Cavitation erosion and corrosion-cavitation synergism behaviour of CoCrFeNiMnTi x high entropy alloy coatings prepared by laser cladding
Source abstract
Abstract
Cavitation erosion and corrosion-cavitation synergism behavior of CoCrFeNiMnTi x ( x = 0.5, 1.0, 1.5, 2.0 in atomic ratio) high entropy alloy coatings were analyzed. The sample with x = 1.0 showed the best cavitation erosion resistance due to the low weight loss and the maximum erosion rate. The protective ability of passivation film also displayed an increased first and then decreased tendency with the increase of Ti content as indicated by corrosion-cavitation synergism determined by open circuit potential method under cavitation erosion and quiescence condition. The sample with x = 1.0 displayed good re-passivation ability of passivation film according to open circuit potential behavior under cavitation erosion and quiescence condition. In general, the sample with x = 1.0 exhibited the highest cavitation erosion, the best self-repairing ability of the passivation film under the corrosion-cavitation synergism condition, which showed a great potential in the application of ocean engineering field as fluid-passing parts.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, Shenyang University of Technology, Shenyang, People's Republic of China
Shenyang Dalu Laser Technology CO., LTD, Shenyang, People's Republic of China
Funding
National Key Research and Development Program of China · Science and Technology Research Project of Liaoning Province · Shenyang Science and Technology Funded Project
References (23)
Show source-provided references
1. 10.1179/1743278215Y.000000003310.1179/1743278215Y.0000000033 ↗
2. 10.1179/147842209X1257940158684310.1179/147842209X12579401586843 ↗
3. Panhalkar N · Corros Eng, Sci Technol · 2015 · 51 · 416
4. 10.1179/14784220377022699710.1179/147842203770226997 ↗
5. 10.1016/0921-5093(89)90317-110.1016/0921-5093(89)90317-1 ↗
6. 10.1016/j.triboint.2019.01.01810.1016/j.triboint.2019.01.018 ↗
7. 10.1016/j.ultsonch.2019.10476010.1016/j.ultsonch.2019.104760 ↗
8. 10.1016/j.ultsonch.2018.09.00410.1016/j.ultsonch.2018.09.004 ↗
9. 10.1016/j.ultsonch.2017.04.01110.1016/j.ultsonch.2017.04.011 ↗
10. 10.1016/j.wear.2017.06.00310.1016/j.wear.2017.06.003 ↗
11. 10.1016/j.surfcoat.2021.12689910.1016/j.surfcoat.2021.126899 ↗
12. 10.1016/j.corsci.2021.10966310.1016/j.corsci.2021.109663 ↗
13. Nair RB · Ultrason Sonochem · 2017 · 1350 · 30450
14. Kwok CT · Surf Coat Technol · 2016 · 0257 · 30081
15. 10.1016/j.optlastec.2016.04.01110.1016/j.optlastec.2016.04.011 ↗
16. Nair RB · Ultrason. Sonochem · 2018 · 1350 · 30515
17. G32-10 A. Standard test method for cavitation erosion using vibratory apparatus. ASTM Int. 2010.
18. 10.1016/j.triboint.2015.04.03910.1016/j.triboint.2015.04.039 ↗
19. 10.20964/2020.01.5110.20964/2020.01.51 ↗
20. 10.1016/j.jallcom.2016.12.19610.1016/j.jallcom.2016.12.196 ↗
21. 10.3390/met1202019810.3390/met12020198 ↗
22. 10.1016/j.wear.2022.20451010.1016/j.wear.2022.204510 ↗
23. 10.1016/j.ceramint.2022.04.04910.1016/j.ceramint.2022.04.049 ↗