journal article·2021-02-17

Atmospheric and immersion corrosion of steel alloyed with aluminium

R. Jeffrey, R. E. Melchers

Publisher page

Abstract

This paper reports a systematic study of longer-term marine atmospheric and immersion corrosion losses for mild steel alloyed with small to moderate amounts (0, 2, 4, 6 and 8% by weight) of aluminium. Such steel coupons were exposed for up to 3 years in temperate sea water and also just below the mud-line, and for up to one year at two severe atmospheric marine locations. Compared with the coupons without aluminium, higher aluminium content reduced corrosion loss in immersed conditions from 10.5% after one year to 2.8% after 3 years. Below the mud-line corrosion losses showed a similar trend but were more varied. In the marine atmosphere, the reduction in corrosion loss for increased aluminium content ranged from 58 to 81% after one-year exposure. The results show that aluminium alloying above about 4% has limited additional benefit for corrosion in any of the marine exposure environments.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Centre for Infrastructure Performance and Reliability, The University of Newcastle, Callaghan, Australia

Funding

Australian Research Council

References (24)

Show source-provided references
1. VanderVoort GF. · 198410.31399/asm.tb.mpp.9781627082600 ↗
2. Roberge P. · 2008
3. Evans UR. · 1960
4. 10.1016/j.corsci.2003.10.00410.1016/j.corsci.2003.10.004 ↗
5. 10.5006/1.327988810.5006/1.3279888 ↗
6. 10.2320/matertrans.42.47810.2320/matertrans.42.478 ↗
7. 10.1016/S0010-938X(02)00186-510.1016/S0010-938X(02)00186-5 ↗
8. Rajendran N, Nishimura T. Electrochemical monitoring of the rust of low alloy steels under atmospheric corrosion environment. In: Meeting Abstracts, 205th Meeting of the electrochemical Society, MA 2004, p. 114 (ISSN: 1091-8213); 2004.
9. 10.4028/www.scientific.net/MSF.475-479.5510.4028/www.scientific.net/MSF.475-479.55 ↗
10. 10.1016/S1359-6454(03)00089-210.1016/S1359-6454(03)00089-2 ↗
11. 10.1023/A:100468231640810.1023/A:1004682316408 ↗
12. Perlade A, Maugis P. Development of new lightweight high strength steels. In: Discussion meeting on the Development of Innovative iron aluminium alloys. Toulouse, May 24, Arcelor Research, Automotive Products Research Centre; 2005.
13. Kubaschewski O. · 1982
14. ASTM Standard G1-03. G1-03: Standard practice for preparing, cleaning, and evaluating corrosion test specimens. Washington: ASTM International; 2011, pp. 1–11.
15. AS/NZS 2728 · 2013
16. Jeffrey R, Melchers RE. Three year observations of corrosion losses for steels at a severe marine atmospheric site. In: Proc corrosion & Prevention 2008; Nov 17–19, Wellington, NZ: Australasian Corrosion Association; 2008. (CDROM, Paper 039).
17. Jeffrey R, Melchers RE. The effect of increasing amounts of nutrient on the corrosion rate of mild steel. In: Proc. ACA Conference, Corrosion & Prevention 2012, Nov 11–14, Melbourne; 2012. (CD ROM, Paper No. 029).
18. 10.1016/j.corsci.2009.06.02010.1016/j.corsci.2009.06.020 ↗
19. 10.5006/1.327838510.5006/1.3278385 ↗
20. 10.3390/cmd101000410.3390/cmd1010004 ↗
21. Schumacher M · 1979
22. 10.6028/NBS.CIRC.57910.6028/NBS.CIRC.579 ↗
23. Southwell CR · Mater Perform · 1976 · 15 · 9
24. 10.1016/0010-938X(83)90024-010.1016/0010-938X(83)90024-0 ↗