Localized corrosion and stress corrosion cracking of stainless steels in halides other than chlorides solutions: a review
Source abstract
Abstract
Abstract Fluorides, bromides, and iodides, despite being less common than chlorides, are present in various environments of industrial relevance. Stainless steels suffer pitting corrosion in solutions of all halides except fluorides, which can be understood considering that fluoride is the anion of a weak acid. The aggressiveness of the rest of the halides for pitting corrosion is on the order Cl − > Br − > I − for stainless steels with Mo content below 3 wt.%. Mo is not as effective in inhibiting Br − pitting corrosion as it is for inhibiting Cl − pitting corrosion. Most of those observations were rationalized based on the effect of anions on pit growth kinetics. Sensitized austenitic stainless steel suffers stress corrosion cracking (SCC) in solutions of all halides, albeit chlorides seem to be the most aggressive. Fluoride SCC is relevant for SCC under insulation of stainless steels, and standards and regulations developed to mitigate this problem consider this ion as aggressive as chloride. For the solubilized stainless steels, aggressiveness toward SCC is in the order Cl − > Br − . The SCC of solubilized stainless steels was not observed in solutions of F − and I − , and the possible reasons for this fact are discussed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Instituto Sabato (UNSAM/CNEA), CONICET, Comisión Nacional de Energía Atómica , Av. Gral. Paz 1499, San Martín , Buenos Aires 1650 , Argentina
References (100+)
Show source-provided references
1. Abd El Meguid EA. Pitting corrosion behavior of type 904L stainless steel in sodium bromide solutions. Corrosion 1997; 53: 623–630.10.5006/1.3290295 ↗
2. Abd El Rehim SS, Abd El Wahaab SM, Abdel Maguid EA. Electrochemical behaviour of nickel anode in H2SO4 solutions and the effect of halide ions. Mater Corros 1986; 37: 550–555.10.1002/maco.19860371006 ↗
3. Acello SJ, Greene ND. Anodic protection of austenitic stainless steels in sulfuric acid-chloride media. Corrosion 1962; 18: 286t–290t.10.5006/0010-9312-18.8.286 ↗
4. Ahluwalia HS. Corrosion under insulation. In: Cramer SD, Covino BS, editors. ASM handbook Vol. 13C: corrosion: environments and industries. Materials Park, OH: ASM International, 2006: 654–658.10.31399/asm.hb.v13c.a0004177 ↗
5. Andresen PL. Stress corrosion cracking of current structural materials in commercial nuclear power plants. Corrosion 2013; 69: 1024–1038.10.5006/0801 ↗
6. Andresen PL. A brief history of environmental cracking in hot water. Corrosion 2019; 75: 240–253.10.5006/2881 ↗
7. Andresen PL, Ford PF. Life prediction by mechanistic modeling and system monitoring of environmental cracking of iron and nickel alloys in aqueous systems. Mater Sci Eng A 1988; A103: 167–184.10.1016/0025-5416(88)90564-2 ↗
8. Asawa M. Stress corrosion cracking of 18-8 austenitic stainless steel in sulfuric acid. Tetsu-to-Hagane 1971; 57: 1340–1349.10.2355/tetsutohagane1955.57.8_1340 ↗
9. Asawa M. Stress corrosion cracking regions on contour maps of dissolution rates for AISI 304 stainless steel in sulfuric acid solutions with chloride, bromide, or iodide. Corrosion 1987; 43: 198–203.10.5006/1.3583136 ↗
10. ASTM A380-17. Standard practice for cleaning, descaling, and passivation of stainless steel parts, equipment, and systems. West Conshohocken, PA: ASTM, 2017.
11. ASTM C692-13. Standard test method for evaluating the influence of thermal insulations on external stress corrosion cracking tendency of austenitic stainless steel. West Conshohocken, PA: ASTM, 2018.
12. ASTM C795-08. Standard specification for thermal insulation for use in contact with austenitic stainless steel. West Conshohocken, PA: ASTM, 2018.
13. ASTM C871-18. Standard test methods for chemical analysis of thermal insulation materials for leachable chloride, fluoride, silicate, and sodium ions. West Conshohocken, PA: ASTM, 2018.
14. Berry WE, White EL, Boyd WK. Stress corrosion cracking of sensitized stainless steel in oxygenated high temperature water. Corrosion 1973; 29: 451–469.10.5006/0010-9312-29.12.451 ↗
15. Black DW, Morris RM. Experience in commissioning large desalination plants in the middle east. Desalination 1981; 39: 229–239.10.1016/S0011-9164(00)86127-5 ↗
16. Bocher F, Huang R, Scully JR. Prediction of critical crevice potentials for Ni-Cr-Mo alloys in simulated crevice solutions as a function of molybdenum content. Corrosion 2010; 66: 055002-1–055002-15.10.5006/1.3430462 ↗
17. Brauns E, Ternes H. Untersuchungen Über Die Transkristalline Spannungsrißkorrosion Austenitischer Chrom-Nickel-Stähle in Heißen Chloridlösungen. Werkstoffe Korros 1968; 19: 1–19.10.1002/maco.19680190102 ↗
18. Brown BF. Stress corrosion cracking control measures (NBS Monograph 156). Washington, DC: National Bureau of Standards, 1977.10.21236/ADA043000 ↗
19. Carroll WM, Lynskey EE. A crevice-free electrode assembly for the determination of reproducible breakdown potentials for stainless steels in halide environments. Corros Sci 1994; 36: 1667–1678.10.1016/0010-938X(94)90061-2 ↗
20. Chambers C, Holliday AK. Modern inorganic chemistry. London, U.K.: Butterworth & Co., 1975.
21. Chandler T. Absorption chiller corrosion protection-SBIR Phase I Final Report – DOE Grant DE-FG03-98ER82658, 1999.
22. Che-Sheng Chen P, Shinohara T, Tsujikawa S. Applicability of the competition concept in determining the stress corrosion cracking behavior of austenitic stainless steels in chloride solutions. Zairyo-to-Kankyo 1997; 46: 313–320.10.3323/jcorr1991.46.313 ↗
23. Chung HM, Ruther WE, Sanecki JE, Hins A, Zaluzec NJ, Kassner TF. Irradiation-assisted stress corrosion cracking of austenitic stainless steels: recent progress and new approaches. J Nucl Mater 1996; 239: 61–79.10.1016/S0022-3115(96)00677-0 ↗
24. Congleton J, Sui G. The stress corrosion cracking of heavily sensitized type 316 stainless steel in water in the temperature range 50–100°C. Corros Sci 1992; 33: 1691–1717.10.1016/0010-938X(92)90003-L ↗
25. Cox B. Environmentally induced cracking of zirconium alloys. Corrosion 1972; 28: 207–217.10.5006/0010-9312-28.6.207 ↗
26. Cragnolino G, Macdonald DD. Intergranular stress corrosion cracking of austenitic stainless steel at temperatures below 100°C – a review. Corrosion 1982; 38: 406–424.10.5006/1.3577354 ↗
27. Cragnolino G, Lin LF, Szklarska-Smialowska Z. Stress corrosion cracking of sensitized type 304 stainless steel in sulfate and chloride solutions at 250°C and 100°C. Corrosion 1981; 37: 312–320.10.5006/1.3577279 ↗
28. Cragnolino GA, Dunn DS, Sridhar N. Environmental effects on stress corrosion cracking of type 316l stainless steel and alloy 825 as high-level nuclear waste container materials, Prepared for Nuclear Regulatory Commission, CNWRA 94-028. San Antonio, TX: Center for Nuclear Waste Regulatory Analyses, 1994.10.5006/C1995-95159 ↗
29. Cragnolino G, Dunn DS, Sridhar N. Environmental factors in the stress corrosion cracking of type 316l stainless steel and alloy 825 in chloride solutions. Corrosion 1996; 52: 194–203.10.5006/1.3292114 ↗
30. Crouse PL. Fluorine: a key enabling element in the nuclear fuel cycle. J South Afr Inst Min Met 2015; 115: 931–935.10.17159/2411-9717/2015/v115n10a5 ↗
31. Dana AW. Stress-corrosion cracking of insulated austenitic stainless steel. ASTM Bull 1957; 225: 46–52.
32. Dana AW, Delong WB. Topic of the month – stress-corrosion cracking test. Corrosion 1956; 12: 19–20.10.5006/0010-9312-12.7.19 ↗
33. Davis JR. Stainless steels ASM specialty handbook. Materials Park, OH: ASM International, 1994.
34. de Castro MAC, Wilde BE. The corrosion and passivation of iron in the presence of halide ions in aqueous solution. Corros Sci 1979; 19: 923–936.10.1016/S0010-938X(79)80084-0 ↗
35. Domínguez-Aguilar MA, Newman RC. Detection of deleterious phases in duplex stainless steel by weak galvanostatic polarization in alkaline solution. Corros Sci 2006; 48: 2577–2591.10.1016/j.corsci.2005.08.018 ↗
36. Downs JD, Harris M, Benton W, Howard SK, Billingham M. New insights into the potential for environmental cracking of corrosion resistant alloys in high-density formate and bromide well completion brines at high temperature. Corrosion/2007, Paper 07097. Houston, TX: NACE International, 2007.10.5006/C2007-07097 ↗
37. Ernst P, Newman RC. The interaction between alloyed molybdenum and dissolved bromide in the pitting corrosion of stainless steels. Electrochem Solid-State Lett 2008; 11: C1–C4.10.1149/1.2801877 ↗
38. Evans GJ, Nugraha T. A study of the kinetics of I2 deposition on stainless steel sampling lines. Nucl Technol 2002; 140: 315–327.10.13182/NT02-A3342 ↗
39. Ford FP, Povich MJ. The effect of oxygen temperature combinations on the stress corrosion susceptibility of sensitized type 304 stainless steel in high purity water. Corrosion 1979; 35: 569–574.10.5006/0010-9312-35.12.569 ↗
40. Ford FP, Silverman M. The prediction of stress corrosion cracking of sensitized 304 stainless steel in 0.01 M Na2SO4 at 97°C. Corrosion 1980; 36: 558–565.10.5006/0010-9312-36.10.558 ↗
41. Francis R, Hebdon S. The selection of stainless steels for seawater pumps. Corrosion/2015, Paper C2015-5446. Houston, TX: NACE International, 2015.10.5006/C2015-05446 ↗
42. Frankel GS. Pitting corrosion of metals – a review of the critical factors. J Electrochem Soc 1998; 145: 2186–2198.10.1149/1.1838615 ↗
43. Frankel GS, Li T, Scully JR. Localized corrosion: passive film breakdown vs pit growth. J Electrochem Soc 2017; 164: 180–181.10.1149/2.1381704jes ↗
44. Galvele JR. Transport processes and the mechanism of pitting of metals. J Electrochem Soc 1976; 123: 464–474.10.1149/1.2132857 ↗
45. Gaudet GT, Mo WT, Hatton TA, Tester JW, Tilly J, Isaacs HS, Newman RC. Mass transfer and electrochemical kinetic interactions in localized pitting corrosion. AIChe J 1986; 32: 949–958.10.1002/aic.690320605 ↗
46. Greenwood NN, Earnshaw A. Chemistry of the elements, 2nd ed. Oxford, UK: Butterworth-Heinemann, 1997.
47. Griess JC, DeVan JH, Perez Blanco H. ORNL/TM-9646 Corrosion of materials in absorption heating and refrigeration fluids. Oak Ridge, TN: Oak Ridge National Laboratory, 1985.10.2172/5415292 ↗
48. Gui F, Cao L, Thodla R, Sridhar N. Localized corrosion and stress corrosion cracking of corrosion resistant alloys in H2S containing environment. Corrosion/2014, Paper 4482. Houston, TX: NACE International, 2014.
49. Guiñon JL, Garcia-Anton J, Pérez-Herranz V, Lacoste G. Corrosion of carbon steels, stainless steels, and titanium in aqueous lithium bromide solution. Corrosion 1994; 50: 240–246.10.5006/1.3293516 ↗
50. Guo R, Ives MB. Pitting susceptibility of stainless steels in bromide solutions at elevated temperatures. Corrosion 1990; 46: 125–129.10.5006/1.3585076 ↗
51. Hänninen HE. Influence of metallurgical variables on environment-sensitive cracking of austenitic alloys. Int Met Rev 1979; 24: 85–136.10.1179/095066079790136372 ↗
52. Harris DC. Quantitative chemical analysis, 7th ed. New York: Freeman and Company, 2007.
53. Haruyama S. Stress corrosion cracking by cooling water of stainless steel shell and tube heat exchangers. Mater Perform 1982; 21: 14–19.
54. Hodgkiess T, Ng NK, Argyropoulos P. The corrosion behaviour of a number of materials exposed to bromine-containing environments. Desalination 1985; 55: 229–246.10.1016/0011-9164(85)80075-8 ↗
55. Horvath J, Uhlig HH. Critical Potentials for pitting corrosion of Ni, Cr-Ni, Cr-Fe, and related stainless steels. J Electrochem Soc 1968; 115: 791–795.10.1149/1.2411433 ↗
56. Huang YL, Cao CN, Lu M, Lin HC. Inhibition effects of I− and I2 on stress corrosion cracking of stainless steel in acidic chloride solutions. Corrosion 1993; 49: 644–649.10.5006/1.3316095 ↗
57. Hutto FB, Tissot RG, Whitaker TE. A new apparatus and test procedure for running ASTM C 692 stress corrosion cracking tests. In: Pollock WI, Barnhart JM, editors. Corrosion of Metals Under Thermal Insulation, ASTM STP 880. Philadelphia, PA: American Society for Testing and Materials, 1985: 211–219.10.1520/STP39171S ↗
58. IAEA-Nuclear Energy Series. Stress corrosion cracking in light water reactors: good practices and lessons learned. Vienna, Austria: International Atomic Energy Agency, 2011.
59. Igual Muñoz A, García Antón J, Guiñón JL, Pérez Herranz V. Corrosion behavior and galvanic coupling of stainless steels, titanium, and alloy 33 in lithium bromide solutions. Corrosion 2003; 59: 606–615.10.5006/1.3277591 ↗
60. ISO 21457:2010(E) International Standard. Petroleum, petrochemical and natural gas industries – materials selection and corrosion control for oil and gas production systems. Geneva, Switzerland: ISO, 2010.
61. Ito K. Determination of iodide in natural water by ion chromatography. Anal Chem 1988; 69: 3628–3632.10.1021/ac9700787 ↗
62. Itzhak D, Elias O. Behavior of type 304 and type 316 austenitic stainless steels in 55 % lithium bromide heavy brine environments. Corrosion 1994; 50: 131–137.10.5006/1.3293501 ↗
63. Itzhak D, Eliezer D. The stress corrosion cracking of welded austenitic stainless steels in MgCl2 solutions in the presence of NaI additions. Corros Sci 1983; 23: 1285–1291.10.1016/0010-938X(83)90078-1 ↗
64. Itzhak D, Elias O, Greenberg Y. Behavior of type 316 austenitic stainless steel under slow strain rate technique conditions in lithium bromide heavy brine environments. Corrosion 1996; 52: 72–78.10.5006/1.3292098 ↗
65. Janik-Czachor M. Effect of halide ions on the nucleation of corrosion pits in iron. Mater Corros 1979; 30: 255–257.10.1002/maco.19790300405 ↗
66. Jesionek M, Szklarska-Smialowska Z. The inhibition of the dissolution of iron in sulfuric acid by halide ions. Corros Sci 1983; 23: 183–187.10.1016/0010-938X(83)90115-4 ↗
67. Kaneko M, Isaacs HS. Pitting of stainless steel in bromide, chloride and bromide/chloride solutions. Corros Sci 2000; 42: 67–78.10.1016/S0010-938X(99)00056-6 ↗
68. Kaneko M, Isaacs HS. Effects of molybdenum on the pitting of ferritic- and austenitic-stainless steels in bromide and chloride solutions. Corros Sci 2002; 44: 1825–1834.10.1016/S0010-938X(02)00003-3 ↗
69. Khalil W, Haupt S, Strehblow HH. The thinning of the passive layer of iron by halides. Werkstoffe Korros 1985; 36: 16–21.10.1002/maco.19850360104 ↗
70. Kiselevskii VN, Kovalev VV, Neklyudov IM, Ozhigov LS. Corrosion-cracking resistance of austenitic stainless steel under stress in an iodine medium. Strength Mater 1993; 25: 864–869.10.1007/BF00774631 ↗
71. Koch GH. Localized corrosion in halides other than chlorides. Mater Perform 1993; 32: 54–58.10.5006/C1993-93437 ↗
72. Kolotyrkin JAM. Pitting corrosion of metals. Corrosion 1963; 19: 261t–268t.10.5006/0010-9312-19.8.261 ↗
73. Kumada M. Bromide stress corrosion cracking of stainless steels in high-temperature water. Zairyo-To-Kankyo 1996; 45: 284–291.10.3323/jcorr1991.45.284 ↗
74. Ladwig KJ, Blythe GM. Flue-gas desulfurization products and other air emissions controls. In: Robl T, Oberlink A, Jones R, editors. Coal combustion products (CCP’s) characteristics, utilization and beneficiation. Duxford, United Kingdom: Woodhead Publishing, 2017: 67–95.10.1016/B978-0-08-100945-1.00003-4 ↗
75. Laycock NJ, Newman RC. Localised dissolution kinetics, salt films and pitting potentials. Corros Sci 1997; 39: 1771–1790.10.1016/S0010-938X(97)00049-8 ↗
76. Lee WSW, Oldfield OW, Todd B. Corrosion problems caused by bromine formation in additive dosed MSF desalination plants. Desalination 1983; 44: 209–221.10.1016/0011-9164(83)87120-3 ↗
77. Li T, Scully JR, Frankel GS. Localized corrosion: passive film breakdown vs. pit growth stability: Part III. A unifying set of principal parameters and criteria for pit stabilization and salt film formation. J Electrochem Soc 2018; 165: 762–770.10.1149/2.0251811jes ↗
78. Li T, Scully JR, Frankel GS. Localized corrosion: passive film breakdown vs. pit growth stability: Part V. Validation of a new framework for pit growth stability using one-dimensional artificial pit electrodes. J Electrochem Soc 2019; 166: C3341–C3354.10.1149/2.0431911jes ↗
79. Lide DR, editor. CRC handbook of chemistry and physics. Boca Raton, FL: CRC Press, 2005.
80. Lillard RS. A review of corrosion issues related to uranyl nitrate base aqueous homogeneous reactors. Corros Eng Sci Technol 2010; 45: 194–203.10.1179/147842210X12659647007121 ↗
81. Liu Y, Xu LN, Zhu JY, Meng Y. Pitting corrosion of 13Cr steel in aerated brine completion fluids. Mater Corros 2014; 65: 1096–1102.10.1002/maco.201307489 ↗
82. Lobb RC. The effect of iodine vapour on creep rupture properties of nitride 20% Cr/25% Ni/Nb/1.5 Ti stainless steel. J Nucl Mater 1978; 74: 212–220.10.1016/0022-3115(78)90360-4 ↗
83. Lobb RC, Jones RB. The influence of iodine vapour on creep rupture properties Of20%Cr/25%Ni/Nb stabilised stainless steel. J Nucl Mater 1976; 59: 280–292.10.1016/0022-3115(76)90060-X ↗
84. Lobb RC, Nicholson RD. The effect of iodine vapour on the creep rupture properties of M316 stainless steel. Mater Sci Eng 1976; 22: 157–165.10.1016/0025-5416(76)90148-8 ↗
85. Macdonald DD, Lei X. Theoretical interpretation of anion size effects in passivity. J Electrochem Soc 2016; 163: 738–744.10.1149/2.0571613jes ↗
86. Malik AU, Siddiqi NA, Andijani IN. Corrosion behavior of some highly alloyed stainless steels in seawater. Desalination 1994; 97: 189–197.10.1016/0011-9164(94)00086-7 ↗
87. Malik AU, Siddiqi NA, Ahmad S, Andijani IN. The effect of dominant alloy additions on the corrosion behavior of some conventional and high alloy stainless steels in seawater. Corros Sci 1995; 37: 1521–1535.10.1016/0010-938X(95)00043-J ↗
88. Mankowski J, Szklarska-Smialowska Z. Studies on accumulation of chloride ions in pits growing during anodic polarization. Corros Sci 1975; 15: 493–501.10.1016/0010-938X(75)90015-3 ↗
89. Mccoubrey JC. The acid strength of the hydrogen halides. Trans Faraday Soc 1955; 51: 743–747.10.1039/tf9555100743 ↗
90. McIntyre D. Factors affecting the stress corrosion cracking of austenitic stainless steels under thermal insulation. In: Pollock WI, Barnhart JM, editors. Corrosion of metals under thermal insulation, ASTM STP 880. Philadelphia, PA: American Society for Testing and Materials, 1985: 27–41.10.1520/STP39154S ↗
91. MIL-I-24244A. Insulation materials, thermal, with special corrosion and chloride requirements. Military Specification, 1974.
92. NACE International SP0198. Standard practice control of corrosion under thermal insulation and fireproofing materials – a systems approach. Houston, TX: NACE International, 2017.
93. Newman RC. 2001 W.R. Whitney Award Lecture: understanding the corrosion of stainless steel. Corrosion 2001; 57: 1030–1041.10.5006/1.3281676 ↗
94. Nguyen VA, Carcea AG, Ghaznavi M, Newman RC. The effect of cation complexation on the predicted “B” value in Galvele’s pit model. J Electrochem Soc 2019; 166: C3297–C3304.10.1149/2.0281911jes ↗
95. Nordin S. Studies on stainless steels for service in desalination plants. Desalination 1983; 44: 255–263.10.1016/0011-9164(83)87124-0 ↗
96. Norsok Standard M-001-Materials Selection. Standards Norway, Lysaker, Norway, 2014.
97. O’Dell CS, Brown BF. Control of stress corrosion cracking by inhibitors (a review of the literature). Washington, DC: Chemistry Department, The American University, 1978.10.6028/NBS.MONO.156 ↗
98. O’Dell CS, Brown BF, Foley RT. An exploratory study of inhibition of intergranular stress corrosion cracking in sensitized type 304 stainless steel. Corrosion 1980; 36: 183–200.10.5006/0010-9312-36.4.183 ↗
99. Ohtsu T, Miyazawa M. Materials selection and corrosion management in a process containing halides, Corrosion/2012, Paper C2012-0001352. Houston, TX: NACE International, 2012.10.5006/C2012-01352 ↗
100. Oldfield JW, Todd B. Corrosion problems caused by bromine formation in MSF desalination plants. Desalination 1981; 38: 233–245.10.1016/S0011-9164(00)86070-1 ↗