Long term integrity against corrosion of titanium used for TRU waste container
Source abstract
Abstract
Commercial grade pure titanium containing palladium (Ti-Grade 17) may be used for transuranic waste containers. The long term integrity of Ti-Grade 17 against corrosion was studied in the concrete permeated alkaline sodium water environment of 0·6 mol [Cl−]+0·223 mol [OH−] at various temperatures up to 80°C. The study focused on the stability of the passive oxide film, the susceptibility to crevice corrosion and cracks in the titanium hydride (TiH2) layer. General corrosion depth for sustained passivation may be determined as ipass times the evaluation period of 104 years, with addition of the electric quantity for the destruction and repair of passivation film. Crevice corrosion sensitivity is not affected by processes such as welding, cold work and heat treatment. Cathodic reactions essential for maintaining the passive state produce hydrogen that, to some extent, is adsorbed to form a hydride layer. This layer subsequently undergoes cracking to cause reduction in the critical hydride layer thickness δc of 10 μm. The crack depth becomes as much as 100 μm at 2000 years.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Nakayama G, Fukaya Y, Akashi M, Sawa S, Kanno T, Owada H, Otsuki A, Asano H: ‘Hydrogen-induced stress corrosion crack initiation and propagation in titanium alloys in deep underground environments’, Proc. 2nd Int. Workshop on ‘Prediction of long term corrosion behaviour in nuclear waste systems’, Nice, France, September 2004, ANDRA, 35.
2. 10.1016/j.jnucmat.2008.06.02910.1016/j.jnucmat.2008.06.029 ↗
3. 10.3323/jcorr1991.45.71710.3323/jcorr1991.45.717 ↗
4. Nakayama G, Fukuda T, Akashi M: ‘Critical condition for initiation of corrosion crevice of stainless steel’ (Jpn.), Proc. Conf. JSCE Materials and Environments, 1993, 415; Tokyo, JSCE.
5. Paton NE, Williams JC: in ‘Hydrogen in metals’, (ed. , Bernstein I M, Thompson A W, ed), 409–431; 1974, Metals Park, OH, ASM International.
6. Shimogoori K: ‘Hydrogen embrittlement of titanium and the prevention method’ (Jpn.), Proc. 47th Japan Conf. Materials and Environments, JSCE., 23; 1982, Tokyo, JSCE.
7. Nakayama G, Nakamura N, Fukaya Y, Akashi M, Ueda H: ‘Assessment of crevice corrosion and hydrogen induced stress-corrosion cracks in titanium–carbon steel composite overpack for geological disposal of high-level radioactive waste’, Proc. Int. Workshop on ‘Prediction of long term corrosion behaviour in nuclear waste systems’, EFC Publication No.36, 373–394; 2003, London, Maney Publishing.10.1201/9781003580232-29 ↗
8. Taniyama Y · J. Mater. Sci. Soc. Jpn · 2006 · 44 · 106
9. Cho H, Kawasaki A, Matsuo T: ‘Examination of hydride generation behavior in Ti-Gr.1 that uses acoustic emission method’, Proc. JSCE Materials and Environments, 219; 2009, Tokyo, JSCE.
10. Takemoto M: Private communication, 2007.
11. 10.1016/S0010-938X(74)80063-610.1016/S0010-938X(74)80063-6 ↗
12. Japanese Society of Corrosion Engineering (ed.): ‘Introduction to Materials Ecology (Jpn.)’, 43–45; 1993, Tokyo, Maruzen.