Abstract

Nickel-based alloy Inconel 617 is a candidate material for advanced ultra-supercritical units. Stress corrosion cracking (SCC) susceptibility of Inconel 617 under low-pressure superheated steam (0.1 MPa), high-pressure superheated steam (8 MPa) and supercritical water (25 MPa) at 650 °C was studied through slow strain rate tensile tests at strain rate of 5 × 10 −7 s −1 . The results indicate that Inconel 617 is susceptible to SCC in both superheated steam and supercritical water, with susceptibility increasing with pressure. In a nitrogen atmosphere, fractures were predominantly transgranular ductile. The fracture surface featured dimples and micropores. In three corrosive environments, both intergranular and transgranular fractures were observed. The rock sugar-like morphology becomes more and more obvious as the pressure increases. A large number of cracks perpendicular to the loading axis were found on gauge surface. The SCC mechanism for Inconel 617 in superheated steam and supercritical water conditions is internal oxidation.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · High-Temperature Coating Behaviors · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Thermal Power Engineering Technology Research Center, North China Electric Power University, Beijing, PR China

Funding

Natural Science Foundation of Hebei Province · National Natural Science Foundation of China · China Postdoctoral Science Foundation · National Key Research and Development Program of China

References (63)

Show source-provided references
1. 10.1016/j.ijfatigue.2021.10651810.1016/j.ijfatigue.2021.106518 ↗
2. Nicol K · 2013
3. Zhang NQ · J Chin Soc Corros Prot · 2017 · 37 · 9
4. Gianfrancesco AD · 2016
5. 10.1016/j.proeng.2013.03.24710.1016/j.proeng.2013.03.247 ↗
6. 10.1016/j.fuel.2012.11.08110.1016/j.fuel.2012.11.081 ↗
7. 10.1016/j.ijpvp.2006.08.00610.1016/j.ijpvp.2006.08.006 ↗
8. Yang HC · Power Equip · 2012 · 26 · 355
9. Jiang H · World Iron Steel · 2014 · 14 · 26
10. Wang TJ · Dongfang Turbine · 2012 · 2 · 46
11. Wang TJ, Fan H, Zhang BQ, et al. Nickel-based superalloy for key components of advanced ultra-supercritical steam turbine operating above 700 °C. In: 2012 technical exchange conference for ultra supercritical units, Ningbo, Zhejiang, China, 2012, p. 7.
12. Peng JQ, Sun FM, Wang MY. Discussion on materials for high and medium pressure rotors of ultra supercritical steam turbines above 700 °C. In: 2012 technical exchange conference for ultra supercritical units, Ningbo, Zhejiang, China, 2012, p. 10.
13. Wang J · J Univ Sci Technol Beijing · 2012 · 34 · 799
14. 10.1007/BF0264387910.1007/BF02643879 ↗
15. Guo Y · Chin J Mater Res · 2016 · 30 · 841
16. Guo Y · Proc CSEE · 2014 · 34 · 2314
17. Yin T · J Mech Strength · 2018 · 40 · 1078
18. 10.1016/j.jnucmat.2014.08.00310.1016/j.jnucmat.2014.08.003 ↗
19. 10.1016/j.ijpvp.2023.10504010.1016/j.ijpvp.2023.105040 ↗
20. Zhou GB · J Chin Soc Power Eng · 2022 · 42 · 475
21. 10.1016/j.ijfatigue.2013.06.00110.1016/j.ijfatigue.2013.06.001 ↗
22. 10.1016/j.msea.2019.13828610.1016/j.msea.2019.138286 ↗
23. 10.1115/1.402508010.1115/1.4025080 ↗
24. 10.1016/j.msea.2006.10.17010.1016/j.msea.2006.10.170 ↗
25. Zhu ZL · J Chin Soc Corros Prot · 2022 · 42 · 655
26. Jiao Y · J Chin Soc Corros Prot · 2021 · 41 · 417
27. EPRI · 2011
28. 10.1016/j.pnucene.2012.10.00110.1016/j.pnucene.2012.10.001 ↗
29. 10.1016/j.jnucmat.2014.12.01410.1016/j.jnucmat.2014.12.014 ↗
30. 10.1007/s12206-016-0901-310.1007/s12206-016-0901-3 ↗
31. 10.1016/j.jnucmat.2019.04.01710.1016/j.jnucmat.2019.04.017 ↗
32. 10.1016/j.corsci.2019.10831310.1016/j.corsci.2019.108313 ↗
33. 10.1016/j.corsci.2018.01.00410.1016/j.corsci.2018.01.004 ↗
34. 10.1016/j.jnucmat.2009.03.00810.1016/j.jnucmat.2009.03.008 ↗
35. Vadlamani RA · Int J Adv Eng Appl · 2012 · 5 · 1
36. Liu QY · Heat Treat Met · 2016 · 41 · 52
37. Liu YT · J Chin Soc Corros Prot · 2022 · 42 · 647
38. 10.1016/j.ijfatigue.2018.08.03510.1016/j.ijfatigue.2018.08.035 ↗
39. 10.1002/maco.20181023710.1002/maco.201810237 ↗
40. 10.5006/1.358314910.5006/1.3583149 ↗
41. 10.5006/1.357929310.5006/1.3579293 ↗
42. 10.1016/S0010-938X(97)86103-310.1016/S0010-938X(97)86103-3 ↗
43. Shen Z · Atom Energy Sci Technol · 2014 · 48 · 1660
44. Fujisawa R, Nishimura K, Nishida T, et al. Cracking susceptibility of Ni base alloys and 316 stainless steel in less oxidizing or reducing SCW. In: NACE 60th annual conference & exposition (CORROSIONNACEXPO 2005), 2005, pp.3871–3883.
45. Tsuchiya Y · NACE International · 2007 · 13 · 07415:1–07415:1
46. Shen Z · Corros Sci Prot Technol · 2014 · 26 · 113
47. Liu BP · J Chin Soc Corros Prot · 2022 · 42 · 513
48. 10.1016/j.corsci.2013.09.01610.1016/j.corsci.2013.09.016 ↗
49. Xu WQ · 2018
50. Gui JJ · 2019
51. 10.5006/1.358203110.5006/1.3582031 ↗
52. 10.1016/j.corsci.2015.04.02010.1016/j.corsci.2015.04.020 ↗
53. 10.1007/s11661-016-3898-410.1007/s11661-016-3898-4 ↗
54. Ma C · J Chin Soc Corros Prot · 2014 · 34 · 37
55. 10.1002/maco.20170992910.1002/maco.201709929 ↗
56. Krupp U · Mater Res (São Carlos, São Paulo, Brazil) · 2004 · 7 · 3510.1590/S1516-14392004000100006 ↗
57. Zhang KQ · J Chin Soc Corros Prot · 2018 · 38 · 517
58. 10.1016/j.electacta.2008.08.04010.1016/j.electacta.2008.08.040 ↗
59. Chu WY · 2013
60. 10.1016/j.actamat.2013.05.01210.1016/j.actamat.2013.05.012 ↗
61. 10.1016/j.msea.2011.04.02910.1016/j.msea.2011.04.029 ↗
62. Zhang NQ · Electr Power · 2011 · 44 · 47
63. 10.1016/j.pnucene.2014.02.00810.1016/j.pnucene.2014.02.008 ↗