journal article·2019-07-04

Influence of dissolved oxygen concentration and exposure temperature on the steam oxidation behaviour of HR3C

Zhen Yang, Jintao Lu, Hao Li, Ming Le, Jingbo Yan, Yong Yuan

Publisher page

Abstract

Oxidation behaviour of an austenitic steel HR3C at 620∼650°C for 1000 h in steam with two different levels of dissolved oxygen (DO), 20 ppb and 5 ppm, was investigated by gravimetry, X-ray diffraction and scanning electron microscopy. Results showed that mainly a single-layered (Cr, Mn)2O3 scale was developed. The oxide growth followed near-power kinetics and was accelerated with DO concentration and exposure temperature. At the higher DO concentration, the formation of (Cr, Mn)2O3 with a much smaller size was favoured. Besides, the oxide scale became undulated and interfacial voids formed. Higher exposure temperature resulted in the growth of the (Cr, Mn)2O3 crystals and the change of their morphology from acicular to granular. Fe3O4 nodules and Ni-Cr spinel occurred at 650°C/5 ppm DO. Related oxidation mechanisms were discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National Engineering Research Center of Clean Coal Combustion for Utility Boilers, Xi'an Thermal Power Research Institute Co., Ltd., Xi'an, People's Republic of China

Funding

National Natural Science Foundation of China · China Huaneng Group, Huaneng Power International, Inc

References (28)

Show source-provided references
1. 10.1016/S0896-8446(03)00031-710.1016/S0896-8446(03)00031-7 ↗
2. Bursik A · Power Plant Chem · 2005 · 7 · 593
3. Dooley RB · Power Plant Chem · 2009 · 11 · 352
4. Dooley RB. · 2005
5. Dooley RB. · Power Plant Chem · 2008 · 10 · 68
6. 10.1016/j.applthermaleng.2015.10.09810.1016/j.applthermaleng.2015.10.098 ↗
7. Dooley RB · Power Plant Chem · 2011 · 13 · 236
8. 10.1016/j.corsci.2005.08.02110.1016/j.corsci.2005.08.021 ↗
9. 10.1016/j.jnucmat.2007.05.02310.1016/j.jnucmat.2007.05.023 ↗
10. 10.1016/j.corsci.2011.11.01310.1016/j.corsci.2011.11.013 ↗
11. 10.1016/j.supflu.2015.10.01710.1016/j.supflu.2015.10.017 ↗
12. 10.1016/j.jnucmat.2007.05.01710.1016/j.jnucmat.2007.05.017 ↗
13. Yang Z · J Chinese Soc Power Eng (China) · 2014 · 35 · 859
14. 10.3184/096034012X1332269813778510.3184/096034012X13322698137785 ↗
15. 10.1016/j.scriptamat.2007.06.05010.1016/j.scriptamat.2007.06.050 ↗
16. 10.1016/j.corsci.2017.06.00910.1016/j.corsci.2017.06.009 ↗
17. 10.1016/j.msea.2007.05.03510.1016/j.msea.2007.05.035 ↗
18. Kofstad P. · 1988
19. 10.1016/j.ssc.2004.03.03310.1016/j.ssc.2004.03.033 ↗
20. 10.1002/adem.20031007910.1002/adem.200310079 ↗
21. 10.1016/S1359-6454(03)00260-X10.1016/S1359-6454(03)00260-X ↗
22. 10.1016/j.actamat.2012.09.00410.1016/j.actamat.2012.09.004 ↗
23. 10.1016/j.corsci.2005.10.01010.1016/j.corsci.2005.10.010 ↗
24. Wagner C. · Zeitschrift für Elektrochemie, Berichte der Bunsengesellschaft für physikalische Chemie · 1959 · 63 · 77210.1002/bbpc.19590630713 ↗
25. Young DJ. · 2008
26. 10.1016/j.corsci.2012.06.00710.1016/j.corsci.2012.06.007 ↗
27. 10.1179/mht.2005.00310.1179/mht.2005.003 ↗
28. Barin I. · 2003