Crack growth behaviour and crack tip chemistry of X70 pipeline steel in near-neutral pH environment
Source abstract
Abstract
In this paper, crack growth behaviour and the crack tip chemistry of X70 pipeline steel in the near-neutral pH environment were investigated using the in-situ measurements. The stress corrosion crack propagated forward under the cyclic load, with a mean crack growth rate (CGR) of 4.28 × 10–3 mm/cycle. The CGR da/dN obeys well with the stress corrosion fatigue mechanism. During the crack propagation, the crack tip environment differed significantly from the bulk solution. An aggressive electrolyte with low pH (about 4.0) and high concentration of Cl– (about 3.8 M) was produced near the crack tip. These results provided the direct evidence for simulating the crack tip solution and investigating the crack tip anodic dissolution.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Parkins R. N. · Corrosion · 2000 · 2000
2. 10.1016/j.electacta.2007.07.01510.1016/j.electacta.2007.07.015 ↗
3. 10.5006/1.328397110.5006/1.3283971 ↗
4. 10.1016/j.elecom.2010.04.02510.1016/j.elecom.2010.04.025 ↗
5. 10.1016/j.corsci.2010.02.02010.1016/j.corsci.2010.02.020 ↗
6. 10.1016/j.corsci.2013.06.05110.1016/j.corsci.2013.06.051 ↗
7. 10.1016/j.corsci.2011.10.00210.1016/j.corsci.2011.10.002 ↗
8. 10.5006/1.358202610.5006/1.3582026 ↗
9. 10.1149/1.241179910.1149/1.2411799 ↗
10. 10.5006/1.329436510.5006/1.3294365 ↗
11. 10.5006/1.358497510.5006/1.3584975 ↗
12. 10.1111/j.1475-1305.2010.00784.x10.1111/j.1475-1305.2010.00784.x ↗
13. 10.1016/j.corsci.2006.12.00110.1016/j.corsci.2006.12.001 ↗
14. ASTM E647: ‘Standard test method for fatigue crack growth rates’, 2005, Philadelphia, The American Society for Testing of Materials.
15. 10.1016/j.corsci.2012.10.03010.1016/j.corsci.2012.10.030 ↗
16. 10.1016/j.corsci.2007.01.01110.1016/j.corsci.2007.01.011 ↗
17. 10.5006/109410.5006/1094 ↗
18. 10.5006/1.358312510.5006/1.3583125 ↗
19. 10.5006/1.327755910.5006/1.3277559 ↗
20. Beavers J. A. · Corrosion · 1998 · 98
21. Beavers J. A. · Corrosion · 2001
22. 10.1007/s11661-007-9184-810.1007/s11661-007-9184-8 ↗
23. 10.1179/1743278215Y.000000003510.1179/1743278215Y.0000000035 ↗
24. 10.5006/1.327817110.5006/1.3278171 ↗
25. 10.1016/S0308-0161(01)00018-710.1016/S0308-0161(01)00018-7 ↗
26. 10.5006/099810.5006/0998 ↗
27. 10.1016/0010-938X(83)90014-810.1016/0010-938X(83)90014-8 ↗
28. L. Sathler and J. van Muylder: ‘CEBELCOR Rapports Techniques’, report, 1974.
29. 10.5006/1.329434810.5006/1.3294348 ↗
30. King F. · Corrosion 2000 · 2000
31. 10.1016/j.corsci.2012.06.01610.1016/j.corsci.2012.06.016 ↗
32. 10.1016/0010-938X(80)90128-610.1016/0010-938X(80)90128-6 ↗