Indoor atmospheric corrosion of copper and steel under heat trap conditions in Cuban tropical climate
Source abstract
Abstract
Corrosion behaviour of copper and steel under heat trap conditions in Cuban tropical climate is reported. Temperature and humidity reach higher values than those reported for traditional outdoor and indoor conditions. Annual calculated time of wetness is in the range corresponding to outdoor or ventilated sheds. This behaviour is not reported for other indoor conditions. Sulphur compounds deposition rate is higher than chloride deposition rate at all corrosion stations. Main corrosion products formed on steel and copper are goethite and brochantite respectively. No significant differences in the statistical influence of exposure time and time of wetness on atmospheric corrosion process of copper and steel under heat trap conditions are determined.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Smart Materials for Construction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Rocha J: ‘Productos electro-electrónicos en ambientes tropicales’, 95–162; 2003, Sao Paulo, Sitta Gráfica Campinas.
2. 10.1016/j.corsci.2006.06.00210.1016/j.corsci.2006.06.002 ↗
3. Cerrad Sánchez SM · Ing. Invest. Tecnol. · 2005 · 4 · 219
4. 10.1016/j.corsci.2007.06.01210.1016/j.corsci.2007.06.012 ↗
5. ‘Corrosion of metals and alloys – classification of corrosivity of atmospheres’, ISO 9223, International Organization for Standardization, Geneva, Switzerland, 1992.
6. 10.1016/j.corsci.2007.06.01110.1016/j.corsci.2007.06.011 ↗
7. Martín Y, Corvo F, Reguera E: Proc. on 9th Congreso Iberoamericano de Metalurgia y Materiales, Ciudad de La Habana, Cuba, Octubre 2006, Palacio de Convenciones, pp. 1258–1272.
8. Martín Y · Revista CENIC Ciencias Químicas · 2007 · 38 · 219
9. ‘Environmental conditions and environmental test for telecommunication equipment – classification of environmental conditions’, ETS 300 019-1-3 a 1-7, 1992.
10. ‘Corrosion of metals and alloys – classification of low corrosivity of indoor atmospheres – determination of corrosion attack’, ISO 11844-2, International Organization for Standardization, Geneva, Switzerland, 2003.
11. ‘Corrosion of metals and alloys – corrosivity of atmosphere – Measurements of pollution’, ISO 9225-92, International Organization for Standardization, Geneva, Switzerland, 1992.
12. 10.1007/BF0118623810.1007/BF01186238 ↗
13. ‘Corrosion of metals and alloys – classification of atmospheres with low corrosivity – determination and estimation of corrosivity’, ISO 11844-1, International Organization for Standardization, Geneva, Switzerland, 2000.
14. 10.1016/0010-938X(95)00058-R10.1016/0010-938X(95)00058-R ↗
15. Corvo F, Betancourt M, González E, Pérez J: Proc. Workshop on ‘Atmospheric corrosion and weathering steels’, Cartagena de India, Col., USA, September 2004, University of Autioquia, pp. 54–63.
16. Corvo F, Rocha J: Proc. Int. Conf. on ‘Corrosion’, Granada, Spain, September 2002, NACE, pp. 596–602.
17. 10.1016/j.corsci.2003.09.01410.1016/j.corsci.2003.09.014 ↗
18. 10.1016/j.corsci.2005.09.01110.1016/j.corsci.2005.09.011 ↗
19. 10.1016/j.corsci.2003.07.00110.1016/j.corsci.2003.07.001 ↗
20. 10.1179/174327808X28627510.1179/174327808X286275 ↗
21. Antunes A, Costa I: Proc. Workshop on ‘Atmospheric corrosion and weathering steels’, Cartagena de India, Col., USA, September 2004, University of Autioquia, pp. 1021–1031.
22. Pourbaix M: Proc. 11th Int. Conf. on ‘Metallic corrosion’, Florence, Italy, April 1990, NACE, pp. 67–73.
23. 10.1016/0010-938X(93)90113-U10.1016/0010-938X(93)90113-U ↗
24. 10.1016/S0261-3069(01)00051-610.1016/S0261-3069(01)00051-6 ↗
25. 10.1016/S0010-938X(01)00097-X10.1016/S0010-938X(01)00097-X ↗
26. Esmanhoto EJ, Kenny ED: Proc. 17th Int. Conf. on ‘Congresso brasileiro de corrosão’, Vol. 23, 283–296; 1993, Rio de Janeiro, ABRACO.