journal article·2017-09

Study on the impact toughness and diffusible hydrogen of G105 drill pipe steel in wet H 2 S environment

Bensheng Huang, Hao Peng, Xiang Chen, Chenglong Gong, Jiachen Li

Publisher page

Abstract

In order to investigate the influence of wet H 2 S environment on impact toughness of G105 drill pipe steel, the impact test of drill pipe exposed to NACE A solution for different time was carried out. Meanwhile, the diffusible hydrogen concentration was measured to study the relationship between diffusible hydrogen and impact toughness damage. The results suggest that with the increase of corrosion time, the impact energy of G105 drill pipes decreases from 107.7 to 88.4 J, and the dynamic fracture toughness decreases gradually. The impact toughness damage increases as the diffusion hydrogen concentration increases. However, the impact energy recovery happened after hydrogen releasing. The quasi-cleavage features occur with the increasing of hydrogen concentration.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering, Southwest Petroleum University, Chengdu, China

Funding

Key Laboratory of Ministry of Education of Oil & Gas Equipment · Key Projects of Sichuan Provincial Education Department · Key Laboratory of Material of Oil & Gas Sichuan Province Education Department

References (24)

Show source-provided references
1. 10.1002/maco.20140817410.1002/maco.201408174 ↗
2. 10.1016/j.corsci.2008.03.00710.1016/j.corsci.2008.03.007 ↗
3. LiuM WangJQ KeW . Corrosion behavior of X52 anti-H2S pipeline steel in high H2S concentration solutions at temperatures ranging from 25°Cto140°C. J Mater Sci Technol. 2013; 48: 380–387.
4. 10.1016/j.matdes.2016.03.03610.1016/j.matdes.2016.03.036 ↗
5. 10.1016/j.corsci.2011.03.01710.1016/j.corsci.2011.03.017 ↗
6. ChoiYS HassaniS VuTN . Abas AZB, effect of H2S on the corrosion behaviour of pipeline steels in supercritical and liquid CO2 environments. Corros. 2016; 71: 999–1009.10.5006/2026 ↗
7. 10.1016/j.corsci.2016.06.00310.1016/j.corsci.2016.06.003 ↗
8. 10.20964/11035510.20964/110355 ↗
9. 10.1016/j.corsci.2012.04.01210.1016/j.corsci.2012.04.012 ↗
10. 10.1016/j.corsci.2012.11.03810.1016/j.corsci.2012.11.038 ↗
11. 10.1016/j.corsci.2008.09.03010.1016/j.corsci.2008.09.030 ↗
12. 10.1016/S0079-6425(02)00014-210.1016/S0079-6425(02)00014-2 ↗
13. 10.1016/j.corsci.2010.12.01110.1016/j.corsci.2010.12.011 ↗
14. 10.1016/j.ijhydene.2010.05.08910.1016/j.ijhydene.2010.05.089 ↗
15. 10.5006/1.329027810.5006/1.3290278 ↗
16. 10.5006/0010-9312-36.11.62510.5006/0010-9312-36.11.625 ↗
17. 10.5006/0010-9312-32.8.32110.5006/0010-9312-32.8.321 ↗
18. 10.1016/j.msea.2005.10.02110.1016/j.msea.2005.10.021 ↗
19. HuangBS ChenX HuangLP. Changes of microstructure and properties of G105 drill pipe in H2S environment. Mater Sci. 2015; 814: 303–312.
20. 10.1016/j.colsurfa.2016.05.01810.1016/j.colsurfa.2016.05.018 ↗
21. 10.3390/ma903020010.3390/ma9030200 ↗
22. SchindlerHJ. Estimation of the dynamic J-R-curve from a single impact bending test mechanisms and mechanics of damage and failure. Vol. 33. New York: W. W. Norton; 1991. p. 245–278.
23. 10.1016/S0997-7538(01)01179-210.1016/S0997-7538(01)01179-2 ↗
24. ChuWY. Hydrogen damage and delayed cracking. Beijing: Metallurgical Industry Publishers; 1988.