Abstract
The main objective of this study is to assess the long-term performance of Pt nanoparticle coated anodised Ti coupons which are used for electrochemical dissolution of spent mixed-oxide nuclear fuels during reprocessing. In this work, electrodes were exposed to a simulated dissolver solution containing a representative fraction of low-activity actinides and fission products in 11.5 N nitric acid in a mock-up of the service dissolver vessel. Platinum nanoparticles were coated onto anodised titanium coupons through a seed-mediated hydrothermal method. The coated coupons were then exposed in the simulated dissolver solution for about 1185 h at 110°C. Morphological and compositional analyses confirmed the presence of metallic Pt nanoparticles on the electrode surface with some localised cracking. The electrochemically active surface area of the Pt-nanoparticle coated anodised titanium coupon after exposure was found to be twice that of polycrystalline platinum thus establishing the durability and efficiency of the coating on the electrode.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Radioactive element chemistry and processing · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Corrosion Science and Technology Division, Indira Gandhi Centre for Atomic Research, Kalpakkam, India
Homi Bhabha National Institute, Kalpakkam, India
References (42)
Show source-provided references
1. 10.1007/BF0322235010.1007/BF03222350 ↗
2. 10.13182/NT92-A3473410.13182/NT92-A34734 ↗
3. 10.1016/S0022-3115(99)00141-510.1016/S0022-3115(99)00141-5 ↗
4. 10.1016/j.pnucene.2005.07.00110.1016/j.pnucene.2005.07.001 ↗
5. 10.1361/10599490377034340210.1361/105994903770343402 ↗
6. 10.1021/jp040732410.1021/jp0407324 ↗
7. 10.1021/nl201745910.1021/nl2017459 ↗
8. 10.1016/j.jpowsour.2011.06.04310.1016/j.jpowsour.2011.06.043 ↗
9. 10.1016/j.jelechem.2004.04.00410.1016/j.jelechem.2004.04.004 ↗
10. 10.1016/j.catcom.2011.07.00810.1016/j.catcom.2011.07.008 ↗
11. 10.1016/S0022-0728(00)00492-710.1016/S0022-0728(00)00492-7 ↗
12. 10.1007/s10800-011-0366-010.1007/s10800-011-0366-0 ↗
13. 10.1179/174329407X26058210.1179/174329407X260582 ↗
14. 10.1016/S0254-0584(00)00268-610.1016/S0254-0584(00)00268-6 ↗
15. 10.1007/s10800-011-0371-310.1007/s10800-011-0371-3 ↗
16. 10.1007/s11665-014-0903-110.1007/s11665-014-0903-1 ↗
17. 10.1016/j.matchemphys.2014.11.04710.1016/j.matchemphys.2014.11.047 ↗
18. 10.1007/s12666-016-0944-210.1007/s12666-016-0944-2 ↗
19. 10.1039/C5RA16245A10.1039/C5RA16245A ↗
20. Rasmi KR · Mater Perf NACE Internl · 2017 · 56 · 48
21. 10.13182/NT14-9010.13182/NT14-90 ↗
22. 10.1016/j.egypro.2011.06.06310.1016/j.egypro.2011.06.063 ↗
23. 10.13182/NT12-7310.13182/NT12-73 ↗
24. 10.1016/j.jnucmat.2016.02.01810.1016/j.jnucmat.2016.02.018 ↗
25. 10.1080/18811248.2007.971129910.1080/18811248.2007.9711299 ↗
26. 10.1088/2043-6262/3/2/02500510.1088/2043-6262/3/2/025005 ↗
27. 10.1016/j.jcat.2016.09.02610.1016/j.jcat.2016.09.026 ↗
28. 10.1016/j.corsci.2013.10.02610.1016/j.corsci.2013.10.026 ↗
29. 10.1039/C5TA03809J10.1039/C5TA03809J ↗
30. 10.1039/C4CE00884G10.1039/C4CE00884G ↗
31. Moulder JF · 1992
32. Jayaraj J · Inter Metallics · 2017 · 89 · 123
33. 10.1038/s41467-018-08144-310.1038/s41467-018-08144-3 ↗
34. 10.5714/CL.2013.14.4.24710.5714/CL.2013.14.4.247 ↗
35. 10.1038/srep4197810.1038/srep41978 ↗
36. 10.1088/1468-6996/12/3/03440110.1088/1468-6996/12/3/034401 ↗
37. 10.1016/j.tsf.2015.07.04110.1016/j.tsf.2015.07.041 ↗
38. 10.1021/j100215a01010.1021/j100215a010 ↗
39. 10.1021/jp209347r10.1021/jp209347r ↗
40. 10.1016/j.elecom.2010.10.02010.1016/j.elecom.2010.10.020 ↗
41. 10.1023/A:102477161802710.1023/A:1024771618027 ↗
42. 10.1021/ed077p119510.1021/ed077p1195 ↗