Abstract

Specimens of AA2099-T8 were immersed for different times ranging from 2 to 180 min in 0.1M NaCl. The development of corrosion around intermetallic particles was studied by scanning electron microscopy (SEM) with energy-dispersive X-ray spectrometry (EDXS). The degradation evolution of each major intermetallic particle after exposure of the alloy to electrolyte allowed to determine which particle corroded during the first stages of immersion. The corrosion of lithium-containing particles was also investigated by transmission electron microscopy (TEM). The earliest stages of attack started with localised corrosion of Al2CuMg (S-phase) particles resulting in dealloying which was followed by trenching around these particles. After 10 min, trenching was observed around Al7Cu2Fe(Mn) particles and then progressed to AlCuFeMnSi particles after 90 min.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Nanoporous metals and alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

French Corrosion Institute, Brest, France

References (24)

Show source-provided references
1. 10.1016/j.matdes.2013.12.00210.1016/j.matdes.2013.12.002 ↗
2. 10.1016/j.matchemphys.2015.05.03710.1016/j.matchemphys.2015.05.037 ↗
3. 10.3390/ma1210160010.3390/ma12101600 ↗
4. Landolt D. Corosion et chimie de surfaces des matériaux. Traité des matériaux; 2003, p. 11.
5. 10.1016/B978-0-12-401698-9.00004-510.1016/B978-0-12-401698-9.00004-5 ↗
6. Huisert M. Electrochemical characterization of filiform corrosion on aluminium rolled products. Technische Universiteit Delft; 2001.
7. Tao J. Surface composition and corrosion behavior of an Al-Cu alloy. Chemical Physics. Université Pierre et Marie Curie-Paris VI; 2016.
8. 10.1149/1.147154610.1149/1.1471546 ↗
9. 10.1016/S0010-938X(99)00012-810.1016/S0010-938X(99)00012-8 ↗
10. 10.1016/j.jallcom.2015.10.18510.1016/j.jallcom.2015.10.185 ↗
11. 10.1002/sia.581710.1002/sia.5817 ↗
12. 10.1016/B978-1-78242-283-9.00004-X10.1016/B978-1-78242-283-9.00004-X ↗
13. 10.1016/j.corsci.2006.12.00210.1016/j.corsci.2006.12.002 ↗
14. 10.1016/j.corsci.2016.02.01810.1016/j.corsci.2016.02.018 ↗
15. 10.1149/1.205494310.1149/1.2054943 ↗
16. 10.1149/2.0931811jes10.1149/2.0931811jes ↗
17. 10.1016/j.corsci.2007.02.00110.1016/j.corsci.2007.02.001 ↗
18. 10.1149/2.0431603jes10.1149/2.0431603jes ↗
19. 10.1016/j.corsci.2010.09.00910.1016/j.corsci.2010.09.009 ↗
20. 10.1016/j.matchemphys.2010.12.01410.1016/j.matchemphys.2010.12.014 ↗
21. 10.4028/www.scientific.net/MSF.765.62910.4028/www.scientific.net/MSF.765.629 ↗
22. 10.1149/1.176478110.1149/1.1764781 ↗
23. 10.5006/1.329033910.5006/1.3290339 ↗
24. Karayan AI. Exfoliation corrosion susceptibility and mechanisms of Al-Li 2060 T8E30 aluminium lithium alloy in acidic media [PhD]; 2015.