journal article·2011-02

Corrosion behaviour of direct current and active screen plasma carburised AISI 316 stainless steel in boiling sulphuric acid solutions

S Corujeira Gallo, H Dong

Publisher page

Abstract

Active screen plasma is a recently developed plasma surface alloying technique, which has shown potential for addressing some drawbacks associated with conventional direct current plasma processes. In this study, the corrosion performance of untreated, direct current and active screen plasma carburised AISI 316 was investigated by immersion in a boiling solution of sulphuric acid. The experimental results show that the corrosion behaviour of expanded austenite produced by low temperature plasma carburising is controlled by the type and density of surface defects; the corrosion properties of the active screen plasma carburised material are superior to that produced by direct current plasma because of the significantly reduced edge effect and surface defects; and the bias level used in the active screen carburising treatment has a profound effect on the corrosion performance of the material. Based on the experimental results, the corrosion mechanisms involved are discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. 10.1016/0257-8972(93)90124-710.1016/0257-8972(93)90124-7 ↗
2. 10.1179/02670849932291164710.1179/026708499322911647 ↗
3. 10.1016/S0257-8972(01)01136-710.1016/S0257-8972(01)01136-7 ↗
4. Edenhofer B · Heat Treat. Met · 1991 · 1 · 6
5. 10.1016/0261-3069(84)90083-910.1016/0261-3069(84)90083-9 ↗
6. 10.1116/1.56994310.1116/1.569943 ↗
7. 10.1023/B:MSAT.0000048840.94386.2510.1023/B:MSAT.0000048840.94386.25 ↗
8. 10.1016/0257-8972(93)90069-Z10.1016/0257-8972(93)90069-Z ↗
9. Georges J · 1999
10. 10.1179/02670840322500620310.1179/026708403225006203 ↗
11. 10.1016/j.msea.2006.05.12210.1016/j.msea.2006.05.122 ↗
12. 10.1179/02670830322500792410.1179/026708303225007924 ↗
13. 10.1016/j.corsci.2003.09.01510.1016/j.corsci.2003.09.015 ↗
14. 10.1149/1.242730410.1149/1.2427304 ↗
15. Monypenny JHG: ‘Stainless iron and steel’, 3rd ed, Vol. 1, 228–359, 523; 1951, London, Chapman and Hall.
16. 10.1016/0261-3069(91)90091-H10.1016/0261-3069(91)90091-H ↗
17. 10.1016/j.actamat.2006.09.04910.1016/j.actamat.2006.09.049 ↗
18. 10.1179/174328405X4753710.1179/174328405X47537 ↗
19. 10.1179/174328407X21324210.1179/174328407X213242 ↗
20. 10.1016/j.surfcoat.2006.01.08010.1016/j.surfcoat.2006.01.080 ↗
21. 10.1016/j.surfcoat.2004.08.09910.1016/j.surfcoat.2004.08.099 ↗
22. 10.1016/j.matchar.2004.11.00410.1016/j.matchar.2004.11.004 ↗
23. 10.1016/j.actamat.2006.06.03010.1016/j.actamat.2006.06.030 ↗
24. 10.1016/j.actamat.2006.03.04810.1016/j.actamat.2006.03.048 ↗
25. 10.1016/S1359-6454(02)00306-310.1016/S1359-6454(02)00306-3 ↗
26. 10.1179/02670840222500627710.1179/026708402225006277 ↗
27. 10.1016/S0257-8972(96)03099-X10.1016/S0257-8972(96)03099-X ↗