journal article·2010-06

Corrosion characteristics of electroless Ni–P coatings deposited on W–Cu composite

H. J. Chen, L. L. Wang, W. Q. Huang, L. Hao

Publisher page

Abstract

Electroless Ni–P coatings were deposited on W–Cu composite substrates using an anodic activation and strike nickel plating pre-treatments; they were then subjected to heat treatment. The morphology and structure of Ni–P coatings were examined using SEM and XRD, also the corrosion characteristics of Ni–P coatings in 3·5 wt-% NaCl solution were investigated by electrochemical tests. Results indicated that the heat treatment temperature affected the surface morphology, structure and corrosion resistance of Ni–P coatings. The weight loss results indicated that the Ni–P coating had a smaller corrosion rate than W–Cu composite in 3·5 wt-% NaCl solution.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Semiconductor materials and interfaces · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Chemistry and Chemical Engineering, Xinyang Normal University, Xinyang 464000, China

Anhui Vocational & Technical College of Industry & Trade Huainan 23200, China

Environmental Corrosion Centre, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

References (25)

Show source-provided references
1. SebastianK. V.: Int. J. Powder Metall. Powder Technol., 1981 17 297.
2. GermanR. M. HensK.F. and JohnsonJ.L.: Int. J. Powder Metall., 1994 30 205.
3. 10.1016/S0263-4368(02)00003-310.1016/S0263-4368(02)00003-3 ↗
4. 10.1016/S0167-577X(03)00071-510.1016/S0167-577X(03)00071-5 ↗
5. 10.1016/S0925-8388(01)01805-910.1016/S0925-8388(01)01805-9 ↗
6. 10.1016/S1359-6462(03)00244-610.1016/S1359-6462(03)00244-6 ↗
7. 10.1016/j.matlet.2003.08.03510.1016/j.matlet.2003.08.035 ↗
8. LiX. W. ChenZ. L. HouH. B.: Corros. Eng. Sci. Technol., In press. DOT 10.1179/147842208X386368.
9. 10.1016/S0257-8972(03)00746-110.1016/S0257-8972(03)00746-1 ↗
10. 10.1016/0001-6160(75)90010-310.1016/0001-6160(75)90010-3 ↗
11. 10.1016/S0925-8388(01)01805-910.1016/S0925-8388(01)01805-9 ↗
12. 10.1016/j.msea.2005.04.01010.1016/j.msea.2005.04.010 ↗
13. 10.1016/j.scriptamat.2004.06.01410.1016/j.scriptamat.2004.06.014 ↗
14. 10.1179/pom.2000.43.1.7910.1179/pom.2000.43.1.79 ↗
15. YangB. and GermanR. M.: Int. J. Powder Metall., 1997 35 55.
16. ZhangD. L.: Prog. Mater. Sci 200449–537.
17. GaffetE. LousionC. HarmelinM. and FaudotF: Mater. Sci. Eng. A 1991 A276 1380.
18. 10.1016/S0079-6425(99)00010-910.1016/S0079-6425(99)00010-9 ↗
19. 10.1179/174329408X32637110.1179/174329408X326371 ↗
20. ‘Standard practice for laboratory immersion corrosion testing of metals’ ASTM G31–72ASTM West Conshohocken PA 1995.
21. 10.1016/S0257-8972(01)01492-X10.1016/S0257-8972(01)01492-X ↗
22. 10.1016/S0257-8972(00)00864-110.1016/S0257-8972(00)00864-1 ↗
23. 10.1016/S0257-8972(01)01337-810.1016/S0257-8972(01)01337-8 ↗
24. 10.1016/j.corsci.2004.12.00210.1016/j.corsci.2004.12.002 ↗
25. 10.1023/A:101849740136510.1023/A:1018497401365 ↗