Abstract
Due to exposure to harsh environments, steel structures are susceptible to corrosion, resulting in a significant reduction in their normal service life and increasingly prominent durability issues. To achieve this, humid-hot cycle and immersion accelerated corrosion tests were conducted. Laser confocal microscopy was utilized to measure surface coordinate parameters, enabling an examination of variations in surface roughness parameters and corrosion pit size over the course of corrosion time. The research findings indicate that during the initial phase of corrosion, a limited number of needle-like pitting products are formed, resulting in relatively mild damage. However, as the corrosion time progresses, the metallic luster diminishes rapidly, and the surface pitting micro-morphology of the specimen gradually transforms into corrosion pits. Microscopic scanning analysis reveals that the corrosion behavior extends rapidly along the horizontal direction, eventually completely enveloping the surface of the specimen, and the accumulation of surface products provides significant protection to the interior of the matrix. Furthermore, using the loss ratio can better analyze the errors that exist in the actual testing process, in order to accurately reflect the corrosion damage evolution law of HSS.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Structural Integrity and Reliability Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Southeast University
Xi'an University of Technology
School of Civil & Mechanical Engineering, Curtin University, Bentley WA, Australia
Funding
SEU Innovation Capability Enhancement Plan for Doctoral Students · Natural Science Foundation of Jiangsu Province · National Natural Science Foundation of China - State Grid Corporation Joint Fund for Smart Grid · Postgraduate Research & Practice Innovation Program of Jiangsu Province · Fund projects funded by the China Scholarship Council
References (51)
Show source-provided references
1. Hou BR, Li XG, Ma XM, et al. The cost of corrosion in China. Npj Mat. Degrad 2017; 1: 1–10.
2. 10.1016/j.marstruc.2020.10271810.1016/j.marstruc.2020.102718 ↗
3. 10.1016/j.oceaneng.2014.05.00310.1016/j.oceaneng.2014.05.003 ↗
4. 10.1016/j.commatsci.2023.11235210.1016/j.commatsci.2023.112352 ↗
5. 10.1016/j.istruc.2021.05.03910.1016/j.istruc.2021.05.039 ↗
6. 10.1016/j.engfailanal.2023.10709810.1016/j.engfailanal.2023.107098 ↗
7. 10.1016/j.corsci.2018.12.02910.1016/j.corsci.2018.12.029 ↗
8. Wei HH. Experimental study on fatigue performance of butt welds of Q690 high strength steel in marine corrosive environment. In: 11th International Conference on Civil Engineering, Singapore, Oct. 20-22, 2023.
9. 10.1016/j.apor.2023.10376410.1016/j.apor.2023.103764 ↗
10. 10.1016/j.corsci.2019.10836810.1016/j.corsci.2019.108368 ↗
11. 10.1016/j.istruc.2020.12.02810.1016/j.istruc.2020.12.028 ↗
12. 10.1016/j.mtcomm.2022.10518410.1016/j.mtcomm.2022.105184 ↗
13. 10.1016/j.marstruc.2010.07.00210.1016/j.marstruc.2010.07.002 ↗
14. 10.1016/j.engfailanal.2023.10735210.1016/j.engfailanal.2023.107352 ↗
15. 10.20964/2021.05.6310.20964/2021.05.63 ↗
16. 10.1016/j.corsci.2022.11049010.1016/j.corsci.2022.110490 ↗
17. 10.1016/j.triboint.2018.01.04910.1016/j.triboint.2018.01.049 ↗
18. 10.1016/j.jre.2020.06.01510.1016/j.jre.2020.06.015 ↗
19. 10.1016/j.jcsr.2020.10616010.1016/j.jcsr.2020.106160 ↗
20. 10.1016/j.marstruc.2013.04.00610.1016/j.marstruc.2013.04.006 ↗
21. 10.1201/978143983255410.1201/9781439832554 ↗
22. 10.1080/1478422X.2019.159095910.1080/1478422X.2019.1590959 ↗
23. 10.1016/j.marstruc.2018.04.00310.1016/j.marstruc.2018.04.003 ↗
24. 10.1007/s40195-018-0797-210.1007/s40195-018-0797-2 ↗
25. 10.1016/j.istruc.2019.06.00210.1016/j.istruc.2019.06.002 ↗
26. 10.1016/j.rser.2016.02.01710.1016/j.rser.2016.02.017 ↗
27. 10.1016/j.istruc.2025.10932410.1016/j.istruc.2025.109324 ↗
28. 10.1007/s13296-021-00468-z10.1007/s13296-021-00468-z ↗
29. 10.1016/j.dibe.2023.10021410.1016/j.dibe.2023.100214 ↗
30. 10.1016/j.apor.2023.10358110.1016/j.apor.2023.103581 ↗
31. 10.1016/j.corcom.2022.03.00110.1016/j.corcom.2022.03.001 ↗
32. 10.1016/j.conbuildmat.2006.07.00810.1016/j.conbuildmat.2006.07.008 ↗
33. 10.1016/j.microrel.2021.11428610.1016/j.microrel.2021.114286 ↗
34. Ezzeldin I, Naggar EI, Newhook J, et al. Accelerated wet/dry corrosion test for buried corrugated mild steel. Case Stud. Constr. Mat 2022; 17: e01152.
35. 10.1016/j.ijhydene.2017.05.21010.1016/j.ijhydene.2017.05.210 ↗
36. 10.1016/j.ijfatigue.2023.10756810.1016/j.ijfatigue.2023.107568 ↗
37. GB/T 1591-2008 Low-alloy high-strength structural steel S. Beijing: National Standards Press of the People’s Republic of China 2008. (in Chinese)
38. Hou BR. My passion for the corrosion protection of ocean splash zone. Mar. Sci 2020; 44: 179–193. in Chinese.
39. 10.1016/j.jobe.2024.10850910.1016/j.jobe.2024.108509 ↗
40. 10.1016/j.conbuildmat.2019.11776310.1016/j.conbuildmat.2019.117763 ↗
41. 10.1016/j.corsci.2023.11121010.1016/j.corsci.2023.111210 ↗
42. 10.1016/j.corsci.2023.11110910.1016/j.corsci.2023.111109 ↗
43. 10.5006/263810.5006/2638 ↗
44. 10.1016/j.engfailanal.2022.10695510.1016/j.engfailanal.2022.106955 ↗
45. 10.1016/j.matpr.2022.05.01810.1016/j.matpr.2022.05.018 ↗
46. Shang Y. Study on the Influence of Corrosion environment on the surface corrosion characteristics of steel structures. Xi'an: Xi'an University of Architecture and Technology, 2011, in Chinese.
47. 10.1016/j.istruc.2022.04.06310.1016/j.istruc.2022.04.063 ↗
48. 10.1016/j.msea.2017.10.04210.1016/j.msea.2017.10.042 ↗
49. 10.20964/2020.11.2210.20964/2020.11.22 ↗
50. 10.1016/j.mtcomm.2025.11217210.1016/j.mtcomm.2025.112172 ↗
51. 10.1016/j.conbuildmat.2025.14261310.1016/j.conbuildmat.2025.142613 ↗