In the present paper, an investigation was carried out to understand the microstructure or secondary phase changes formed during thermal ageing at nose temperature (where Cr diffusion was faster) and its influence on the pitting corrosion behaviour of type 316LN SS with marginally lower Cr in as-received (AR) and 10% cold work (CW). X-ray diffraction studies confirmed Cr23C6 and Cr2N in AR and CW conditions. On thermal ageing, AR material from 0 to 10 h and CW from 10 to 24 h, although with lower Cr, the degree of sensitisation (DOS) and pitting potential (Epit) were insignificant due to nitrogen where as above 10 h in AR condition and below 10 h in CW condition resulted reductions in pitting potential (Epit) in different chloride mediums. These results provide new insights on the interplay between pitting, microstructures, alloying elements.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Corrosion Science and Technology Division, Metallurgy and Materials Group, Indira Gandhi Centre for Atomic Research, Kalpakkam, India
HomiBhaba National Institute, Kalpakkam, India
References (34)
Show source-provided references
1. 10.1002/srin.20180008710.1002/srin.201800087 ↗
2. 10.1016/j.jnucmat.2015.06.06010.1016/j.jnucmat.2015.06.060 ↗
3. 10.1080/1478422X.2015.110406510.1080/1478422X.2015.1104065 ↗
4. Harish Kumar D · Int J Mech Eng Robot Res · 2013 · 2 · 1
5. Singh M · Int J Sci Technol Res · 2019 · 8 · 2023
6. 10.20964/2018.07.7410.20964/2018.07.74 ↗
7. 10.1007/s11661-019-05623-010.1007/s11661-019-05623-0 ↗
8. Loto C · Int J Electrochem Sci · 2012 · 7 · 378710.1016/S1452-3981(23)13997-6 ↗
9. 10.5006/0010-9312-36.10.56510.5006/0010-9312-36.10.565 ↗
10. 10.1016/0010-938X(80)90054-210.1016/0010-938X(80)90054-2 ↗
11. 10.1016/0022-3115(94)90334-410.1016/0022-3115(94)90334-4 ↗
12. 10.1007/s11665-021-05454-410.1007/s11665-021-05454-4 ↗
13. 10.1016/j.jnucmat.2020.15257210.1016/j.jnucmat.2020.152572 ↗
14. 10.1007/s11661-011-1053-910.1007/s11661-011-1053-9 ↗
15. Pradhan SK · Corros Sci · 2018 · 158 · 1
16. 10.1016/S0022-3115(99)00255-X10.1016/S0022-3115(99)00255-X ↗
17. 10.31399/asm.fach.v02.c900134910.31399/asm.fach.v02.c9001349 ↗
18. Kasiviswanathan KV · 2003
19. 10.4028/www.scientific.net/AMR.794.67010.4028/www.scientific.net/AMR.794.670 ↗
20. 10.1007/BF0264765910.1007/BF02647659 ↗
21. 10.1007/BF0075226810.1007/BF00752268 ↗
22. ASTM A262-14. Standard practices for detecting susceptibility to intergranular attack in austenitic stainless steel. West Conshohocken (PA); 2014. p. 1–24.
23. 10.1016/j.corsci.2003.09.02010.1016/j.corsci.2003.09.020 ↗
24. 10.30544/12710.30544/127 ↗
25. Lai J.K.L. · 1983 · 61 · 101
26. 10.5006/1.358394510.5006/1.3583945 ↗
27. 10.1021/acsaem.9b0196510.1021/acsaem.9b01965 ↗
28. 10.1533/9780857094018.10610.1533/9780857094018.106 ↗
29. 10.1149/1.183861510.1149/1.1838615 ↗
30. Christionpisteoius P. Stability and metastability of corrosion pits on SS. Ph.D thesis, Cambridge University; 1991. p. 1–41.
31. 10.2298/CICEQ110406032A10.2298/CICEQ110406032A ↗
32. 10.5006/0010-9312-31.1.3010.5006/0010-9312-31.1.30 ↗
33. Merezhka D · 2018 · 1125
34. Sedricks AJ. · 1979