Effect of hydrocarbon volume ratio in sweet top-of-the-line corrosion under water-hydrocarbon co-condensation
Source abstract
Abstract
Wet gas pipelines transport unprocessed natural gas that contains water and carbon dioxide (CO 2 ), which combination can lead to severe wall loss caused by CO 2 or sweet corrosion in carbon steel. Under specific conditions, CO 2 corrosion occurs at the top section of the pipeline, which is known as top-of-the-line corrosion (TLC). TLC tests were conducted in the water-hydrocarbon co-condensation environment using 10 vol% n-heptane and 25 vol% n-heptane to simulate the internal condition of a wet gas pipeline to study the effect of hydrocarbon volume ratio towards TLC. The presence of n-heptane showed minimal effect on the gas temperature profile; however, n-heptane suppressed the water condensation, resulting in a tremendous decrease in the water condensation rate (WCR). The TLC rates were found to be lower in the presence of n-heptane, which can be attributed to the reduced WCR and water-wetted areas. The presence of n-heptane had no significant effect on the pitting rates but showed an increasing pit ratio as the n-heptane volume increased. TLC tests were conducted at three durations: one day, two days and three days showing that n-heptane has no significant effect on corrosion kinetics.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Chemical Engineering, College of Engineering, Universiti Teknologi MARA, Shah Alam, Selangor, Malaysia
Industrial Corrosion Research Center (InCORE), School of Chemical Engineering, College of Engineering, Universiti Teknologi MARA, Shah Alam, Selangor, Malaysia
Department of Applied Physics, Faculty of Science and Technology, Universiti Kebangsaan Malaysia, Bangi, Selangor, Malaysia
Funding
Kementerian Pendidikan Malaysia
References (20)
Show source-provided references
1. Pipeline and riser loss of containment 2001 - 2012 (PARLOC 2012) . London, UK, 2015.
2. Report 2013-B: pipeline performance in Alberta, 1990–2012 . Calgary, Alberta, 2013.
3. Annual report for pipeline mileage and facilities, https://www.phmsa.dot.gov/data-and-statistics/pipeline/pipeline-mileage-and-facilities (2021, accessed 8 December 2022).
4. Gunaltun YM, Supriyatman D, Achmad J. Top of the line corrosion in multiphase gas lines: a case history. In: Corrosion 99 , San Antonio, TX, 25–30 April 1999, pp.36. Houston, TX: NACE.
5. Larrey D · 2000 · 0071
6. 10.5006/222210.5006/2222 ↗
7. 10.1016/B978-0-08-101105-8.00016-410.1016/B978-0-08-101105-8.00016-4 ↗
8. Nyborg R, Dugstad A. Top of the line corrosion and water condensation rates in wet gas pipelines. In: NACE corrosion conference & expo 2007 , Nashville, TN, 11–15 March 2007, p.07555. Houston, TX: NACE.
9. 10.1016/B978-0-12-809570-6.00004-710.1016/B978-0-12-809570-6.00004-7 ↗
10. Jufri FSM · 2022 · 167
11. 10.4028/p-60952910.4028/p-609529 ↗
12. Pojtanabuntoeng T. Influence of water/hydrocarbon co-condensation on top of the line corrosion . Ohio University, 2012.
13. Pojtanabuntoeng T, Singer M, Nesic S. Water/hydrocarbon co-condensation and the influence on top-of-the-line corrosion. In: NACE international corrosion conference & expo, 2011, p.11330. NACE International.
14. ASTM International. ASTM G01-03 standard practice for preparing, cleaning, and evaluating corrosion tests specimens . West Conshohocken, PA, 2011.
15. ASTM International. ASTM G46-94 standard guide for examination and evaluation of pitting corrosion . West Conshohocken, PA, 2018.
16. API. Line pipe API specification 5L, 46th Edition, April 2018. Washington, DC, 2018.
17. 10.1520/G0031-12A10.1520/G0031-12A ↗
18. 10.5006/356910.5006/3569 ↗
19. HACH Iron, total, FerroVer method . 2014.
20. Yang X · J Trop Oceanogr · 2018 · 37 · 86