Abstract

The mechanical and thermal behaviour of traditional clay bricks were investigated after one hour exposure at three different temperatures (200, 400, 600 °C). Specimens collected from small-scale production units in Cameroon were used. It has been shown that the mechanical behaviour of traditional clay bricks after exposure depends on their quality of firing, which is most of the time affected by the limits of the traditional technologies used for their production. Among the samples collected, bricks of good quality and low quality of firing were identified. Bricks of good quality of firing have shown a progressive decay of mechanical strength from 200 °C after an increase from the room temperature to 200 °C. Those of low quality have shown an increase in mechanical strength from 400 °C after a stability observed between the room temperature and 400 °C. Both bricks have shown a phenomenon of embrittlement with the increase of the exposure temperature, which was much accentuated in the case of less fired bricks. Thermal conductivity of both bricks has shown a quasi-stability with exposure temperature due to their high porosity from the beginning.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Hygrothermal properties of building materials · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Dugal SK (2008) Building materials, 3rd edn. New Age International Publishers, New Delhi
2. Domone P, Illston J (2010) Construction materials: their nature and behavior, 4th edn. Spon Press, London, New-York10.4324/9780203927571 ↗
3. Berge B (2009) The ecology of building materials, 2nd edn. Architectural Press, Jordan Hill, Burlington10.4324/9780080949741 ↗
4. Lyons A (2010) Materials for architects and builders, 4th edn. Elsevier, Oxford, Burlington10.4324/9780080949598 ↗
5. Allen E, Iano J (2008) Fundamentals of building construction: materials and methods, 5th edn. Wiley, New York
6. Russo S, Sciarretta F (2012) Experimental and theoretical investigation on masonry after high temperature exposure. Exp Mech 52:341–359. doi: 10.1007/s11340-011-9493-010.1007/s11340-011-9493-0 ↗
7. Russo S, Boscato G, Sciarretta F (2008) Behaviour of a historical masonry structure subjected to fire. Mason Int 21(1):1–14
8. Russo S, Sciarretta F (2009) Residual strength of traditional brick masonry subjected to high temperatures. In: Mazzolani F (ed) Protection of historical buildings—ProHiTech 09. Balkema, Rome, pp 1417–1422
9. Russo Salvatore, Sciarretta Francesca (2013) Masonry exposed to high temperatures: mechanical behaviour and properties—an overview. Fire Safty J 55:69–8610.1016/j.firesaf.2012.10.001 ↗
10. Ngon Ngon GF (2007) Etude morphologique, minéralogique, géochimique et cristallographique des argiles latéritiques et argiles hydromorphes de la région de Yaoundé (Cameroun). Thèse doctorat/Ph.D, Université de Yaoundé I
11. Norme Européenne EN 771-1 (2011): Spécification des éléments de maçonnerie—Partie 1: Briques de terre cuite
12. Thê-Duong N (2009) Etude du comportement au Feu des Maçonneries de Briques en Terre cuite. Université Paris-Est, Thèse de Doctorat
13. Görhan Gökhan, Simsek O (2013) Porous clay bricks manufactured with rice husks. Constr Build Mater 40:390–39610.1016/j.conbuildmat.2012.09.110 ↗
14. Bing Q (2009) Influence de l’endommagement sur les propriétés d’élasticité de matériaux modèles, approche expérimentale et numérique. Thèse de Doctorat, Université de Limoges
15. Simonin F (2000) Comportement thermomécanique des bétons réfractaires alumineux contenant du spinelle de magnésium. Thèse de Doctorat, Institut National des Sciences Appliquées de Lyon
16. Ngon Ngon GF et al (2012) Study of physical and mechanical applications on ceramics of the lateritic and alluvial clayey mixtures of the Yaoundé region (Cameroon). Constr Build Mater 31:294–29910.1016/j.conbuildmat.2011.12.108 ↗
17. Norme EN 772-3 (1999) : Méthodes d’essais des éléments de maçonnerie- Partie 3 : Détermination du volume net et du pourcentage des vides des éléments de maçonneries en terre cuite par pesée hydrostatique
18. Norme EN 1745 (2012): Maçonnerie et éléments de maçonnerie, Méthodes pour la détermination des propriétés thermiques
19. Norme Européenne EN 772-1 (2011): Méthodes d’essais des éléments de maçonnerie -Partie 1: Détermination de la résistance à la compression
20. Kornmann M (2005) Matériaux de construction en terre cuite—fabrication et propriétés, 1st edn. Septima, Paris
21. Furlani E, Maschio S (2013) Mechanical properties and microstructure of fast fired tiles made with blends of kaolin and olivine powders. Ceram Int 39:9391–939610.1016/j.ceramint.2013.04.113 ↗
22. Carretero MI, Dondi M, Fabbri B, Raimondo M (2002) The influence of shaping and firing technology on ceramic properties of calcareous and non-calcareous illitic–chloritic clays. Appl Clay Sci 20:301–30610.1016/S0169-1317(01)00076-X ↗
23. Robinson GC, Borchelt JG (1994) Factors Influencing Clay Brick Durability. 10th IBBMaC, Calgary Canada. http://www.hms.civil.uminho.pt/ibmac/1994/1295.pdf . Accessed 19 Feb 2016
24. Chen Xudong, Shengxing Wu, Zhhou Jikai (2013) Influence o porosity on compressive and tensile strength of cement mortar. Constr Build Mater 40:869–87410.1016/j.conbuildmat.2012.11.072 ↗
25. Prosper Pliya BA (2010) Contribution des fibres de polypropylène et métalliques à l’amélioration du comportement du béton soumis à une température élevée. Université de Cergy-Pontoise, Thèse de Doctorat