Corrosion behaviour analysis of galvanised steel in severe marine and extremely cold climatic conditions
Source abstract
Abstract
The corrosion mechanism of galvanised steel (GS) was systematically compared under the Wanning marine atmosphere and the Mohe extremely cold conditions through corrosion rate analysis, morphological observations, corrosion product analysis, and electrochemical measurements. The findings demonstrate a significant environmental influence on GS corrosion behaviour. GS exhibited significantly higher corrosion rates in the Wanning marine environment than in the Mohe extremely cold environment. In the Wanning marine environment, the corrosion product layer undergoes progressively densifying over time, thereby enhancing the corrosion barrier effectiveness of the zinc coating. The electrochemical migration of Cl − in marine environments promotes its adsorption onto the coating surface, subsequent dissolution, and enhanced ionic conductivity within the electrolyte film. Following 36-month exposure, Cl − infiltration through the coating initiated microstructural collapse, with subsequent corrosion rate manifesting a distinctive V-shaped trajectory, it reached a minimum value of 3.357 g·m −2 ·a −1 at the 24-month then increased rapidly to 26.089 g·m −2 ·a −1 at the 36-month. In contrast, the prevailing low temperatures in Mohe induced the progressive densification of the corrosion product layer over time, which acted as an enhanced protective barrier for GS and mitigated corrosion progression. The corrosion rate reached a minimum value of 2.286 g·m −2 ·a −1 at the 36-month of exposure.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Northeastern University
Institute of Metal Research, Chinese Academy of Sciences
Liaoning Shenyang Soil and Atmosphere Corrosion of Material National Observation and Research Station, Shenyang, China
Funding
Natural Science Foundation of Shenyang Municipality · National Key Research and Development Program of China
References (43)
Show source-provided references
1. 10.1016/j.jmrt.2024.01.27010.1016/j.jmrt.2024.01.270 ↗
2. 10.1016/j.corsci.2014.05.01610.1016/j.corsci.2014.05.016 ↗
3. 10.1016/j.corsci.2024.11221410.1016/j.corsci.2024.112214 ↗
4. 10.1080/1478422X.2020.175016210.1080/1478422X.2020.1750162 ↗
5. 10.5006/117710.5006/1177 ↗
6. 10.1016/j.corsci.2014.05.01410.1016/j.corsci.2014.05.014 ↗
7. 10.1016/j.matchemphys.2017.05.04310.1016/j.matchemphys.2017.05.043 ↗
8. 10.1016/j.corsci.2013.11.02710.1016/j.corsci.2013.11.027 ↗
9. 10.1016/S1003-6326(18)64905-210.1016/S1003-6326(18)64905-2 ↗
10. 10.1016/S0010-938X(96)00086-810.1016/S0010-938X(96)00086-8 ↗
11. Cui T, Cheng J, Song J, et al. Accelerated corrosion behavior of high strength aluminum alloy in simulated polar atmosphere. Equip Environ Eng 2025; 22: 61–68.
12. Leng W, Shi X, Xin Y, et al. Correlation of corrosion information acquired by indoor acceleration testing and by real low temperature marine atmosphere exposure in polar region for Ni-Cr-Mo-V steel. J Chin Soc Corros Prot 2024; 44: 91–99.
13. 10.5006/245810.5006/2458 ↗
14. 10.1016/j.corsci.2014.06.01710.1016/j.corsci.2014.06.017 ↗
15. 10.1016/j.jmrt.2024.10.08010.1016/j.jmrt.2024.10.080 ↗
16. 10.1016/j.corsci.2010.11.00410.1016/j.corsci.2010.11.004 ↗
17. 10.1016/j.corsci.2017.06.02510.1016/j.corsci.2017.06.025 ↗
18. 10.1016/j.jmrt.2022.12.17610.1016/j.jmrt.2022.12.176 ↗
19. 10.1134/S003317320807002310.1134/S0033173208070023 ↗
20. 10.1016/j.corsci.2013.06.04710.1016/j.corsci.2013.06.047 ↗
21. 10.1016/j.corsci.2009.11.00210.1016/j.corsci.2009.11.002 ↗
22. Liu Y, Cao G, Wang Z, et al. Atmospheric corrosion behavior of galvanized steel at Hongyanhe Nuclear Power Station. Surf Technol 2016; 45: 152–157.
23. 10.1016/j.corsci.2016.04.00210.1016/j.corsci.2016.04.002 ↗
24. Yao W, Cai Y. Atmospheric corrosion performance of zinc at several selected test sits in China. Corros Sci Technol Prot 2003; 15: 192–195.
25. 10.1016/S0254-0584(02)00110-410.1016/S0254-0584(02)00110-4 ↗
26. 10.1016/j.corsci.2010.05.04410.1016/j.corsci.2010.05.044 ↗
27. 10.1016/j.corsci.2012.08.01410.1016/j.corsci.2012.08.014 ↗
28. 10.1016/j.corsci.2007.03.03210.1016/j.corsci.2007.03.032 ↗
29. Li M, Dong N, Shang T, et al. Study on initial corrosion behavior of Zn-Al-Mg coating and pure zinc coating in typical atmospheric environment. Surf Technol 2024; 53: 120–129.
30. 10.1016/j.corsci.2012.08.05610.1016/j.corsci.2012.08.056 ↗
31. 10.20964/2021.12.0610.20964/2021.12.06 ↗
32. Liu Y. Corrosion behavior of galvanized steels in Cl-containing acid rain atmospheric environment. Graduate University of Chinese Academy of Sciences, Shenyang, China, 2015.
33. 10.1016/S0013-4686(01)00431-510.1016/S0013-4686(01)00431-5 ↗
34. 10.4028/www.scientific.net/MSF.940.5910.4028/www.scientific.net/MSF.940.59 ↗
35. 10.1002/maco.20140805810.1002/maco.201408058 ↗
36. Barsoukov E, Macdonald RJ. Impedance spectroscopy: theory, experiment, and applications. J Am Chem Soc 2005; 127: 12431.
37. 10.1016/j.jmst.2020.03.02410.1016/j.jmst.2020.03.024 ↗
38. 10.1016/j.corsci.2018.12.03310.1016/j.corsci.2018.12.033 ↗
39. 10.1016/0010-938X(93)90082-R10.1016/0010-938X(93)90082-R ↗
40. 10.1016/0010-938X(93)90096-Y10.1016/0010-938X(93)90096-Y ↗
41. 10.1002/maco.20120695910.1002/maco.201206959 ↗
42. 10.1016/0010-938X(94)90052-310.1016/0010-938X(94)90052-3 ↗
43. 10.1016/j.corsci.2011.01.04410.1016/j.corsci.2011.01.044 ↗