Abstract
The development of severe localised corrosion (SLC) on the 2198-T8 alloy was investigated in solutions of various NaCl concentrations (0.001, 0.005 and 0.01 mol L−1). Immersion tests, optical profilometry, conventional and local electrochemical analyses were performed to evaluate the corrosion behaviour of the alloy. Immersion tests showed that the alloy is susceptible to SLC in all conditions, although the pits sizes were dependent on the solution concentration. The largest anodic areas, corresponding to SLC sites, were observed for the sample immersed in 0.001 mol L−1 NaCl, whereas pits with similar sizes were observed for the samples immersed in solutions with 0.005 and 0.01 mol L−1 of NaCl. Moreover, the maximum depth of attack was observed for the sample immersed in 0.001 mol L−1 NaCl. These results were in agreement with the scanning ion-selective electrode technique (SIET) maps which showed stronger acidification on the sample exposed to 0.001 mol L−1 NaCl solution.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Science and Technology Center, Nuclear and Energy Research Institute – IPEN/CNEN, São Paulo, Brazil
Funding
CAPES · FAPESP
References (44)
Show source-provided references
1. Polmear IJ. · Mater Forum · 2004 · 28 · 1
2. 10.1016/j.matdes.2013.12.00210.1016/j.matdes.2013.12.002 ↗
3. Prasad NE · 2014
4. 10.1007/s11665-018-3244-710.1007/s11665-018-3244-7 ↗
5. 10.1016/j.ijfatigue.2013.07.00910.1016/j.ijfatigue.2013.07.009 ↗
6. Donatus U · Corros Eng Sci Technol · 2018 · 54 · 1
7. 10.1557/jmr.2018.3310.1557/jmr.2018.33 ↗
8. Araujo JVdS · Corros Eng Sci Technol · 2019 · 54 · 110.1080/1478422X.2018.1521591 ↗
9. 10.5006/305410.5006/3054 ↗
10. 10.1016/j.matchemphys.2015.05.03710.1016/j.matchemphys.2015.05.037 ↗
11. 10.1149/1.204844710.1149/1.2048447 ↗
12. 10.1002/maco.20040382410.1002/maco.200403824 ↗
13. 10.1016/j.corsci.2006.12.00210.1016/j.corsci.2006.12.002 ↗
14. 10.3390/ma1210160010.3390/ma12101600 ↗
15. 10.1016/S1003-6326(16)64252-810.1016/S1003-6326(16)64252-8 ↗
16. 10.1016/j.corsci.2011.05.06610.1016/j.corsci.2011.05.066 ↗
17. 10.1016/j.corsci.2014.03.00110.1016/j.corsci.2014.03.001 ↗
18. Lamaka S · 2010 · 2162
19. 10.1088/0957-0233/22/7/07570410.1088/0957-0233/22/7/075704 ↗
20. Souto RM · 2010 · 1769
21. Izquierdo J · Int J Electrochem Sci · 2012 · 7 · 1137710.1016/S1452-3981(23)16951-3 ↗
22. 10.1016/S1674-4799(09)60014-510.1016/S1674-4799(09)60014-5 ↗
23. 10.1016/j.apsusc.2017.11.14110.1016/j.apsusc.2017.11.141 ↗
24. 10.5006/235410.5006/2354 ↗
25. 10.1016/j.elecom.2017.05.00710.1016/j.elecom.2017.05.007 ↗
26. 10.1016/j.electacta.2011.01.09110.1016/j.electacta.2011.01.091 ↗
27. 10.1016/j.corsci.2018.01.02810.1016/j.corsci.2018.01.028 ↗
28. 10.1080/1478422X.2019.160547210.1080/1478422X.2019.1605472 ↗
29. Silva RMP · Surf Coatings Technol · 2019 · 51 · 982
30. 10.1007/BF0034878110.1007/BF00348781 ↗
31. 10.1557/jmr.2014.12110.1557/jmr.2014.121 ↗
32. 10.1016/B978-0-12-401698-9.00002-110.1016/B978-0-12-401698-9.00002-1 ↗
33. 10.1016/j.jare.2017.12.00410.1016/j.jare.2017.12.004 ↗
34. 10.1016/j.corsci.2016.02.01810.1016/j.corsci.2016.02.018 ↗
35. 10.1002/sia.581710.1002/sia.5817 ↗
36. 10.5006/241810.5006/2418 ↗
37. 10.1149/1.356220610.1149/1.3562206 ↗
38. Hughes AE · 2011 · 223
39. 10.1201/978020390913310.1201/9780203909133 ↗
40. 10.1002/9780470381588.ch1310.1002/9780470381588.ch13 ↗
41. 10.1016/j.electacta.2012.04.02010.1016/j.electacta.2012.04.020 ↗
42. 10.1016/j.jallcom.2015.10.18510.1016/j.jallcom.2015.10.185 ↗
43. 10.1590/1980-5373-mr-2020-016110.1590/1980-5373-mr-2020-0161 ↗
44. 10.1149/2.0541911jes10.1149/2.0541911jes ↗