Accelerated corrosion test and field test of steel and zinc coupons at buffer areas and cross passages in a mass rapid transit tunnel
Source abstract
Abstract
A study has been conducted to measure the distribution of temperature, relative humidity and corrosivity due to uniform corrosion along the Mass Rapid Transit (MRT) North East Line (NEL) tunnel in Singapore. The corrosion rates of carbon steel 1010 and zinc coupons at the buffer areas of ten stations and five cross passages along the NEL were monitored over a period of one year. The median temperatures were between 31 and 36°C while the median relative humidity varied between 43 and 53%. At all exposure sites, the values of relative humidity corresponding to the 75th percentile values were below 60%, with very few data points registering above 80%. The cross passages showed a lower degree of fluctuations in the temperature and relative humidity compared to the buffer areas. The corrosivity levels showed some differences between exposure sites, but their values were generally low and could be categorised as C1 according to the ISO 9223:2012 categorisation. A set of procedures for an accelerated laboratory test to approximate the corrosion in the tunnel was also studied. The test procedures involved the exposure to a salt fog containing 0.12% Na2SO4 + 0.05% NaCl, followed by a drying phase and subsequent exposure to a constant temperature of 40°C and a constant relative humidity of 60%. It was found that after exposure for 80 h, the accelerated tests were able to generate the degree of corrosion observed in the most severe conditions in the field.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Infrastructure Maintenance and Monitoring · Asphalt Pavement Performance Evaluation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Singapore Institute of Technology, Singapore
Land Transport Authority, Singapore
SBS Transit, Singapore
Funding
Land Transport Authority Singapore
References (43)
Show source-provided references
1. ISO 12944-2. Paints and varnishes – corrosion protection of steel structures by protective paint systems – part 2: classification of environments. 2017.
2. ISO 9223. Corrosion of metals and alloys – corrosivity of atmospheres – classification, determination and estimation. 2012.
3. ANSI/ISA-71-04. Environmental conditions for process measurement and control systems: airborne contaminations. 2013.
4. 10.1016/j.coldregions.2020.10314110.1016/j.coldregions.2020.103141 ↗
5. Luo Y · J. Traffic Transport Eng · 2019 · 6 · 297
6. 10.2219/rtriqr.57.3_19910.2219/rtriqr.57.3_199 ↗
7. Andrén A · J Earth Sci Geotech Eng · 2020 · 10 · 161
8. 10.1007/978-3-642-27957-7_3310.1007/978-3-642-27957-7_33 ↗
9. 10.1155/2020/473249010.1155/2020/4732490 ↗
10. 10.1080/10962247.2013.85214410.1080/10962247.2013.852144 ↗
11. 10.1016/j.atmosenv.2004.02.03910.1016/j.atmosenv.2004.02.039 ↗
12. 10.1016/S1352-2310(96)00193-810.1016/S1352-2310(96)00193-8 ↗
13. 10.1007/s00603-021-02547-310.1007/s00603-021-02547-3 ↗
14. Kreislova K, Geiplova H, Licbinsky R, et al. Corrosivity of road tunnel microclimate. EUROCORR. 2012.
15. 10.1007/978-981-15-9199-0_5110.1007/978-981-15-9199-0_51 ↗
16. 10.1016/0010-938X(93)90028-F10.1016/0010-938X(93)90028-F ↗
17. 10.1016/j.matchemphys.2013.07.00910.1016/j.matchemphys.2013.07.009 ↗
18. ISO 9227. Corrosion tests in artificial atmospheres – salt spray tests. 2017.
19. ASTM B117-19. Standard practice for operating salt spray (fog) apparatus. 2019.
20. 10.1108/eb00739210.1108/eb007392 ↗
21. 10.1155/2014/41957010.1155/2014/419570 ↗
22. Carlsson B, Engström G, Hög Lejre A, et al. Guidelines for selection of accelerated corrosion test for product qualification. Nordic Innovation Centre, Report NT TR597, 2005. Available from: www.nordicinnovation.net.
23. 10.1007/s10800-005-1322-710.1007/s10800-005-1322-7 ↗
24. 10.1016/j.corsci.2004.10.01210.1016/j.corsci.2004.10.012 ↗
25. Montgomery EL · 2012 · 5655
26. 10.1016/j.conbuildmat.2021.12570610.1016/j.conbuildmat.2021.125706 ↗
27. 10.1016/j.corsci.2014.05.01410.1016/j.corsci.2014.05.014 ↗
28. 10.1016/0010-938X(89)90066-810.1016/0010-938X(89)90066-8 ↗
29. 10.1007/s11998-008-9135-310.1007/s11998-008-9135-3 ↗
30. ASTM G1-03. Standard practice for preparing, cleaning, and evaluating corrosion test specimens. 2011.
31. Goh KH · 2014
32. ISO 9226. Corrosion of metals and alloys – corrosivity of atmospheres – determination of corrosion rate of standard specimens for the evaluation of corrosivity. 2012.
33. 10.1179/147842209X1257940158676210.1179/147842209X12579401586762 ↗
34. 10.1177/1420326X2095041110.1177/1420326X20950411 ↗
35. 10.14773/cst.2017.16.1.3810.14773/cst.2017.16.1.38 ↗
36. 10.3989/revmetalm.112510.3989/revmetalm.1125 ↗
37. 10.1520/MPC2018002610.1520/MPC20180026 ↗
38. Qi Y · Int J Electrochem Sci · 2014 · 9 · 210110.1016/S1452-3981(23)07914-2 ↗
39. Hasan BO · Adv Chem Eng Res · 2013 · 2 · 61
40. Kajiyama H · JFE Technol Rep · 2007 · 9 · 80
41. 10.1179/174327806X9403610.1179/174327806X94036 ↗
42. Gore R, Witska RICH, Kirby JR, et al. Corrosive gas environmental testing for electrical contacts. Proceedings of the Thirty Fifth Meeting of the IEEE Holm Conference on Electrical Contacts. IEEE, 1989. p. 123–131. Chicago, Illinois.10.1109/HOLM.1989.77931 ↗
43. ISO 21207. Corrosion tests in artificial atmospheres – accelerated corrosion tests involving alternate exposure to corrosion-promoting gases, neutral salt-spray and drying. 2015.