Crack initiation in tapered high Si stainless steel specimens – stress threshold analyses
Source abstract
Abstract
Tapered specimens were used for an accelerated test technique to study the crack initiation of high Si stainless steel by means of constant elongation rate tensile testing in a simulated pressurised water reactor environment. Detailed crack density distributions were obtained by applying an advanced crack detection algorithm on iteratively displaced scanning electron microscopy pictures featuring stress corrosion cracks along the specimen’s gauge length. By means of finite-element analysis, prominent peaks in the crack density graphs are demonstrated to be related to stress relief and stress build-up during the crack initiation phase. Intrinsic scatter related to the crack detection suggests that stress corrosion cracking is independent of the strain-rate for strain-rates lower than 10−6 s−1. Based on the extrapolation to constant load conditions, the critical threshold value for the duplex high Si stainless steel is estimated to be around 580 MPa.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Non-Destructive Testing Techniques · Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Studiecentrum voor Kernenergie/Centre d’Etude, de l’Energie Nuclèaire, SCK•CEN, Mol, Belgium,
Electron Microscopy for Materials Science – EMAT, University of Antwerp, Antwerpen, Belgium,
Funding
Electrabel
References (22)
Show source-provided references
1. Cattant F · 2014
2. 10.1016/S0022-3115(99)00075-610.1016/S0022-3115(99)00075-6 ↗
3. Rao AS. Degradation of LWR core internal materials owing to neutron irradiation, NUREG/CR-7027; 2010.
4. 10.5006/1.328058010.5006/1.3280580 ↗
5. 10.5006/1.327833110.5006/1.3278331 ↗
6. 10.5006/1.327848310.5006/1.3278483 ↗
7. 10.5006/080310.5006/0803 ↗
8. 10.3390/met710039210.3390/met7100392 ↗
9. 10.1016/j.jnucmat.2015.02.03810.1016/j.jnucmat.2015.02.038 ↗
10. 10.1080/18811248.2008.971189410.1080/18811248.2008.9711894 ↗
11. Conermann J, Shogan R, Fujimoto K, et al. Irradiation effects in a highly irradiated cold worked stainless steel removed from a commercial PWR. In: Proceedings of the 12th International Conference on Environmental Degradation of Materials in Nuclear Power System – Water Reactors, TMS, 2005, p. 277.
12. Zajec B, Hojná A, Bosch RW, et al. DELIVERABLE D6.2 – Applied experimental procedures, 2018.
13. 10.1080/1478422X.2017.134024510.1080/1478422X.2017.1340245 ↗
14. 10.1007/978-3-030-04639-2_13110.1007/978-3-030-04639-2_131 ↗
15. 10.1038/nmeth.201910.1038/nmeth.2019 ↗
16. Kilian R, Devrient B. Experimental data on crack initiation, FP6 project PERFECT deliverable C35c; 2008.
17. 10.1016/0257-8972(88)90113-210.1016/0257-8972(88)90113-2 ↗
18. 10.1080/02670836.2017.132008510.1080/02670836.2017.1320085 ↗
19. 10.1533/9781845693466.2.8710.1533/9781845693466.2.87 ↗
20. 10.1109/34.65993010.1109/34.659930 ↗
21. 10.2355/isijinternational.41.106810.2355/isijinternational.41.1068 ↗
22. 10.1016/j.jnucmat.2014.12.01410.1016/j.jnucmat.2014.12.014 ↗