journal article·2023-05-19

Localised corrosion failure of an L245N pipeline in a CO 2 –O 2 –Cl − environment

Jihui Leng, Zhiyuan Tian, Kexi Liao, Tengjiao He, Xin Liu, Guoxi He, Xin Tang, Guoqiang Xia

Publisher page

Abstract

Multicomponent thermal fluid flooding has become a widely used and very effective heavy-oil recovery technology, but the harsh CO2–O2–Cl− environment can lead to serious corrosion perforation failure of the pipeline. Therefore, the influence of O2 content and main controlling factors on corrosion perforation were investigated through a weight-loss experiment, corrosion defect test, characterization and grey correlation method. The results showed that, with the increase in O2 content, the general corrosion rate and localized corrosion rate increased. The uneven protection performance of the product after the addition of O2 was found to be the key cause of localized corrosion. In addition, the synergistic effect of O2–Cl− promoted the lateral and longitudinal expansion of pits. The results of the grey correlation showed that the temperature (30–120 °C) had a greater impact on localized corrosion compared with the content of O2 (0–0.045 MPa) and Cl− (0–16,000 mg/L).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Petroleum Engineering School, Southwest Petroleum University, Chengdu, People’s Republic of China

Kunming Maintenance and Repair Branch, Southwest Petroleum and Gas Pipeline Co., Ltd., PipeChina, Kunming, People’s Republic of China

Funding

National Natural Science Foundation of China

References (46)

Show source-provided references
1. 10.1002/maco.20170994010.1002/maco.201709940 ↗
2. 10.1002/maco.20181054210.1002/maco.201810542 ↗
3. 10.1016/j.isatra.2021.06.00610.1016/j.isatra.2021.06.006 ↗
4. He GX · Proc Bienn Int Pipeline Conf IPC · 2020 · 3 · 1
5. 10.1016/j.engfailanal.2021.10572010.1016/j.engfailanal.2021.105720 ↗
6. 10.1016/j.electacta.2018.09.11410.1016/j.electacta.2018.09.114 ↗
7. 10.1016/j.corsci.2020.10853110.1016/j.corsci.2020.108531 ↗
8. 10.1016/j.ijhydene.2015.09.07010.1016/j.ijhydene.2015.09.070 ↗
9. Du Y · J Zhejiang Univ · 2017 · 51 · 429
10. 10.1016/j.ijheatmasstransfer.2017.03.10310.1016/j.ijheatmasstransfer.2017.03.103 ↗
11. Zhao S · Arab J Sci Eng · 2022
12. 10.1016/j.engfailanal.2018.03.00610.1016/j.engfailanal.2018.03.006 ↗
13. 10.1016/j.jngse.2015.12.05210.1016/j.jngse.2015.12.052 ↗
14. 10.5006/1.358521210.5006/1.3585212 ↗
15. 10.1016/j.corsci.2017.07.00310.1016/j.corsci.2017.07.003 ↗
16. 10.1002/sia.305710.1002/sia.3057 ↗
17. Schmitt G. Fundamental aspects of CO 2 metal loss corrosion – Part II: influence of different parameters on CO 2 corrosion mechanism. CORROSION 2015 (Dallas, Texas, US). NACE 2015;6033.
18. 10.1021/ef300279510.1021/ef3002795 ↗
19. 10.1016/j.matdes.2010.01.03810.1016/j.matdes.2010.01.038 ↗
20. 10.1007/s10800-012-0389-110.1007/s10800-012-0389-1 ↗
21. Rosli NR, Nešić S, Choi YS, et al. Corrosion of UNS G10180 steel in supercritical and subcritical CO 2 with O 2 as a contaminant, CORROSION 2016 (Vancouver, British Columbia, Can). NACE 2016;7527.
22. 10.1016/j.corsci.2010.12.01410.1016/j.corsci.2010.12.014 ↗
23. 10.1016/j.corsci.2021.10993510.1016/j.corsci.2021.109935 ↗
24. 10.20964/2020.09.2410.20964/2020.09.24 ↗
25. 10.5006/1.327819510.5006/1.3278195 ↗
26. 10.1016/j.corsci.2014.03.02510.1016/j.corsci.2014.03.025 ↗
27. 10.1016/j.matchemphys.2021.12501610.1016/j.matchemphys.2021.125016 ↗
28. 10.1016/j.engfailanal.2021.10562210.1016/j.engfailanal.2021.105622 ↗
29. 10.1021/es102578c10.1021/es102578c ↗
30. 10.1016/j.apsusc.2014.12.10910.1016/j.apsusc.2014.12.109 ↗
31. 10.1016/S0378-7753(00)00376-110.1016/S0378-7753(00)00376-1 ↗
32. 10.1016/j.corsci.2012.03.02210.1016/j.corsci.2012.03.022 ↗
33. 10.1016/j.engfailanal.2021.10574810.1016/j.engfailanal.2021.105748 ↗
34. Liu W, Wu F, Dou JJ, et al. Effect of Cl − concentration on erosion-corrosion behavior of S43400 and S31603 stainless steels in high temperature and high pressure CO 2 -O 2 environment. CORROSION 2015 (Dallas, Texas, US). NACE 2015;5973.
35. 10.1016/j.engfailanal.2022.10633210.1016/j.engfailanal.2022.106332 ↗
36. ASTM Committee G-1 on corrosion of metals, standard practice for preparing, cleaning, and evaluating corrosion test specimens. ASTM International. 2011.
37. 10.1016/j.corsci.2021.10935010.1016/j.corsci.2021.109350 ↗
38. 10.1016/j.corsci.2018.03.02010.1016/j.corsci.2018.03.020 ↗
39. 10.3390/ma1109163510.3390/ma11091635 ↗
40. 10.1149/1.212740110.1149/1.2127401 ↗
41. 10.1016/j.ijggc.2011.05.01010.1016/j.ijggc.2011.05.010 ↗
42. 10.1016/j.corsci.2015.08.01610.1016/j.corsci.2015.08.016 ↗
43. 10.1016/j.corsci.2007.06.00610.1016/j.corsci.2007.06.006 ↗
44. 10.1149/1.210838110.1149/1.2108381 ↗
45. 10.1016/j.egypro.2011.02.05110.1016/j.egypro.2011.02.051 ↗
46. 10.5006/0010-9312-35.3.13610.5006/0010-9312-35.3.136 ↗