Hydrogen in metallic alloys ─ embrittlement and enhanced plasticity: a review
Source abstract
Abstract
Abstract The evolution of ideas concerning the nature of hydrogen embrittlement of engineering metallic materials is described based on a number of the proposed hypotheses and corresponding experiments. The main attention is paid to two of them, namely hydrogen-enhanced decohesion (HEDE) and hydrogen-enhanced localized plasticity (HELP). Recent attempts to interconnect the both models as HELP + HEDE and HELP-mediated HEDE ones are also estimated. A conclusion is made that HELP model is preferential for understanding the entire array of experimental data with a caveat that it is necessary to consider the chemical nature of hydrogen atoms and view them not only as point defects. Based on the studies of hydrogen effect on the atomic interactions in iron, nickel, titanium, and its alloys, it is shown that the electron approach to HELP phenomenon adequately describes two competitive features of hydrogen behavior in metals: increased brittleness and enhanced plasticity. Due to the increase in the concentration of free electrons, hydrogen decreases the elasticity moduli, which causes the crystal lattice to soften. For this reason, the formation of hydrogen atmospheres around the dislocations decreases the start stress of dislocation sources, as well as line tension of emitted dislocations, enhancing thereby their mobility, and weakens repulsion between dislocations in their pile-ups. The range of temperatures and strain rates in which hydrogen embrittlement occurs is controlled by the enthalpies of hydrogen atoms’ diffusion and their binding to dislocations. The resulting consequences for mechanical properties depend on the short-range atomic order, SRO, which inherently occurs in the metallic solid solutions and localizes plastic deformation both in the cases of short-range atomic ordering and of short-range atomic decomposition. Hydrogen enhances slip localization because of its different solubility in the submicrovolumes of short-range decomposed solid solutions. If SRO is absent or not remarkably formed, the hydrogen-increased concentration of free electrons results in enhanced plasticity. Available positive hydrogen effects on the plasticity of titanium β-alloys and austenitic steels are presented and interpreted.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
G.V. Kurdyumov Institute for Metal Physics, National Academy of Sciences of Ukraine , Kyiv 03142 , Ukraine
References (100+)
Show source-provided references
1. Alvaro, A., Thue Jensen, I., Kheradmand, N., Lovvik, O.M., and Olden, V. (2015). Hydrogen embrittlement in nickel, revisited by first principles modeling, cohesive zone simulation and nanomechanical testing. Int. J. Hydrogen Energy 40: 16892–16900, https://doi.org/10.1016/j.ijhydene.2015.06.069.10.1016/j.ijhydene.2015.06.069 ↗
2. Anisimova, L.I., Aksenov, Yu.A., Badaeva, M.G., Vas`ko, N.V., Kolmogorov, V.L., and Mozhaiskii, V.S. (1992). Reversible alloying with hydrogen and deformation of the titanium alloy VT6. Met. Sci. Heat Treat. 34: 143–147, https://doi.org/10.1007/BF00769883.10.1007/BF00769883 ↗
3. Asano, S. and Otsuka, R. (1976). The lattice hardening due to dissolved hydrogen in iron and steel. Scr. Mater. 10: 1015–1020, https://doi.org/10.1016/0036-9748(76)90119-8.10.1016/0036-9748(76)90119-8 ↗
4. Ashok, S., Stoloff, N.S., Glicksman, M.E., and Slavin, T. (1981). Liquid metal and hydrogen embrittlement of amorphous alloys. Scr. Metall. 15: 331–337, https://doi.org/10.1016/0036-9748(81)90355-0.10.1016/0036-9748(81)90355-0 ↗
5. Bader, R.F.W. (1995). Theory of atoms in molecules, Available at: http://www.chemistry.mcmaster.ca/bader/aim.
6. Bader, R.F.W. (1998). Atoms in molecules. In: Encyclopedia of computational chemistry. John Wiley & Sons Inc., Hoboken, p. 64.10.1002/0470845015.caa012 ↗
7. Baranowski, B. (1959). The kinetics of saturation of electrolytic nickel layers with cathodic hydrogen. Bull. Acad. Polon. Sci. 7: 907.
8. Bastien, P. and Azou, P. (1951). Influence de l’écrouissage sur le frottement intérieur du fer et del’acier, chargés ou non en hydrogéne. C. R. Acad. Sci. Paris 232: 1845–1848.
9. Beachem, C.D. (1972). A new model for hydrogen-assisted cracking (hydrogen “embrittlement”). Metall. Mater. Trans. 3: 441–455, https://doi.org/10.1007/bf02642048.10.1007/BF02642048 ↗
10. Beavers, J. and Bubenik, T.A (2017). Stress corrosion cracking, Ch.12. In: El-Sherik, A.M. (Ed.). Trends in oil and gas corrosion research and technologies. Woodhead Publishing Series in Energy, Boston, pp. 295–314.10.1016/B978-0-08-101105-8.00012-7 ↗
11. Bernstein, I.M., Garber, R., and Presouyre, G.M. (1975). Effect of dissolved hydrogen on mechanical behavior of metals. In: Thompson, A.W. and Bernstein, I.M. (Eds.), Effect of hydrogen on behavior of materials. TMS-AIME, New York, pp. 37–58.
12. Bertch, K.M., Wang, S., Nagao, A., and Robertson, I.M. (2019). Hydrogen-induced compatibility constraints across grain boundary drive intergranular failure of Ni. Mater. Sci. Eng. A 760: 58–67, https://doi.org/10.1016/j.msea.2019.05.36.10.1016/j.msea.2019.05.036 ↗
13. Bilby, B.A. and Hewitt, J. (1962). Hydrogen in steel – the stability of micro-cracks. Acta Metall. 10: 587–600, https://doi.org/10.1016/0001-6160(62)90048-2.10.1016/0001-6160(62)90048-2 ↗
14. Birnbaum, H.K. (1978). Hydrogen related failure mechanisms in metals. Technical report for Office of Naval Research, AD-A064 854. University of Illinoice at Urbana-Champaign, Illinoice 61801, USA.
15. Birnbaum, H.K., Buckley, C., Zeides, S., Sirois, E., Rozenak, P., Spooner, S., and Lin, J.S. (1997). Hydrogen in aluminum. J. Alloys Compd. 253–254: 260–264, https://doi.org/10.1016/S0925-8388(96)02968-4.10.1016/S0925-8388(96)02968-4 ↗
16. Birnbaum, H.K. and Sofronis, P. (1994). Hydrogen-enhanced localized plasticity – a mechanism for hydrogen-related fracture. Mater. Sci. Eng. A 176: 191–202, https://doi.org/10.1016/0921-5093(94)90975-x.10.1016/0921-5093(94)90975-X ↗
17. Bobyr, A.M., Bugaev, V.N., and Smirnov, A.A. (1991). Rep. Acad. Sci. USSR 320: 1113–1115.
18. Bond, G., Robertson, I., and Birnbaum, H. (1988). Effects of hydrogen on deformation and fracture processes in high-purity aluminum. Acta Metall. 36: 2193–2197, https://doi.org/10.1016/0001-6160(88)90320-3.10.1016/0001-6160(88)90320-3 ↗
19. Boniszewski, T. and Smith, G.C. (1963). The influence of hydrogen on the plastic deformation ductility and fracture of nickel in tension. Acta Metall. 11: 165–178, https://doi.org/10.1016/0001-6160(63)90209-8.10.1016/0001-6160(63)90209-8 ↗
20. Carter, C.B. and Holmes, S.M. (1977). The stacking-fault energy of nickel. Philos. Mag. 35: 1161–1172, https://doi.org/10.1080/14786437708232942.10.1080/14786437708232942 ↗
21. Charnock, W. and Nutting, J. (1967). The effect of carbon and nickel upon the stacking fault energy. Met. Sci. 1: 123–127, https://doi.org/10.1179/msc.1967.1.1.123.10.1179/msc.1967.1.1.123 ↗
22. Chen, S.H., Katz, Y., and Gerberich, W.W. (1991). Crack-tip strain fields and fracture microplasticity in hydrogen-induced cracking of Fe-3 wt% Si single crystals. Philos. Mag. A 63: 131–155, https://doi.org/10.1080/01418619108204598.10.1080/01418619108204598 ↗
23. Chen, S.R. and Tang, D. (1990). Effect of interstitial atom concentration on lattice parameters of martensite and retained austenite in iron-carbon-nitrogen alloys. Mater. Sci. Forum 56-58: 201–206.10.4028/www.scientific.net/MSF.56-58.201 ↗
24. Cowley, J.M. (1950). X-ray measurement of order in single crystals of Cu3Au. J. Appl. Phys. 21: 24–30, https://doi.org/10.1063/1.1699415.10.1063/1.1699415 ↗
25. Cuitiño, A.M. and Ortiz, M. (1996). Ductile fracture by vacancy condensation in f.c.c. single crystals. Acta Mater. 44: 427–436, https://doi.org/10.1016/1359-6454(95)00220-0.10.1016/1359-6454(95)00220-0 ↗
26. Degallaix, S., Dickson, J.I., and Foct, J. (1989). Effect of nitrogen on fatigue and creep-fatigue behavior of austenitic stainless steels. In: Foct, J. and Hendr, A. (Eds.), High nitrogen steels, HNS 88. Institute of Metals, London, pp. 380–386.
27. Delafosse, D. (2012). Hydrogen effects on the plasticity of fcc crystals. In: Gangloff, R.P. and Somerday, B.P. (Eds.), Gaseous hydrogen embrittlement of materials in energy technologies. Woodhead Publishing, Cambridge, UK, pp. 247–285.10.1533/9780857095374.2.247 ↗
28. Delafosse, D. and Magnin, T. (2001). Hydrogen induced plasticity in stress corrosion cracking of engineering systems. Eng. Fract. Mech. 68: 693–729, https://doi.org/10.1016/s0013-7944(00)00121-1.10.1016/S0013-7944(00)00121-1 ↗
29. Deng, Y. and Barnoush, A. (2018). Hydrogen embrittlement revealed via novel in situ fracture experiments using notched micro-cantilever specimens. Acta Mater. 142: 236–247, https://doi.org/10.1016/j.actamat.2017.09.057.10.1016/j.actamat.2017.09.057 ↗
30. Ding, Y., Yu, H., Zhao, K., Lin, M., Xiao, S., Ortiz, M., He, J., and Zhang, Z. (2021). Hydrogen-induced transgranular to intergranular fracture transition in bi-crystalline nickel. Scr. Mater. 204: 114–122, https://doi.org/10.1016/j.scriptamat.2021.114122.10.1016/j.scriptamat.2021.114122 ↗
31. Djukic, M.B., Bakic, G.M., Sijacki Zeravcic, V., Sedmak, A., and Rajicic, B. (2019). The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion. Eng. Fract. Mech. 216: 106528, https://doi.org/10.1016/j.engfracmech.2019.106528.10.1016/j.engfracmech.2019.106528 ↗
32. Djukic, M.B., Bakic, G.M., Zeravcic, V.S., Sedmak, A., and Rajicic, B. (2016). Hydrogen embrittlement of industrial components: prediction, prevention, and models. Corrosion 72: 943–961, https://doi.org/10.5006/1958.10.5006/1958 ↗
33. Djukic, M.B., Zeravcic, V.S., Bakic, G.M., Sedmak, A., and Rajicic, B. (2014). Hydrogen embrittlement of low carbon structural steel. Procedia Mater. Sci. 3: 1167–1172, https://doi.org/10.1016/j,mspro.2014.06.190.10.1016/j.mspro.2014.06.190 ↗
34. Djukic, M.B., Zeravcic, V.S., Bakic, G.M., Sedmak, A., and Rajicic, B. (2015). Hydrogen damage of steels: a case study and hydrogen embrittlement model. Eng. Failure Anal. 58: 485–498.10.1016/j.engfailanal.2015.05.017 ↗
35. Dmytrakh, I.M., Syrotyuk, A.M., and Leshchak, R.L. (2018). Specific features of the deformation and fracture of low-alloy steels in hydrogen-containing media: influence of hydrogen concentration in the metal. Mater. Sci. 54: 295–308, https://doi.org/10.1007/s11003-018-0186-z.10.1007/s11003-018-0186-z ↗
36. Dmytrakh, M., Leshchak, R.L., and Syrotyuk, A.M. (2015). Effect of hydrogen concentration on strain behaviour of pipeline steel. Int. J. Hydrogen Energy 40: 4011–4018, https://doi.org/10.1016/j.ijhydene.2015.01.094.10.1016/j.ijhydene.2015.01.094 ↗
37. Eastman, I., Matsumoto, T., Narita, N., Heubaum, F., and Birnbaum, H.K. (1980). Hydrogen effects in nickel-embrittlement or enhanced ductility. In: Bernstein, I.M. and Thompson, A.W. (Eds.), Proc intern conf on hydrogen in metals. AIME, New York, pp. 397–409.
38. Eliezer, D., Eliaz, N., Senkov, O., and Froes, F. (2000). Positive effects of hydrogen in metals. Mater. Sci. Eng. A 280: 220–224, https://doi.org/10.1016/s0921-5093(99)00670-x.10.1016/S0921-5093(99)00670-X ↗
39. Epperson, J.E., Fürnrohr, P., and Ortiz, C. (1978). The short-range-order structure of α-phase Cu–Al alloys. Acta Crystallogr., Sect. A: Cryst. Phys., Diffr., Theor. Gen. Crystallogr. 34: 667–681, https://doi.org/10.1107/s0567739478001424.10.1107/S0567739478001424 ↗
40. Ferreira, P.J., Robertson, I.M., and Birnbaum, H.K. (1998). Hydrogen effects on the interaction between dislocations. Acta Mater. 46: 1749–1757, https://doi.org/10.1016/s1359-6454(97)00349-2.10.1016/S1359-6454(97)00349-2 ↗
41. Ferreira, P.J., Robertson, I.M., and Birnbaum, H.K. (1999). Hydrogen effects on the character of dislocations in high-purity aluminum. Acta Mater. 47: 2991–2998, https://doi.org/10.1016/s1359-6454(99)00156-1.10.1016/S1359-6454(99)00156-1 ↗
42. Fisher, E.S., Westlake, D.G., and Ockers, S.T. (1975). Effects of hydrogen and oxygen on the elastic moduli of vanadium, niobium, and tantalum single crystals. Phys. Status Solidi A 28: 591–602, https://doi.org/10.1002/pssa.2210280225.10.1002/pssa.2210280225 ↗
43. Fournier, L., Delafosse, D., and Magnin, T. (1999). Cathodic hydrogen embrittlement in alloy 718. Mater. Sci. Eng. A 269: 111–119, https://doi.org/10.1016/s0921-5093(99)00167-7.10.1016/S0921-5093(99)00167-7 ↗
44. Froes, F.H., Senkov, O.N., and Qasi, J.I. (2003). Beneficial effects of hydrogen as a temporary alloying element in titanium alloys: an overview. In: Srivatsan, T.S. and Varin, R.A. (Eds.), Intern symposium on processing and fabrication of advanced materials XI. ASM International, Materials Park, OH, pp. 295–305.
45. Froes, F.H., Senkov, O.N., and Qasi, J.I. (2004). Hydrogen as a temporary alloying element in titanium alloys: thermohydrogen processing. Int. Mater. Rev. 49: 227–245, https://doi.org/10.1179/095066004225010550.10.1179/095066004225010550 ↗
46. Fukai, Y., Ishii, Y., Goto, Y., and Watanabe, K. (2000). Formation of superabundant vacancies in Pd-H alloys. Formation of superabundant vacancies in Pd-H alloys. J. Alloys Compd. 313: 121–132, https://doi.org/10.1016/S0925-8388(00)01195-6.10.1016/S0925-8388(00)01195-6 ↗
47. Fukai, Y., Mori, K., and Shinomiya, H. (2003). The phase diagram and superabundant vacancy formation in Fe-H alloys under high hydrogen pressures. J. Alloys Compd. 348: 105–109, https://doi.org/10.1016/S0925-8388(02)00806-X.10.1016/S0925-8388(02)00806-X ↗
48. Fukai, Y. and Okuma, N. (1993). Evidence of copious vacancy formation in Ni and Pd under a high hydrogen pressure. Jpn. J. Appl. Phys. 32: L1256–L1259, https://doi.org/10.1143/JJAP.32.L1256.10.1143/JJAP.32.L1256 ↗
49. Fukai, Y. and Okuma, N. (1994). Formation of superabundant vacancies in Pd hydride under high hydrogen pressures. Phys. Rev. Lett. 73: 1640–1643, https://doi.org/10.1103/PhysRevLett.73.1640.10.1103/PhysRevLett.73.1640 ↗
50. Fukai, Y., Shizuku, Y., and Kurokawa, Y. (2001). Superabundant vacancy formation in Ni-H alloys. J. Alloys Compd. 329: 195–201, https://doi.org/10.1016/S0925-8388(01)01603-6.10.1016/S0925-8388(01)01603-6 ↗
51. Furukawa, M., Miura, Y., and Nemoto, M. (1985). Strengthening mechanisms in Al-Li alloys containing coherent ordered phases. Trans. Jpn. Inst. Met. 26: 230–235, https://doi.org/10.2320/matertrans1960.26.230.10.2320/matertrans1960.26.230 ↗
52. Gabidullin, R.M., Kolachev, B.A., and Drozdov, P.D. (1971). Estimation of conditions for manifestation of reversible hydrogen brittleness of metals (in Russian). Problems Strength 12: 36–40.10.1007/BF01527704 ↗
53. Garner, F.A. and McCarthy, J.M. (1990). Spinodal-like decomposition of Fe-Ni and Fe-Ni-Cr “invar” alloys during neutron or ion irradiation. In: Russel, K.C. and Smith, D.F. (Eds.), Physical metallurgy of controlled expansion invar-type alloys. TMS-AIME, Warendale, PA, pp. 187–206.
54. Garofalo, F., Chou, Y.T., and Ambegaokar, V. (1960). Effect of hydrogen on stability of microcracks in iron and steel. Acta Metall. 8: 504–512, https://doi.org/10.1016/0001-6160(60)90103-6.10.1016/0001-6160(60)90103-6 ↗
55. Gavriljuk, V., Petrov, Yu., and Shanina, B. (2006). Effect of nitrogen on the electron structure and stacking fault energy in austenitic steels. Scr. Mater. 55: 537–540, https://doi.org/10.1016/j.scriptamat.2006.05.025.10.1016/j.scriptamat.2006.05.025 ↗
56. Gavriljuk, V.G. (1996). Nitrogen in iron and steel. ISIJ Int. 36: 738–745, https://doi.org/10.2355/isijinternational.36.738.10.2355/isijinternational.36.738 ↗
57. Gavriljuk, V.G. and Berns, H. (1999). High nitrogen steels. Springer, Berlin.10.1007/978-3-662-03760-7 ↗
58. Gavriljuk, V.G., Bugaev, V.N., Petrov, Yu.N., Tarasenko, A.V., and Yanchitski, B.Z. (1996a). Hydrogen-induced equilibrium vacancies in fcc iron base alloys. Scr. Mater. 34: 903–907, https://doi.org/10.1016/1359-6462(95)00580-3.10.1016/1359-6462(95)00580-3 ↗
59. Gavriljuk, V.G., Shanina, B.D., Baran, N.P., Maximenko, V.M., Baran, N.P., and Maksimenko, V.M. (1993). Electron-spin-resonance study of electron properties in nitrogen and carbon austenite. Phys. Rev. B 48: 3224–3231, https://doi.org/10.2355/isijinternational.36.738.10.1103/PhysRevB.48.3224 ↗
60. Gavriljuk, V.G., Shanina, B.D., and Berns, H. (2000). On the correlation between electron structure and short-range atomic order in iron-based alloys. Acta Mater. 48: 3879–3893, https://doi.org/10.1016/S1359-6454(00)00192-0.10.1016/S1359-6454(00)00192-0 ↗
61. Gavriljuk, V.G., Shanina, B.D., Shyvanyuk, V.N., and Teus, S.M. (2010). Electronic effect on hydrogen brittleness of austenitic steels. J. Appl. Phys. 108: 083723, https://doi.org/10.1063/1.3499610.10.1063/1.3499610 ↗
62. Gavriljuk, V.G., Shyvaniuk, V.M., and Teus, S.M. (2022). Hydrogen in engineering metallic materials. Springer Nature, Chem, Switzerland.10.1007/978-3-030-98550-9 ↗
63. Gavriljuk, V.G., Sozinov, A.L., Foct, J., Petrov, Yu.N., and Polushkin, Yu.A. (1998). Effect of nitrogen on the temperature dependence of the yield strength of austenitic steels. Acta Mater. 46: 1157–1163, https://doi.org/10.1016/S1359-6454(97)00322-4.10.1016/S1359-6454(97)00322-4 ↗
64. Gavriljuk, V.G., Teus, S.M., Shanina, B.D., and Konchits, A.A. (2017). On the nature of similarity in embrittlement of metals by hydrogen and surfactants. Mater. Sci. Eng. Int. J. 1: 70–79, https://doi.org/10.15406/mseij.2017.01.00013.10.15406/mseij.2017.01.00013 ↗
65. Gavriljuk, V.G., Tyshchenko, A.I., Bliznuk, V.V., Yakovleva, I.L., Riedner, S., and Berns, H. (2008). Cold work hardening of high-strength austenitic steels. Steel Res. Int. 79: 413–422, https://doi.org/10.1002/srin.200806147.10.1002/srin.200806147 ↗
66. Gavriljuk Valentin, G., Shanina Bela, D., Shyvanyuk Vladyslav, N., and Teus Sergey, M. (2013). Hydrogen embrittlement of austenitic steels: electron approach (review article). Corros. Rev. 31: 33–50, https://doi.org/10.1515/corrrev-2013-0024.10.1515/corrrev-2013-0024 ↗
67. Gerberich, W.W., Oriani, R.A., Lji, M.-J., Chen, X., and Foecke, T. (1991). The necessity of both plasticity and brittleness in the fracture thresholds of iron. Philos. Mag. A 63: 363–376, https://doi.org/10.1080/01418619108204854.10.1080/01418619108204854 ↗
68. Gerberich, W.W., Stauffer, D.D., and Sofronis, P. (2009). A coexistent view of hydrogen effects on mechanical behaviour of crystals: HELP and HEDE. In: Somerday, B., Sofronis, P., and Jones, R. (Eds.). Effect of hydrogen on materials. Proc of 2008 intern hydrogen conf. ASM, Jackson, pp. 38–45.
69. Gerold, V. and Karnthaler, H.P. (1989). On the origin of planar slip in f.c.c. alloys. Acta Metall. 37: 2177–2183, https://doi.org/10.1016/0001-6160(89)90143-0.10.1016/0001-6160(89)90143-0 ↗
70. Gibala, R. (1967). Internal friction in hydrogen-charged iron. Trans. Metall. Soc. AIME 239: 1574–1585.
71. Guitar, A., Vigna, G., and Luppo, M.I. (2009). Microstructure and tensile properties after thermohydrogen processing of Ti-6 Al-4V. J. Mech. Behav. Biomed. Mater. 2: 156–163, https://doi.org/10.1016/j.jmbbm.2008.06.002.10.1016/j.jmbbm.2008.06.002 ↗
72. Guzmán, A.A., Jeon, J., Hartmaier, A., and Janisch, R. (2020). Hydrogen embrittlement at cleavage planes and grain boundaries in bcc iron-revisiting the first-principles cohesive zone model. Materials 13: 5785, https://doi.org/10.3390/ma13245785.10.3390/ma13245785 ↗
73. Hancock, G.G. and Johnson, H.H. (1966). Hydrogen, oxygen and subcritical crack growth in a high-strength steel. TMS AIME 236: 513–515.
74. Hänninen, H. and Hakkarainen, T. (1979). Fractographic characteristics of a hydrogen-charged AISI 316 type austenitic stainless steel. Metall. Trans. A 10: 1196–1199, https://doi.org/10.1007/bf02811667.10.1007/BF02811667 ↗
75. Hänninen, H.E. (2003). Stress corrosion cracking. In: Milne, I., Ritchie, R., and Karihaloo, B.L. (Eds.), Comprehensive structural integrity, Vol. 6, pp. 1–29.10.1016/B0-08-043749-4/06133-4 ↗
76. Harris, Z.D., Lawrence, S.K., Medlin, D.L., Guetard, G., Burns, J.T., and Somerday, B.P. (2018). Elucidating the contribution of mobile hydrogen-deformation interactions to hydrogen-induced intergranular cracking in polycrystalline nickel. Acta Mater. 158: 180–192, https://doi.org/10.1016/j.actamat.2018.07.043.10.1016/j.actamat.2018.07.043 ↗
77. Hayashi, E., Kurokawa, Y., and Fukai, Y. (1998). Hydrogen-induced enhancement of interdiffusion in Cu-Ni diffusion couples. Phys. Rev. Lett. 80: 5588–5590, https://doi.org/10.1103/physrevlett.80.5588.10.1103/PhysRevLett.80.5588 ↗
78. Herrera, C., Plaut, C.L., and Padilha, A.F. (2007). Structural dependence of grain boundary energy in Fe-based polycrystals identified by OIM measurements. Mater. Sci. Forum 550: 423–428, https://doi.org/10.4028/www.scientific.net/msf.550.423.10.4028/www.scientific.net/MSF.550.411 ↗
79. Hirth, J.P. and Johnson, H.H. (1976). Hydrogen problems in energy related technology. Corrosion 32: 3–26, https://doi.org/10.5006/0010-9312-32.1.3.10.5006/0010-9312-32.1.3 ↗
80. Hughes, D.A. and Hansen, N. (1991). Microstructural evolution in nickel during rolling and torsion. Mater. Sci. Technol. 7: 544–553, https://doi.org/10.1179/mst.1991.7.6.544.10.1179/026708391790183736 ↗
81. Hwang, C. and Bernstein, I.M. (1986). The effect of strain on hydrogen-induced dislocation morphologies in single crystal iron. Acta Metall. 34: 1011–1020, https://doi.org/10.1016/0001-6160(86)90210-5.10.1016/0001-6160(86)90210-5 ↗
82. Ilyin, A.A., Kollerov, M.Y., Mamonov, A.M., Krastilevsky, A.A., and Makarenkov, D.Y. (1995). Hydrogen influence on martensitic transformation and shape memory effect in titanium alloys. J. Phys. IV 05: 1145–1150, https://doi.org/10.1051/jp4/1995581145.10.1051/jp4/1995581145 ↗
83. Ilyin, A.A., Polkin, S., Mamonov, A.M., and Nosov, V.K. (1995a). In: Blenkinsop, P.A. and Evans, W. J. (Eds.), Titanium 95: science and technology, Vol. 4. The Institute of Materials, London, pp. 2462–2469.
84. Ivasishin, O.M., Anokhin, V.M., Demidik, A.N., and Savvakin, D.G. (2000). Cost-effective blended elemental powder metallurgy of titanium alloys for transportation application. Key Eng. Mater. 188: 55–62, https://doi.org/10.4028/www.scientific.net/KEM.188.55.10.4028/www.scientific.net/KEM.188.55 ↗
85. Ivasishin, O.M. and Moxson, V. (2015). Low cost titanium hydride powder metallurgy. In: Oian, M. and Froes, F.H. (Eds.). Titanium powder metallurgy: science, technology and applications. Elsevier, Oxford, UK, pp. 117–147.10.1016/B978-0-12-800054-0.00008-3 ↗
86. Jiang, D.E. and Carter, E.A. (2004). First principles assessment of ideal fracture energies of materials with mobile impurities: implications for hydrogen embrittlement of metals. Acta Mater. 52: 4801–4807, https://doi.org/10.1016/j.actamat.2004.06.037.10.1016/j.actamat.2004.06.037 ↗
87. Johnson, H.H. (1969). On hydrogen brittleness in high strength steels. In: Staehle, R.W., Forty, A.J., and Van Rooyen, D. (Eds.), Fundamental aspects of stress corrosion cracking. NACE, Houston, USA, pp. 439–444.
88. Kacher, J. and Robertson, I.M. (2014). In situ and tomographic analysis of dislocation/grain boundary interactions in α-titanium. Philos. Mag. 94: 814–829, https://doi.org/10.1080/14786435.2013.868942.10.1080/14786435.2013.868942 ↗
89. Katzarov, I.H. and Paxton, A.T. (2017). Hydrogen embrittlement II. Analysis of hydrogen-enhanced decohesion across (111) planes in α -Fe. Phys. Rev. Mater. 1: 033603, https://doi.org/10.1103/physrevmaterials.1.033603.10.1103/PhysRevMaterials.1.033603 ↗
90. Kerr, W.R. (1985). The effect of hydrogen as a temporary alloying element on the microstructure and tensile properties of Ti-6Al-4V. Metall. Trans. A 16: 1077–1087, https://doi.org/10.1007/bf02811677.10.1007/BF02811677 ↗
91. Kerr, W.R., Smith, P.R., Bidwell, L.R., Rozenblum, M.E., Gurney, F.G., and Mahajan, Y. (1980). Hydrogen as an alloying element in titanium (Hydrovac). In: Kimura, H. and Izumi, O. (Eds.). Proc 4th intern conf on titanium “titanium 80: Science and technologies”, 4. Metallurgical Society of AIME, Warrendale, Pa., Kyoto, pp. 2477–2486.
92. Kikuchi, M., Tanaka, T., and Tanaka, R. (1974). Quenching defects in a nitrogen-containing austenitic stainless steel. Metall. Trans. 5: 1520–1521, https://doi.org/10.1007/BF02646645.10.1007/BF02646645 ↗
93. Kirchheim, R. (2007). Reducing grain boundary, dislocation line and vacancy formation energies by solute segregation II. Experimental evidence and consequences. Acta Mater. 55: 5139–5148, https://doi.org/10.1016/j.actamat.2007.05.033.10.1016/j.actamat.2007.05.033 ↗
94. Kirchheim, R. (2012). Solid solution softening and hardening by mobile solute atoms with special focus on hydrogen. Scr. Mater. 67: 767–770, https://doi.org/10.1016/j.scriptamat.2012.07.022.10.1016/j.scriptamat.2012.07.022 ↗
95. Kolachev, B.A. (1985). Hydrogen brittleness of metals. Metallurgia, Moscow, (in Russian).
96. Kolachev, B.A. (1993). Reversible hydrogen alloying of titanium alloys. Met. Sci. Heat Treat. 35: 586–591, https://doi.org/10.1007/bf00778671.10.1007/BF00778671 ↗
97. Kolachev, B.A., Ilyin, A.A., and Mamonov, A.M. (1991a). Thermohydrogen treatment of titanium alloys (in Russian). In: Metal Science and Treatment of Titanium and Refractory alloys. VILS, Moscow, pp. 131–142.
98. Kolachev, B.A., Malkov, A.V., Nizkin, I.D., Mitin, A.V., and Korostylev, A.F. (1991). On a possibility to decrease temperature of hot upsetting of bolts from VT16 alloy using reversible alloying with hydrogen (in Russian). Metallic 3: 67–69.
99. Kolachev, B.A. and Nosov, V.K. (1984). Hydrogen plastification and superplasticity of titanium alloys (in Russian). Phys. Met. Metallogr. 57: 288–297.
100. Kolachev, B.A., Nosov, V.K., Lyvanov, V.A., Shypunov, G.I., and Chuchuryukin, A.D. (1972). Hydrogen effect on technological plasticity of Ti+9%Al alloy (in Russian). Izvestiya Vusov: Non-Ferrous Metallurgy 4: 137–142.