The influence of different locations on copper corrosion with different external electric fields under a chloride-containing thin electrolyte layer
Source abstract
Abstract
The influence of different locations on copper corrosion with different external electric fields under a chloride-containing thin electrolyte layer was studied using polarisation curve measurement and surface analysis techniques. The results indicated that, under an external direct current electric field, the anodic current densities near the positive plate were smaller than that near the negative plate, while the cathodic current densities near the positive plate were larger than that near the negative plate. However, at different locations in an external alternating current electric field, the anodic current densities were little change, while the cathodic current densities were obviously different.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures · Electrodeposition and Electroless Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Chemistry and Environmental Engineering, Key Laboratory of Green Chemical Process of Ministry of Education, Key Laboratory of Novel Reactor and Green Chemical Technology of Hubei Province, Wuhan Institute of Technology, Wuhan, People’s Republic of China
Funding
China National Funds for Distinguished Young Scientists · Graduate Student Innovation Foundation of Wuhan Institute of Technology · National Natural Science Foundation of Hubei
References (25)
Show source-provided references
1. 10.1016/j.corsci.2009.11.00310.1016/j.corsci.2009.11.003 ↗
2. 10.1016/j.corsci.2006.12.01310.1016/j.corsci.2006.12.013 ↗
3. 10.1016/j.corsci.2005.09.01110.1016/j.corsci.2005.09.011 ↗
4. 10.1126/science.234.4774.34010.1126/science.234.4774.340 ↗
5. 10.1016/j.corsci.2015.08.02210.1016/j.corsci.2015.08.022 ↗
6. 10.1016/j.electacta.2014.07.16010.1016/j.electacta.2014.07.160 ↗
7. 10.1016/j.corsci.2011.06.00410.1016/j.corsci.2011.06.004 ↗
8. 10.1016/j.corsci.2006.06.02210.1016/j.corsci.2006.06.022 ↗
9. 10.1016/j.electacta.2006.01.05810.1016/j.electacta.2006.01.058 ↗
10. 10.1016/S0010-938X(73)80010-110.1016/S0010-938X(73)80010-1 ↗
11. 10.1016/S0010-938X(02)00257-310.1016/S0010-938X(02)00257-3 ↗
12. 10.1016/S1003-6326(14)63059-410.1016/S1003-6326(14)63059-4 ↗
13. 10.1016/j.corsci.2013.05.01910.1016/j.corsci.2013.05.019 ↗
14. 10.1016/j.corsci.2011.04.01710.1016/j.corsci.2011.04.017 ↗
15. 10.1080/1478422X.2018.147125010.1080/1478422X.2018.1471250 ↗
16. 10.1080/1478422X.2017.138601710.1080/1478422X.2017.1386017 ↗
17. 10.1179/1743278213Y.000000010010.1179/1743278213Y.0000000100 ↗
18. 10.1016/j.matchemphys.2016.06.06410.1016/j.matchemphys.2016.06.064 ↗
19. 10.1016/S1003-6326(16)64414-X10.1016/S1003-6326(16)64414-X ↗
20. 10.1016/j.corsci.2013.11.01210.1016/j.corsci.2013.11.012 ↗
21. 10.1149/1.210833510.1149/1.2108335 ↗
22. 10.1080/1478422X.2018.154475910.1080/1478422X.2018.1544759 ↗
23. 10.1007/s11664-017-5727-y10.1007/s11664-017-5727-y ↗
24. 10.1007/s11664-017-5395-y10.1007/s11664-017-5395-y ↗
25. 10.1149/1.183842210.1149/1.1838422 ↗