journal article·2024-08

Corrosion behaviour of FeCoNiCrAl high-entropy alloy in molten NaCl–KCl–MgCl 2 chloride salt

Huayi Lu, Sen Li, Yanli Wang

Publisher page

Abstract

Molten NaCl–KCl–MgCl 2 is becoming a potential heat transfer fluid (HTF) and thermal energy storage (TES) material in the third generation of concentrated solar energy power (CSP) stations due to its excellent heat storage-capacity and thermal stability. However, the strong corrosion of the molten chloride salt at high temperature limits its industrial application. In this study, the corrosion behaviour of FeCoNiCrAl HEA with BCC + FCC phase structure in molten NaCl–KCl–MgCl 2 (24.5–20.55–54.95 wt-%) at 650 °C under argon was investigated by a combination of weight loss and electrochemical methods. The results show that, the corrosion of FeCoNiCrAl HEA in molten chloride salt mainly manifests as the selective dissolution of Fe and Cr. With the further increase of immersion time, oxides gradually crack and slightly flake, resulting in large weight loss of FeCoNiCrAl HEA.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Phase Change Materials Research · High Entropy Alloys Studies · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Guangxi Key Laboratory of Electrochemical Energy Materials, School of Chemistry and Chemical Engineering, Guangxi University, Nanning, PR China

Funding

Natural Science Foundation of Guangxi Province

References (26)

Show source-provided references
1. 10.1016/j.apenergy.2022.11970810.1016/j.apenergy.2022.119708 ↗
2. 10.1016/j.enconman.2022.11622210.1016/j.enconman.2022.116222 ↗
3. 10.1016/j.solmat.2020.11067510.1016/j.solmat.2020.110675 ↗
4. 10.1016/j.solmat.2019.02.01210.1016/j.solmat.2019.02.012 ↗
5. 10.1016/j.solmat.2023.11223310.1016/j.solmat.2023.112233 ↗
6. 10.1016/j.eng.2020.06.02710.1016/j.eng.2020.06.027 ↗
7. 10.1016/j.rser.2013.11.01010.1016/j.rser.2013.11.010 ↗
8. 10.1016/j.solmat.2016.05.05210.1016/j.solmat.2016.05.052 ↗
9. 10.1002/adem.20030056710.1002/adem.200300567 ↗
10. 10.1016/j.actamat.2016.08.08110.1016/j.actamat.2016.08.081 ↗
11. 10.1016/j.mattod.2015.11.02610.1016/j.mattod.2015.11.026 ↗
12. 10.1016/j.jmst.2022.08.04610.1016/j.jmst.2022.08.046 ↗
13. 10.1016/j.solmat.2021.11122210.1016/j.solmat.2021.111222 ↗
14. 10.3390/e2502029610.3390/e25020296 ↗
15. 10.1016/j.solener.2016.05.03010.1016/j.solener.2016.05.030 ↗
16. 10.1016/j.corsci.2016.02.01010.1016/j.corsci.2016.02.010 ↗
17. LI Y · Corros Sci Prot Technol · 2000 · 12 · 41
18. 10.1016/j.solmat.2021.11155710.1016/j.solmat.2021.111557 ↗
19. 10.1016/j.solmat.2022.11173710.1016/j.solmat.2022.111737 ↗
20. 10.1016/j.solmat.2018.06.04410.1016/j.solmat.2018.06.044 ↗
21. 10.1016/j.solmat.2020.11076810.1016/j.solmat.2020.110768 ↗
22. 10.1063/1.511760110.1063/1.5117601 ↗
23. 10.2172/105173210.2172/1051732 ↗
24. 10.1016/S0010-938X(99)00142-010.1016/S0010-938X(99)00142-0 ↗
25. 10.1016/j.solmat.2018.12.02010.1016/j.solmat.2018.12.020 ↗
26. 10.1016/j.corsci.2020.10918310.1016/j.corsci.2020.109183 ↗