An attempt has been made to investigate the evolution of intergranular corrosion (IGC) resistance of HR3C heat-resistant austenitic stainless steel. The double-loop electrochemical potentiokinetic reactivation (DL-EPR) tests were conducted to evaluate the IGC resistance of HR3C steel. The results show that the side peaks can be observed in active–passive region of DL-EPR curves due to inhomogeneous distribution of the chromium dissolved in matrix. The variation of the degree of sensitisation (DOS) during sensitising at 800°C can be divided into three regions (sensitisation dominant region, desensitisation dominant region and equilibrium region). When HR3C steel is sensitised at 800°C for over 24 h, the equilibrium state in DOS can be reached. Simultaneously, the IGC morphologies after DL-EPR tests can correlate well with the DOS. On the basis of the equilibrium state in DOS, proper heat treatments and corrosion protection measures can be taken to avoid IGC of HR3C steel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan, PR China

Shanxi Institute of Technology, Yangquan, PR China

Funding

National Natural Science Foundation of China · Natural Science Foundation of Shanxi Province

References (21)

Show source-provided references
1. 10.1016/j.jmatprotec.2016.04.02610.1016/j.jmatprotec.2016.04.026 ↗
2. 10.1016/j.electacta.2008.08.04510.1016/j.electacta.2008.08.045 ↗
3. 10.1016/j.corsci.2006.01.00310.1016/j.corsci.2006.01.003 ↗
4. 10.1016/j.corsci.2015.08.02710.1016/j.corsci.2015.08.027 ↗
5. 10.1016/j.msea.2009.12.03910.1016/j.msea.2009.12.039 ↗
6. 10.1179/0960340915Z.00000000011910.1179/0960340915Z.000000000119 ↗
7. 10.1179/174892408X38286010.1179/174892408X382860 ↗
8. 10.1179/1743284713Y.000000034710.1179/1743284713Y.0000000347 ↗
9. 10.1016/j.matchemphys.2015.02.03010.1016/j.matchemphys.2015.02.030 ↗
10. 10.1016/0254-0584(84)90062-210.1016/0254-0584(84)90062-2 ↗
11. 10.1016/0010-938X(66)80014-810.1016/0010-938X(66)80014-8 ↗
12. 10.5006/1.358491810.5006/1.3584918 ↗
13. 10.1016/j.matchar.2007.04.00410.1016/j.matchar.2007.04.004 ↗
14. 10.1016/j.commatsci.2009.02.00810.1016/j.commatsci.2009.02.008 ↗
15. 10.1016/j.corsci.2010.02.01510.1016/j.corsci.2010.02.015 ↗
16. 10.5006/1.359383610.5006/1.3593836 ↗
17. ASTM A262 A · 2002
18. 10.1016/j.corsci.2008.10.01510.1016/j.corsci.2008.10.015 ↗
19. 10.5006/1.329207210.5006/1.3292072 ↗
20. 10.5006/1.329361010.5006/1.3293610 ↗
21. 10.1179/174328005X1434810.1179/174328005X14348 ↗