Corrosion of iron in liquid uranium hexafluoride
Source abstract
Abstract
Here is reported a dedicated and reliable experimental setup which has been designed to study the corrosive effects of liquid uranium hexafluoride (UF6) on pure metallic iron at 80°C and 3 bars of pressure. Three corrosion tests have been carried out, ranging from several hundred to almost one thousand hours. No uniform corrosion was observed on early-stage samples. However, a nodule facies consisting in FeF2 and UFx (with 4 < x < 5) deposits is observed at the surface of the iron samples. These FeF2 nodules grow with time and merge, leading finally to the formation of an almost continuous FeF2 layer. The thickness of the layer over time seems to follow a parabolic kinetics law, finally reaching 15 µm after about one thousand hours of immersion in liquid UF6. After the nodules have merged, many cracks can be observed in the FeF2 layer, probably due to the growing stresses as the corrosion layer is formed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
AREVA, Hall de Recherche de Pierrelatte, Chemistry and Enrichment Division, Pierrelatte, France
CEA, DEN, Service de la Corrosion et du Comportement des Matériaux dans leur Environnement (SCCME), CEA, Université Paris-Saclay, Gif-sur-Yvette, France
Institut de Chimie de Clermont Ferrand, Aubière, France
New Areva Holding, DRD, Paris la Défense, France
Institut de Physique Nucléaire, Orsay, France
References (5)
Show source-provided references
1. 10.1007/978-3-662-02293-110.1007/978-3-662-02293-1 ↗
2. Agron P · 1948
3. Leitnaker JM. · High Temp Sci. · 1980 · 12 · 289
4. Pilling NB · J Inst Met. · 1923 · 29 · 529
5. 10.1107/S010876818900766410.1107/S0108768189007664 ↗