2005.02.007 ↗
20. French · Mater. Perform · 1978 · 3 · 20
21. Chen · Corros. Sci · 2009 · 51 · 119710.1016/j.corsci.2009.02.020 ↗
22. Hyodo · Corros. Sci · 1987 · 27 · 107710.1016/0010-938X(87)90100-4 ↗
23. Scheider · Eng. Frac. Mech · 2008 · 75 · 428310.1016/j.engfracmech.2007.10.002 ↗
24. Huang · Appl. Phys. Lett · 1999 · 74 · 98210.1063/1.123430 ↗
25. “Evaluation of Prediction Tool for Sour Water Corrosion,”
26. Millero · Mar. Chem · 1986 · 18 · 12110.1016/0304-4203(86)90003-4 ↗
27. “Standard Test Method for Determining Volume Fraction by Systematic Manual Point Count
28. Mitani · Appl. Phys. A · 1992 · 54 · 54310.1007/BF00324337 ↗
29. Zapffe · Trans. AIME · 1941 · 145 · 225
30. Khmelnitskiy · Vacuum · 2005 · 78 · 27310.1016/j.vacuum.2005.01.038 ↗