Long term integrity of overpack closure weld for HLW geological disposal Part 2 – corrosion properties under anaerobic conditions
Source abstract
Abstract
The corrosion behaviour of a carbon steel weld joint under anaerobic conditions was investigated to estimate the long term integrity of the carbon steel overpack. The welded specimens in this study were prepared using three different welding methods: gas tungsten arc welding, gas metal arc welding and electron beam welding. General corrosion was observed for each immersion specimen, and the corrosion rate at the weld joint was the same as or less than that of the base metal. The concentration of hydrogen that absorbed during immersion testing was <2·48×10−5 mol kg[Fe]−1 (0·05 ppm) after 3 years, a value regarded as having little influence on hydrogen embrittlement. The susceptibility to hydrogen embrittlement was the highest in the base metal, suggesting that there was little adverse effect on the weld joint from welding. The welded carbon steel overpack is assumed to maintain its resistance to corrosion as a disposal container for the expected lifetime under anaerobic underground conditions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. ‘H12: project to establish the scientific and technical basis for HLW disposal in Japan’, JNC TN1410 2000-3, JNC, Ibaraki, Japan, 2000.
2. 10.1179/1743278210Y.000000001110.1179/1743278210Y.0000000011 ↗
3. 10.1080/18811248.2004.972642410.1080/18811248.2004.9726424 ↗
4. 10.1080/18811248.2008.971149110.1080/18811248.2008.9711491 ↗
5. 10.1080/18811248.2006.971108310.1080/18811248.2006.9711083 ↗
6. Taniguchi N, Honda A, Kawasaki M, Tsuru T: ‘The Assessment of Corrosion Type and Corrosion Rate of Carbon Steel in Compacted Bentonite) JNC TN8400 99-003, JNC, Ibaraki, Japan, 1999.
7. Nagmo M: ‘Fundamentals of hydrogen embrittlement’, 117; 2008; Tokyo, Uchida Rokakuho Publishing.
8. 10.2355/isijinternational.43.52010.2355/isijinternational.43.520 ↗
9. Matsuyama S · Nikkan Kogyo Shimbun · 1989 · 70
10. 10.2355/isijinternational.50.11510.2355/isijinternational.50.115 ↗
11. Hinotani S · Tetsu-to-Hagane · 1984 · 70 · 42010.2355/tetsutohagane1955.70.3_420 ↗
12. ‘H21: development on the performance of engineering barrier system (1/2)’, Radioactive Waste Management Funding and Research Center (RWMC), Tokyo, Japan, 2010.