Interface electrochemical corrosion behaviour of alclad Al–Zn–Mg–Cu–Cr Al alloy adhesively bonded with carbon fibre reinforced plastic stiffener
Source abstract
Abstract
Stiffening of Al alloy aircraft structures with carbon fibre reinforced plastic laminate called ‘patches’ is considered as a viable option to enhance fatigue life. Interface so created between the reinforcement and Al alloy structure is potential site for crevice corrosion attack. Therefore, studies were conducted to investigate the interface corrosion behaviour of peak and two-step aged Al–Zn–Mg–Cu–Cr alclad alloy with and without the patch and examine the possibility to control the interfacial attack with the addition of cerium chloride inhibitor exposed to 3·5 wt-% NaCl solution for the durations of 2 and 168 h. Electrochemical impedance spectroscopy revealed that the interface attack was significantly reduced by the addition of 1000 ppm cerium chloride. The response of the peak and two-step aged alloy for such an addition was further investigated and found that the alloy under step aged condition behaves better than that of the peak aged condition.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete Corrosion and Durability · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. 10.1023/A:101045370259610.1023/A:1010453702596 ↗
2. 10.4028/www.scientific.net/MSF.242.1110.4028/www.scientific.net/MSF.242.11 ↗
3. 10.1016/S0921-5093(99)00674-710.1016/S0921-5093(99)00674-7 ↗
4. 10.1016/0010-4361(87)90293-X10.1016/0010-4361(87)90293-X ↗
5. 10.1016/j.ijfatigue.2008.11.00910.1016/j.ijfatigue.2008.11.009 ↗
6. 10.1016/S0263-8223(02)00338-010.1016/S0263-8223(02)00338-0 ↗
7. 10.1016/S0263-8223(00)00011-810.1016/S0263-8223(00)00011-8 ↗
8. Hinton B. R. W. · Met. Forum · 1984 · 7 · 211
9. Hinton B. R. W. · Mater. Forum · 1986 · 9 · 162
10. 10.1016/S0300-9440(98)00015-010.1016/S0300-9440(98)00015-0 ↗
11. 10.1016/j.apsusc.2004.05.26810.1016/j.apsusc.2004.05.268 ↗
12. Mishra A. K. · Corros. Sci. · 2007 · 4910.1016/j.corsci.2006.06.026 ↗
13. 10.1016/S1002-0721(10)60338-910.1016/S1002-0721(10)60338-9 ↗
14. Hill J. A. · J. Alloys Compd · 2011 · 509
15. Muster T. H. · J. Electrochem. Soc. · 2012 · 67 · 95
16. 10.1016/j.corsci.2012.03.02310.1016/j.corsci.2012.03.023 ↗
17. Hatch J. E. ‘Aluminium: properties and physical metallurgy’, 2nd edn, Vol. 1, 270–281; 1984, Materials Park, OH, ASM International.
18. 10.1149/1.169538510.1149/1.1695385 ↗
19. 10.1149/1.186998410.1149/1.1869984 ↗
20. 10.1016/0925-8388(92)90359-H10.1016/0925-8388(92)90359-H ↗
21. 10.1016/j.matchemphys.2007.02.07910.1016/j.matchemphys.2007.02.079 ↗
22. Arnott D. R. · Mater. Perform. · 1987 · 26 · 42
23. Hinton B. R. W., Forsyth M., Seter M. and Tan M. Y. ‘Recent developments in corrosion inhibitors based on rare earth metal compounds’, Proc. 16th Asian Pacific Corrosion Control Conf. on ‘Corrosion prevention and environmental protection of materials for a new era’, Kaohsiung, Taiwan, October 2012, The Corrosion Engineering Association of the Republic of China, Paper 86.
24. Bethencourt M. · Corros. Sci. · 1998 · 4010.1016/S0010-938X(98)00077-8 ↗
25. 10.1002/1521-4176(200105)52:5<344::AID-MACO344>3.0.CO;2-S10.1002/1521-4176(200105)52:5<344::AID-MACO344>3.0.CO;2-S ↗
26. 10.1016/j.surfcoat.2011.03.07310.1016/j.surfcoat.2011.03.073 ↗
27. 10.1016/j.corsci.2012.08.05310.1016/j.corsci.2012.08.053 ↗
28. Conde A. · Sci. · 39 · 295
29. Mansfeld F., Lin S. and Shih H. ‘Corrosion protection of metal matrix composites’, Report ARO-24150·4-MS-A, University of Southern California, Los Angeles, CA, USA, 1990.
30. 10.5006/1.357931310.5006/1.3579313 ↗
31. Park J. K. · Metall. Trans. A · 1983 · 14
32. 10.1016/S0010-938X(98)00002-X10.1016/S0010-938X(98)00002-X ↗
33. Kannan M. B. · Adv. Mater. Sci. · 2007 · 7 · 21
34. Kannan M. B. · J. Mater. Sci. · 2007 · 42
35. Kannan M. B. · Scr. Mater. · 2004 · 51
36. Sarkar B. · Metall. Trans. A · 1981 · 1210.1007/BF02643806 ↗
37. 10.1016/S1003-6326(08)60130-210.1016/S1003-6326(08)60130-2 ↗
38. 10.1016/S1005-8850(07)60047-410.1016/S1005-8850(07)60047-4 ↗
39. 10.5006/1.328772610.5006/1.3287726 ↗
40. 10.1016/S0257-8972(03)00743-610.1016/S0257-8972(03)00743-6 ↗
41. 10.1016/0010-938X(87)90088-610.1016/0010-938X(87)90088-6 ↗
42. Holroyd N. J. H. · 2000 · 173
43. 10.5006/1.358490510.5006/1.3584905 ↗
44. McCafferty E. · Corros. Sci. · 2003 · 45
45. Cooper K. R. · Corros. Sci. · 2007 · 4910.1016/j.corsci.2006.12.001 ↗
46. 10.1016/j.corsci.2009.01.01610.1016/j.corsci.2009.01.016 ↗