The corrosion behaviour and mechanism of solid-state sintered silicon carbide ceramics in the mixed HF–HNO3 acid solution were investigated in this paper. The corrosion results of SiC in different corrosion medium demonstrated that the corrosion of ceramic was affected by the coefficient of HF and HNO3. In addition, the results of different corrosion time showed that the corrosion process can be divided into three stages: 0–6, 6–24, 24–96 h, which was also proved by the strength degradation of SiC after being corroded for different time. Because the relationship between mass loss and corrosion time was linear, the corrosion of first two stages was controlled by chemical reaction. Owing to the scattered data of mass loss in the third stage, the apparent activation is introduced to investigate the control mechanism. The corrosion results at different corrosion temperatures demonstrated that the corrosion mechanism was diffusion control in the third stage, and the apparent activation energy was 198.47 ± 13.97 kJ mol−1.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences, 1295 Ding xi Road, 200050 Shanghai, China

Department of Materials Science and Engineering, Shanghai University, 99 Shang da Road, 200444 Shanghai, China

Key Laboratory of Inorganic Functional Materials and Devices, Shanghai Institute of Ceramics, 1295 Ding xi Road, 200050 Shanghai, China

Funding

National Natural Science Foundation of China · Chinese Academy of Sciences

References (21)

Show source-provided references
1. 10.1016/j.jeurceramsoc.2005.12.00110.1016/j.jeurceramsoc.2005.12.001 ↗
2. 10.1016/j.jeurceramsoc.2006.05.08210.1016/j.jeurceramsoc.2006.05.082 ↗
3. 10.1016/j.jeurceramsoc.2003.07.01610.1016/j.jeurceramsoc.2003.07.016 ↗
4. 10.1016/S0955-2219(02)00280-710.1016/S0955-2219(02)00280-7 ↗
5. 10.1111/j.1151-2916.2000.tb01348.x10.1111/j.1151-2916.2000.tb01348.x ↗
6. 10.1111/j.1551-2916.2006.01401.x10.1111/j.1551-2916.2006.01401.x ↗
7. 10.1111/j.1551-2916.2011.04553.x10.1111/j.1551-2916.2011.04553.x ↗
8. 10.1179/00070599479826769210.1179/000705994798267692 ↗
9. 10.1111/j.1151-2916.1989.tb06217.x10.1111/j.1151-2916.1989.tb06217.x ↗
10. 10.1016/j.jeurceramsoc.2006.07.01110.1016/j.jeurceramsoc.2006.07.011 ↗
11. 10.1111/jace.1309610.1111/jace.13096 ↗
12. Budd S. M. · Phys. Chem. Glasses · 1961 · 2 · 111
13. Budd S. M. · Phys. Chem. Glasses · 1961 · 2 · 115
14. 10.1111/j.1151-2916.1987.tb05708.x10.1111/j.1151-2916.1987.tb05708.x ↗
15. 10.1111/j.1151-2916.1982.tb10471.x10.1111/j.1151-2916.1982.tb10471.x ↗
16. 10.1023/A:101864362686710.1023/A:1018643626867 ↗
17. 10.1111/jace.1340910.1111/jace.13409 ↗
18. 10.1111/j.1151-2916.1993.tb03684.x10.1111/j.1151-2916.1993.tb03684.x ↗
19. 10.1016/0955-2219(92)90010-B10.1016/0955-2219(92)90010-B ↗
20. 10.1063/1.171394510.1063/1.1713945 ↗
21. 10.1103/RevModPhys.57.43710.1103/RevModPhys.57.437 ↗