Improved corrosion resistance of SS316L in molten nitrates containing chloride ions: Pre-oxidation treatment
Source abstract
Abstract
This study investigates the influence of pre-oxidation treatment on the corrosion of SS316L in molten solar salt with added chloride ions. The results show that bare SS316L is subjected to severe corrosion in a molten solar salt containing a large amount of chloride ions, with a loose oxide layer forming on the surface and exhibiting pronounced delamination. However, after being pre-oxidised at 800 °C for 5 h, a continuous and dense oxide layer on the surface of SS316L was formed. The pre-formed Fe 3 O 4 and Cr 2 O 3 oxide layer enables the oxide/matrix interface to maintain low oxygen and chlorine pressure, thereby slowing down the oxidation–chlorination reaction rate. Finally, corrosion products with a three-layered structure consisting of Fe 2 O 3 , Fe 3 O 4 , FeCr 2 O 4 and NiFe 2 O 4 are formed, which maintains the integrity structure during the whole immersion and improves the corrosion resistance of SS316L. Roles of the pre-oxidation mechanism give new insights into alloy protection in molten nitrates with chloride ions. It offers a novel approach to enhancing the corrosion resistance of next-generation concentrated solar power equipment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Phase Change Materials Research · Solar Thermal and Photovoltaic Systems · Radiative Heat Transfer Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Guangxi University
Funding
the innovation Project of Guangxi Graduate Education · the Guangxi Major Talents Program · the Opening Project of Guangxi Key Laboratory of Petrochemical Resource Processing and Process Intensification Technology
References (26)
Show source-provided references
1. 10.1016/j.rser.2017.05.06710.1016/j.rser.2017.05.067 ↗
2. 10.1016/j.solmat.2023.11241110.1016/j.solmat.2023.112411 ↗
3. 10.1016/j.solmat.2021.11133110.1016/j.solmat.2021.111331 ↗
4. 10.1016/j.solener.2020.12.05710.1016/j.solener.2020.12.057 ↗
5. 10.1016/j.est.2024.11088610.1016/j.est.2024.110886 ↗
6. 10.1016/j.apenergy.2009.06.02210.1016/j.apenergy.2009.06.022 ↗
7. 10.1016/j.solener.2011.05.00410.1016/j.solener.2011.05.004 ↗
8. 10.1016/j.solener.2021.11.05810.1016/j.solener.2021.11.058 ↗
9. 10.1007/s10853-013-7214-z10.1007/s10853-013-7214-z ↗
10. 10.1002/maco.20160930010.1002/maco.201609300 ↗
11. 10.1016/j.est.2021.10267510.1016/j.est.2021.102675 ↗
12. 10.1007/s11085-021-10025-y10.1007/s11085-021-10025-y ↗
13. 10.1016/j.renene.2015.07.09010.1016/j.renene.2015.07.090 ↗
14. 10.1016/j.solmat.2017.01.02810.1016/j.solmat.2017.01.028 ↗
15. 10.1016/j.solmat.2024.11282010.1016/j.solmat.2024.112820 ↗
16. 10.1007/s11085-024-10309-z10.1007/s11085-024-10309-z ↗
17. 10.1016/j.jmrt.2025.04.20710.1016/j.jmrt.2025.04.207 ↗
18. Wu J. Study on the properties of chromium carbide coating prepared by using molten salt electrodeposition and disproportionation reaction and its properties. Nanning, Guangxi: Guangxi University, 2022.
19. 10.3390/met1406063910.3390/met14060639 ↗
20. 10.1016/j.surfcoat.2024.13074410.1016/j.surfcoat.2024.130744 ↗
21. 10.1016/j.corsci.2020.10847310.1016/j.corsci.2020.108473 ↗
22. 10.1016/j.solmat.2019.11016210.1016/j.solmat.2019.110162 ↗
23. 10.1016/j.surfcoat.2018.05.08110.1016/j.surfcoat.2018.05.081 ↗
24. 10.1016/j.jallcom.2016.06.02310.1016/j.jallcom.2016.06.023 ↗
25. 10.1016/j.ijhydene.2014.05.12210.1016/j.ijhydene.2014.05.122 ↗
26. 10.1016/j.ssi.2010.12.01710.1016/j.ssi.2010.12.017 ↗