Stress corrosion cracking in the context of deep geological nuclear disposal – investigations on P235 and P265 steels
Source abstract
Abstract
Stress corrosion cracking of P235 and P265 steels is investigated through slow strain rate and constant deformation tests on samples exposed in a cell reproducing the underground conditions of the French deep geological nuclear disposal, at 25 and 90°C. The samples were taken from the base metal, the heat affected zone and the fusion zone of a P265 steel weld joint. Tests were performed at the free corrosion potential and under polarisation in the cathodic or anodic domains. Long-term constant deformation tests were also carried out to evaluate the behaviour of the material under static loading in hydrated clay environment. The results show a significant sensitivity of the tested materials to environmental cracking in the experimental conditions, with an enhancement of the effect of the environment for the weld metal. A mechanism of hydrogen embrittlement is proposed to be responsible for the cracking phenomenon. Susceptibility to environmental assisted cracking observed during these tests indicates the need to optimise welding parameters and steel chemical composition and metallurgy, particularly regarding the presence of inclusions in the base metal and stress relief of the weld metal. This paper is part of a supplement on the 6th International Workshop on Long-Term Prediction of Corrosion Damage in Nuclear Waste Systems.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Den-Service de la Corrosion et du Comportement des Matériaux dans leur Environnement (SCCME), CEA, Université Paris-Saclay, Gif-sur-Yvette, France
Laboratoire Analyse et Modélisation pour la Biologie et l’Environnement, UMR 8587, CNRS-CEA-Université d’Evry Val d’Essonne, Evry, France
Andra, Chatenay Malabry, France
References (15)
Show source-provided references
1. 10.5006/1.331912910.5006/1.3319129 ↗
2. Crusset D · Corros Eng Sci Technol
3. Féron D · 2003
4. 10.1179/1743278210Y.000000001610.1179/1743278210Y.0000000016 ↗
5. 10.1179/1743278210Y.000000002110.1179/1743278210Y.0000000021 ↗
6. Parkins RN. A review of stress corrosion cracking of high pressure gas pipelines. NACE International Conference Corrosion 2000. Paper No. 00363.10.5006/C2000-00363 ↗
7. Beavers JA, Durr BS, Delanty BS, et al. Near-neutral pH SCC: crack propagation in susceptible soil environments. NACE International Conference Corrosion 2001. Paper No. 01217.10.5006/C2001-01217 ↗
8. 10.5006/1.328487610.5006/1.3284876 ↗
9. Danielson MJ, Jones RH. Effects of microstructure and microchemistry on the SCC behaviour of archival and modern pipeline steels in a high pH environment. NACE International Conference Corrosion 2001. Paper No. 01211.10.5006/C2001-01211 ↗
10. Elboujdaini M, Wang Z, Revie RW, et al. Stress crack initiation processes: pitting and microcrack coalescence. NACE International Conference Corrosion 2000. Paper No. 00379.10.5006/C2000-00379 ↗
11. Didot A. Corrosion sous contrainte des aciers non alliés dans les conditions du stockage géologique [PhD thesis]. France: Université Technologique de Compiègne; 2008 December 7.
12. 10.1016/j.ijhydene.2005.04.00710.1016/j.ijhydene.2005.04.007 ↗
13. 10.1016/S0010-938X(97)89248-710.1016/S0010-938X(97)89248-7 ↗
14. Kermani MB, Boucher C, Crolet JL, et al. Limites of linepipe weld harness for domains of sour service in oil and gaz production. NACE International CORROSION 2000. paper 00361.2000.10.5006/C2000-00157 ↗
15. Brass AM, Chene J, Coudreuse L. Fragilisation des aciers par l’hydrogène : mécanismes. Techniques de l’ingénieur, M175.