Understanding and quantifying the anoxic corrosion of carbon steel in a Swiss L/ILW repository environment

Nick Senior, Roger Newman, Steve Wang, Nikitas Diomidis

Abstract

The anaerobic corrosion of steel was monitored under simulated Swiss low-/intermediate-level waste repository conditions. Steel was studied both as bare rods and cast in cement, in water vapour, simulating the unsaturated anoxic phase, and during immersion in various pore waters, representative of the saturated phase. All tests were performed at 50°C. Hydrogen evolution from grout, comprising commercial cement and sand, was also studied. Grouted steel specimens initially generated hydrogen that was comparable to grout alone, which was attributed to the presence of iron detritus from the ball-milling of cement clinker. The corrosion rate of immersed test specimens peaked during the first 100 days, likely due to the formation of a passive film. Corrosion rates generally declined to <3 nm/year, although there were several notable exceptions where hydrogen generation was erratic. This was attributed to localised corrosion and may be an important factor to understand when modelling hydrogen generation rates.This paper is part of a supplement on the 6th International Workshop on Long-Term Prediction of Corrosion Damage in Nuclear Waste Systems.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

CanmetMATERIALS, Hamilton, Canada

Department of Chemical Engineering and Applied Chemistry, University of Toronto, Toronto, Canada

Nagra, Wettingen, Switzerland

Funding

Nagra

References (10)

Show source-provided references
1. Diomidis N, Cloet V, Leupin OX, et al. Production, consumption and transport of gases in deep geological repositories according to the Swiss disposal concept. Nagra, Wettingen, Switzerland; 2016. (Nagra Technical Report NTB 16-03).
2. Diomidis N. Scientific basis for the production of gas due to corrosion in a deep geological repository. Nagra, Wettingen, Switzerland; 2014. (Nagra Arbeitsbericht NAB 14-21).
3. Smart NR, Blackwood DJ, March GP, et al. The anaerobic corrosion of carbon and stainless steels in simulated repository environments – a summary review of Nirex research. AEA Technology, Harwell, UK; 2004. (Report AEAT/ERRA-0313).
4. Kaneko M, Norihiko M, Fujiwara A, et al. Evaluation of gas generation rate by metal corrosion in the reducing environment. RWMC Technical Report RWMC-TRE-03003. RWMC, Tokyo, Japan; 2004.
5. Fujiwara A. Gas generation by steel corrosion under reductive conditions – continuous measurement tests. Presented at the GASNET Workshop; 2002 November 12–14; Cologne, Germany.
6. Bradbury MH, Baeyens B. Far-field sorption databases for performance assessment of a high-level radioactive waste repository in an undisturbed Opalinus Clay host rock. Nagra, Wettingen, Switzerland; 2003. (Nagra Technical Report NTB 02-19).
7. 10.1179/1743278210Y.000000001010.1179/1743278210Y.0000000010 ↗
8. Simpson JP. Experiments on container materials for Swiss high-level waste disposal projects, Part-IV. Nagra Technical Report NTB 89-19. Nagra, Wettingen, Switzerland; 1989.
9. 10.1557/PROC-556-119910.1557/PROC-556-1199 ↗
10. Nishimura T · Kobe Steel Eng Rep · 2003 · 53 · 78