journal article·2016-06-01

A review of hydrogen embrittlement of martensitic advanced high-strength steels

Jeffrey Venezuela, Qinglong Liu, Mingxing Zhang, Qingjun Zhou, Andrej Atrens

Corrosion Reviews· Volume 34· Issue 3
Publisher page

Abstract

Abstract The martensitic advanced high-strength steels (MS-AHSS) are used to create fuel-efficient, crashworthy cars. Hydrogen embrittlement (HE) is an issue with high-strength steels; thus, the interaction of hydrogen with MS-AHSS needs to be studied. There are only a few published works on the HE of MS-AHSS. The current literature indicates that the HE susceptibility of MS-AHSS is affected by (i) the strength of the steel, (ii) the applied strain rate, (iii) the concentration of hydrogen, (iv) microstructure, (v) tempering, (vi) residual stress, (vii) fabrication route, (viii) inclusions, (ix) metallic coatings, and (x) specific precipitates. Some of the unresolved issues include (i) the correlation of laboratory results to service performance, (ii) establishing the conditions or factors that lead to a certain HE response, (iii) studying the effect of stress rate on HE, and (iv) a comprehensive understanding of hydrogen trapping in MS-AHSS.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Division of Materials, School of Mining and Mechanical Engineering, The University of Queensland, St. Lucia 4072, Australia

Baoshan Iron & Steel Co., Ltd., Research Institute, Shanghai 201900, China

References (100+)

Show source-provided references
1. Abraham A. Future Growth of AHSS. Ducker Worldwide. Great Designs in Steel Seminar. Available at: http://www.ducker.com/. Retrieved July 17, 2014.
2. Akiyama E, Wang M, Li S, Zhang Z, Kimura Y, Uno N, Tsuzaki K. Studies of evaluation of hydrogen embrittlement property of high-strength steels with consideration of the effect of atmospheric corrosion. Metall Mater Trans A 2013; 44: 1290–1300.10.1007/s11661-012-1403-2 ↗
3. Albert SK, Ramasubbu V, Parvathavarthini N, Gill TPS. Hydrogen-assisted cracking and diffusible hydrogen content in Cr-Mo steel welds. Sadhana 2003; 28: 383–393.10.1007/BF02706439 ↗
4. Allain S, Chateau JP, Bouaziz O, Migot S, Guelton N, Frommeyerr G, Brux U. Microstructures and mechanical properties of high-strength FeMn-Al-C light TRIPLEX steels. Steel Res Int 2006; 77: 627–633.10.1002/srin.200606440 ↗
5. Aosaka T. Metal hydrogen systems: hydrogen trapping behaviour in plain carbon and Cr-Mo alloy steel. In: Veziroglu N, editor. Proc Int Symp Metal Hydrogen Syst. Oxford: Pergamon, 1982: 197–204.10.1016/B978-0-08-027311-2.50024-3 ↗
6. ArcelorMittal. Steel Providing Solutions to OEMs Challenges. Available at: http://automotive.arcelormittal.com/. Retrieved July 21, 2014a.
7. ArcelorMittal. Usibor: Steels for Hot Stamping. Available at: http://automotive.arcelormittal.com/. Retrieved April 12, 2014b.
8. ArcelorMittal. MartINsite® Steels. Available at: http://automotive.arcelormittal.com/. Retrieved September 12, 2015.
9. Askeland D, Fulay P, Wright V. The science and engineering of materials, SI edition, Canada: Cengage Learning, 2011.
10. Atrens A, Dannhaeuser G. Stress corrosion cracking of Zircaloy-4 cladding tubes, part I. Threshold in the presence of iodine. J Nucl Mater 1984; 126: 91–102.10.1016/0022-3115(84)90078-3 ↗
11. Atrens A, Oehlert A. Linearly-increasing-stress testing of carbon steel in 4 N NaNO3 and on Bayer liquor. J Mater Sci 1998; 33: 783–788.10.1023/A:1004314517742 ↗
12. Atrens A, Brosnan CC, Ramamurthy S, Oehlert A, Smith IO. Linearly increasing stress test (LIST) for SCC research. Meas Sci Technol 1993; 4: 1281–1292.10.1088/0957-0233/4/11/017 ↗
13. Automotive Applications Council. AHSS 101 – The Evolving Use of Advanced High-Strength Steels for Automotive Application. Available at: http://www.autosteel.org/. Retrieved April 20, 2014.
14. Baboian R. Corrosion tests and standards: application and interpretation, 2nd ed., West Conshohocken, PA: ASTM International, 2005: 302–321.10.1520/MNL20_2ND-EB ↗
15. Banerji SK, McMahon CJ, Feng C. Intergranular fracture in 4340-type steels: effects of impurities and hydrogen. Met Trans A 1978; 9A: 237–247.10.1007/BF02646706 ↗
16. Barnett WJ, Troiano AR. Crack propagation in hydrogen induced brittle fracture of steel. J Met 1957; 9: 486–494.10.1007/BF03397905 ↗
17. Barnoush A, Vehoff H. Electrochemical nanoindentation: a new approach to probe hydrogen deformation interaction. Scr Metall 2006; 55: 185–198.10.1016/j.scriptamat.2006.03.041 ↗
18. Barnoush A, Asgari M, Johnsen R, Hoel R. Hydrogen effect on nanomechanical properties of the nitrided steel. Metall Mater Trans A 2013; 44: 766–775.10.1007/s11661-012-1462-4 ↗
19. Bates JF, Loginow AW. Principles of stress corrosion cracking as related to steels. Corrosion 1964; 20: 189–197.10.5006/0010-9312-20.6.189t ↗
20. Beachem CD. A new model for hydrogen assisted cracking (hydrogen embrittlement). Metall Trans 1972; 3: 437–451.10.1007/BF02642048 ↗
21. Becker WT, Shipley RJ, editors. Hydrogen Damage and Embrittlement, Failure Analysis and Prevention. Vol 11 ASM Handbook, Materials Park, OH: ASM International, 1986.
22. Bell T, Owen WS. Martensite in iron-nitrogen alloys. J Iron Steel Inst 1967; 205: 428–434.
23. Bergers K, Camisao de Souza E, Thomas I, Mabho N, Flock J. Determination of hydrogen in steel by thermal desorption mass spectrometry. J Flock Steel Res Int 2010; 81: 499–507.10.1002/srin.201000023 ↗
24. Bernstein IM, Garber R, Pressouyre GM. Effect of hydrogen on behavior of materials. In: Thompson AW, Bernstein IM, editors. Effect of hydrogen on behavior of materials. New York: TMS-AIME, 1976: 37.
25. Bernstein IM, Thompson AW. Effect of metallurgical variables on environmental fracture of steels. Int Met Rev 1976; 21: 269–287.
26. Bhat SP. Advances in High Strength Steels for Automotive Applications. Automotive Product Applications Arcelor Mittal, 2008. Available at: http://www.autosteel.org/. Retrieved April 12, 2014.
27. Bhattacharya D. An overview of advanced high strength steels (AHSS). Advanced High Strength Steel Workshop. Arlington, VA: Auto/Steel Partnership, October 22–23, 2006.
28. Bhattacharya D. Metallurgical perspectives on advanced sheet steels. In: Weng Y, Dong H, Gan Y, editors. Advanced steels: the recent scenario in steel science and technology. New York: Metallurgical Industry Press and Springer-Verlag GmbH, 2011: 174.10.1007/978-3-642-17665-4_18 ↗
29. Bhattacharya D. The MartINsite® Success Story – From Shoe Shanks to Car Bumpers. Available at: http://automotive.arcelormittal.com/. Retrieved June 15, 2015.
30. Birnbaum HK. Mechanisms of hydrogen related fracture of metals. In: Moody NR, Thompson AW, editors. Hydrogen effects on materials behavior. Warrendale, PA: TMS, 1990: 639–658.10.21236/ADA208210 ↗
31. Birnbaum HK. Hydrogen effects on deformation-relation between dislocation behavior and the macroscopic stress strain behavior. Scr Metall Mater 1994a; 31: 149–153.10.1016/0956-716X(94)90166-X ↗
32. Birnbaum HK, Sofronis P. Hydrogen-enhanced localized plasticity – a mechanism for hydrogen related fracture. Mater Sci Eng A 1994b; 176: 191–202.10.1016/0921-5093(94)90975-X ↗
33. Birnbaum HK, Robertson IM, Sofronis P, Teter D. Mechanisms of hydrogen related fracture – a review. In: Magnin T, editor. Corrosion-deformation interactions, 1997: 172.
34. Birnbaum HK, Robertson IM, Sofronis P. Hydrogen effects on plasticity. In: Lépinoux J, editor. Multiscale phenomena in plasticity. Kluwer Academic Pub, 2000: 367–381.10.1007/978-94-011-4048-5_29 ↗
35. Bockris J. Modern electrochemistry: an introduction to an interdisciplinary area, Plenum Press, 2000.
36. Bockris J, Potter E. The mechanism of hydrogen evolution at nickel cathodes in aqueous solutions. J Chem Phys 2004; 20: 614.10.1063/1.1700503 ↗
37. Bond GM, Robertson IM, Birnbaum HK. On the determination of the hydrogen fugacity in an environmental cell TEM facility. Scr Metall 1986; 20: 653–658.10.1016/0036-9748(86)90484-9 ↗
38. Bouaziz O, Zurob H, Huang M. Driving force and logic of development of advanced high strength steels for automotive applications. Steel Res Int 2013; 84: 937–947.10.1002/srin.201200288 ↗
39. Brass AM, Chene J. Influence of deformation on the hydrogen behavior in iron and nickel base alloys: a review of experimental data. Mater Sci Eng A 1998; 242: 210–221.10.1016/S0921-5093(97)00523-6 ↗
40. Brass AM, Chanfreau A, Chêne J. Helium 3 precipitation in tritiated AISI 316 stainless steels. In: Thompson NW, Moody NR, editors. Hydrogen effects on material behavior. Warrendale: TMS, 1990: 19.
41. Briant CL, Banerji SK. Intergranular failure in steel: the role of grain boundary composition. Int Metall Rev 1978; 23: 164–199.10.1179/095066078790136652 ↗
42. Briant CL, Banerji SK. Treatise on materials science and technology: embrittlement of engineering alloys, New York: Academic Press, 1983.
43. Cailletet ML. Comptes Rendus 1868; 68: 847–850.
44. Calabrese L, Bonaccorsi L, Galeano M, Proverbio E, Pietro D, di Cappuccini F. Identification of damage evolution during SCC on 17-4 PH stainless steel by combining electrochemical noise and acoustic emission techniques. Corros Sci 2015; 98: 573–584.10.1016/j.corsci.2015.05.063 ↗
45. Callister WD, Rethwisch DG. Materials science and engineering: an introduction, Hoboken, NJ: John Wiley and Sons, Inc., 2014.
46. Carter TJ, Cornish LA. Hydrogen in metals. Eng Fail Anal 2001; 8: 113–121.10.1016/S1350-6307(99)00040-0 ↗
47. Chasse KR, Singh PM. Hydrogen embrittlement of a duplex stainless steel in alkaline sulfide solution. Corros J Sci Eng 2011; 67: 1–12.10.5006/1.3546848 ↗
48. Choo WY, Lee JY. Thermal analysis of trapped hydrogen in pure iron. Metall Trans 1982; 13A: 135–140.10.1007/BF02642424 ↗
49. Christmann K. Some general aspects of hydrogen chemisorption on metal surfaces. Prog Surf Sci 1995; 48: 15–26.10.1016/0079-6816(95)93412-Z ↗
50. Clum JA. The role of hydrogen in dislocation generation in iron alloys. Scr Metall 1975; 9: 51–58.10.1016/0036-9748(75)90145-3 ↗
51. Cohen M. Martensitic transformations in materials science and engineering. Trans JIM 1988; 29: 609–624.10.2320/matertrans1960.29.609 ↗
52. Conder RJ, Felton P, Burke R, Dent P. Hydrogen embrittlement testing of high strength low carbon martensitic steels, corrosion 2015, San Antonio, TX: NACE International, 2010.10.5006/C2010-10290 ↗
53. Cwiek J. Prevention methods against hydrogen degradation of steel. JAMME 2010; 43: 214–221.
54. Darken LS, Smith RP. Behavior of hydrogen in steel during and after immersion in acid. Corrosion 1949; 5: 1.10.5006/0010-9312-5.1.1 ↗
55. Dautovich DP, Floreen S. International Corrosion Conference – the stress corrosion and hydrogen embrittlement behavior of maraging steels. In: Proceedings, 1977: 798–815.
56. Davies RG. Influence of martensite composition and content on the properties of dual-phase steels. Metall Trans A 1978; 9A: 671–679.10.1007/BF02659924 ↗
57. Daw MS, Baskes MI. Application of embedded atom method to hydrogen embrittlement. In: Jones RH, Latanision RM, editors. Chemistry and physics of fracture. Netherlands: Martinus Nijhoff, 1987: 196–218.10.1007/978-94-009-3665-2_12 ↗
58. de Jong AM, Niemantsverdriet JW. Thermal desorption analysis: comparative test of ten commonly applied procedures. Surf Sci 1990; 233: 355–365.10.1016/0039-6028(90)90649-S ↗
59. Demeri MY. Advanced high-strength steels: science, technology and applications, Materials Park, OH: ASM International, 2013.10.31399/asm.tb.ahsssta.9781627082792 ↗
60. Depover T, Perez-Escobar D, Wallaert E, Zermout Z, Verbeken K. Effect of hydrogen charging on the mechanical properties of advanced high strength steels. Int J Hydrogen Energy 2014; 39: 4647–4656.10.1016/j.ijhydene.2013.12.190 ↗
61. Depover T, Monbaliu O, Wallaert E, Verbeken K. Effect of Ti, Mo and Cr based precipitates on the hydrogen trapping and embrittlement of Fe-C-X Q&T alloys. Int J Hydrogen Energy 2015; 40: 16977–16984.10.1016/j.ijhydene.2015.06.157 ↗
62. Devanathan MAV, Stachurski Z. The absorption and diffusion of electrolytic hydrogen in palladium. Proc R Soc 1962; A270: 90–102.10.1098/rspa.1962.0205 ↗
63. Devanathan MAV, Stachurski Z. The mechanism of hydrogen evolution in iron in acid solutions by determination of permeation rates. J Electrochem Soc 1964; 111: 619–623.10.1149/1.2426195 ↗
64. Dietzel W, Atrens A, Barnoush A. Mechanics of modern test methods and quantitative-accelerated testing for hydrogen embrittlement. In: Gangloff RP, Somerday BP, editors. Gaseous hydrogen embrittlement of materials in energy technologies. Woodhead Publishing Ltd., 2012.10.1533/9780857093899.2.237 ↗
65. Donovan JA. Accelerated evolution of hydrogen from metals during plastic deformation. Metall Trans 1976; 7A: 1677–1683.10.1007/BF02817885 ↗
66. Doshida T, Nakamura M, Saito H, Sawada T, Takai K. Hydrogen-enhanced lattice defect formation and hydrogen embrittlement of cyclically prestressed tempered martensitic steel. Acta Mater 2013; 61: 7755–7766.10.1016/j.actamat.2013.09.015 ↗
67. Ebrahimi Z, Krauss G. Mechanisms of tempered martensite embrittlement in medium carbon steels. Acta Metall 1984; 32: 1767–1777.10.1016/0001-6160(84)90233-5 ↗
68. Elboujdaini M, Revie RW. Metallurgical factors in stress corrosion cracking (SCC) and hydrogen-induced cracking (HIC). J Solid State Electrochem 2009; 13: 1091–1099.10.1007/s10008-009-0799-0 ↗
69. Eliaz N, Shachar A, Tal B, Eliezer D. Characteristics of hydrogen embrittlement, stress corrosion cracking and tempered martensite embrittlement in high-strength steels. Eng Fail Anal 2002; 9: 167–184.10.1016/S1350-6307(01)00009-7 ↗
70. Enomoto M, Hirakami D, Tarui T. Thermal desorption analysis of hydrogen in high strength martensitic steels. Metall Mater Trans A 2012; 43A: 572–581.10.1007/s11661-011-0909-3 ↗
71. Evers S, Senöz C, Rohwerder M. Hydrogen detection in metals: a review and introduction of a Kelvin probe approach. Sci Technol Adv Mater 2013; 14: 014201.10.1088/1468-6996/14/1/014201 ↗
72. Fenske JA, Robertson IM, Ayer R, Hukle M, Lillig D, Newbury B. Microstructure and hydrogen-induced failure mechanisms in Fe-Ni weldments. Metall Mater Trans A 2012; 43A: 3011–3022.10.1007/s11661-012-1129-1 ↗
73. Fernandez JF, Cuevas F, Sanchez C. Simultaneous differential scanning calorimetry and thermal desorption spectroscopy measurements for the study of the decomposition of metal hydrides. J Alloy Compd 2000; 298: 244–253.10.1016/S0925-8388(99)00620-9 ↗
74. Ferreira PJ, Robertson IM, Birnbaum HK. Hydrogen effects on the interaction between dislocations. Acta Metall 1998; 46: 1749–1757.10.1016/S1359-6454(97)00349-2 ↗
75. Figueroa D, Robinson MJ. Hydrogen transport and embrittlement in 300 M and AerMet100 ultra high strength steels. Corros Sci 2010; 52: 1593–1602.10.1016/j.corsci.2010.01.001 ↗
76. Fischer TE. Hydrogen on metal surfaces. In: Fiore NF, Berkowitz BJ, editors. Advanced techniques for characterizing hydrogen in metals. Met Soc AIME 1982: 135–148.
77. Flitt H, Bockris J. Hydrogen/metal interactions with special reference to electrochemical approaches. Int J Hydrogen Energy 1981; 6: 119–138.10.1016/0360-3199(81)90001-X ↗
78. Frappart S, Oudriss A, Feaugas X, Creus J, Bouhattate J, Thébault F, Delattre L, Marchebois H. Hydrogen trapping in martensitic steel investigated using electrochemical permeation and thermal desorption spectroscopy. Scr Mater 2011; 65: 859–862.10.1016/j.scriptamat.2011.07.042 ↗
79. Frappart S, Feaugas X, Creus J, Thebault F, Delattre L, Marchebois H. Hydrogen solubility, diffusivity and trapping in a tempered Fe-C-Cr martensitic steel under various mechanical stress states. Mater Sci Eng A 2012; 534: 384–393.10.1016/j.msea.2011.11.084 ↗
80. Fritzmeier LG, Chandler WT. Hydrogen-embrittlement – rocket motor applications. In: Superalloys, supercomposites and superceramics. Academic Press, 1989: 491–524.10.1016/B978-0-12-690845-9.50021-X ↗
81. Frommeyer G, Brüx U, Neumann P. Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes. ISIJ Int 2003; 43: 438–446.10.2355/isijinternational.43.438 ↗
82. Fuchigami H, Minami H, Nagumo M. Effect of grain size on the susceptibility of martensitic steel to hydrogen-related failure. Philos Mag Lett 2006; 86: 21–29.10.1080/09500830500482316 ↗
83. Fukai Y. Formation of superabundant vacancies in M-H alloys and some of its consequences: a review. J Alloy Compd 2003; 356–357: 263–269.10.1016/S0925-8388(02)01269-0 ↗
84. Fukushima H, Birnbaum HK. Surface and grain boundary segregation of deuterium in nickel. Acta Metall 1984; 32: 851–859.10.1016/0001-6160(84)90021-X ↗
85. Gamboa E, Atrens A. Environmental influence on the stress corrosion cracking of rock bolts. Eng Fail Anal 2003a; 10: 521–558.10.1016/S1350-6307(03)00036-0 ↗
86. Gamboa E, Atrens A. Stress corrosion cracking fracture mechanisms in rock bolts. J Mater Sci 2003b; 38: 3813–3829.10.1023/A:1025996620197 ↗
87. Gamboa E, Atrens A. Material influence on the stress corrosion cracking of rock bolts. Eng Fail Anal 2005; 12: 201–235.10.1016/j.engfailanal.2004.07.002 ↗
88. Gangloff RP. A review and analysis of the threshold for hydrogen embrittlement of steel. In: Levy M, Isserow S, editors. Corrosion prevention and control. Watertown, MA: U.S. Army Laboratory Command, Materials Technology Laboratory, 1986: 64–111.
89. Gangloff RP. Hydrogen assisted cracking of high strength alloys. In: Milne I, Ritchie RO, Karihaloo B, editors. Comprehensive structural integrity. Vol. 6, Environmentally assisted fracture. Elsevier, 2003: 31–101.10.1016/B0-08-043749-4/06134-6 ↗
90. Gangloff RP, Wei RP. Gaseous hydrogen embrittlement of high strength steels. Metall Trans A 1977; 8: 1043–1053.10.1007/BF02667388 ↗
91. García TE, Rodríguez C, Belzunce FJ, Peñuelas I, Arroyo B. Development of a methodology to study the hydrogen embrittlement of steels by means of the small punch test. Mater Sci Eng A 2015; 626: 342–351.10.1016/j.msea.2014.12.083 ↗
92. Garrison Jr WM, Moody NR. Hydrogen embrittlement of high strength steels. In: Gangloff RP, Somerday BP, editors. Gaseous hydrogen embrittlement of materials in energy technologies. Woodhead Publishing Ltd., 2012: 421–484.10.1533/9780857093899.3.421 ↗
93. Gerberich W. Effect of hydrogen on high-strength and martensitic steels. In: Bernstein IM, Thompson AW, editors. Hydrogen in metals. Metals Park, OH: ASM, 1974: 115–147.
94. Ghassemieh E. Materials in Automotive Application, State of the Art and Prospects. Available at: http://www.intechopen.com/. Retrieved July 14, 2014.
95. Gibala R, Kumnick AJ. Hydrogen trapping in iron and steel. In: Hehemann RF, Gibala R, editors. Hydrogen embrittlement and stress corrosion cracking: a Troiano Festschrift. OH: ASM, 1985: 61–77.
96. Goldstein J, Newbury DE, Joy DC, Lyman CE, Echlin P, Lifshin E, Sawyer L, Michael JR. Scanning Electron Microscopy and X-ray Microanalysis, 3rd ed., Springer-Verlag, 2003.10.1007/978-1-4615-0215-9 ↗
97. Grabke HJ, Gehrmann F, Riecke E. Hydrogen in microalloyed steels. Steel Res Int 2001; 72: 225–235.10.1002/srin.200100110 ↗
98. Grässel O, Krüger L, Frommeyer G, Meyer LW. High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development – properties – application. Int J Plasticity 2000; 16: 1391–1409.10.1016/S0749-6419(00)00015-2 ↗
99. Hagihara Y, Shobu T, Hisamori N, Suzuki H, Takai K, Hirai K. Delayed fracture using CSRT and hydrogen trapping characteristics of V-bearing high-strength steel. ISIJ Int 2012; 52: 298–306.10.2355/isijinternational.52.298 ↗
100. Ham J, Jang Y, Lee G, Kim B, Rhee K, Cho C. Evaluation method of sensitivity of hydrogen embrittlement for high strength bolts. Mater Sci Eng A 2013; 581: 83–89.10.1016/j.msea.2013.06.012 ↗