Electrochemical hydrogen permeation tests under galvanostatic hydrogen charging conditions conventionally used for hydrogen embrittlement study
Source abstract
Abstract
Abstract Electrochemical hydrogen permeation tests using pure Fe sheet specimens were performed under various galvanostatic hydrogen charging conditions commonly applied to tensile test specimens used for evaluation of hydrogen embrittlement property to obtain a guideline for efficient hydrogen charging method for a wide range of hydrogen content. Aqueous NaCl solutions containing varied concentrations of ammonium thiocyanate and a 0.1- m NaOH solution were used as electrolytes for relatively high and low hydrogen content, respectively. Addition of ammonium thiocyanate changes the mechanism of hydrogen evolution reaction and enhances hydrogen entry. By changing the concentration of ammonium thiocyanate and by changing cathodic current density, a wide range of hydrogen content can be covered. The hydrogen content in an AISI 4135 steel estimated from hydrogen permeation current density obtained for a pure Fe specimen was in good agreement with the hydrogen content experimentally measured by hydrogen thermal desorption analysis for the AISI 4135 steel. The hydrogen permeation current density data in various hydrogen charging conditions can be used as a reference for hydrogen charging of specimens.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Reliability Unit, National Institute for Materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan
School of Chemical Engineering and Energy, Zhengzhou University, 100 Science Avenue, Zhengzhou, Henan 450001, China
References (41)
Show source-provided references
1. Akiyama E. Hydrogen thermal desorption analysis for the studies of hydrogen embrittlement of high strength steels. J Vac Soc Jpn 2014; 57: 207–213.10.3131/jvsj2.57.207 ↗
2. Akiyama E, Li S, Shinohara T, Zhang Z, Tsuzaki K. Hydrogen entry into Fe and high strength steels under simulated atmospheric corrosion. Electrochim Acta 2011a; 56: 1799–1805.10.1016/j.electacta.2010.09.043 ↗
3. Akiyama E, Matsukado K, Li S, Tsuzaki K. Constant-load delayed fracture test of atmospherically corroded high strength steels appl. Surf Sci 2011b; 257: 8725–8281.10.1016/j.apsusc.2011.03.037 ↗
4. Bockris JOM, McBreen J, Nanis L. The hydrogen evolution kinetics and hydrogen entry into α-iron. J Electrochem Soc 1965; 112: 1025–1031.10.1149/1.2423335 ↗
5. Bockris JOM, Beck W, Genshaw MA, Subramanyan PK, Williams FS. The effect of stress on the chemical potential of hydrogen in iron and steel. Acta Metall 1971; 19: 1209–1281.10.1016/0001-6160(71)90054-X ↗
6. Chida T, Hagihara Y, Akiyama E, Iwanaga K, Takagi S, Ohishi H, Hayakawa M, Hirakami D, Tarui T. Comparison of constant load, SSRT and CSRT methods for hydrogen embrittlement evaluation using round bar specimens of high strength steels. Tetsu-to-Hagané 2014; 100: 1298–1305.10.2355/tetsutohagane.100.1298 ↗
7. Devanathan MAV, Stachurski Z. The mechanism of hydrogen evolution on iron in acid solutions by determination of permeation rates J. Electrochem Soc 1964; 111: 619–623.10.1149/1.2426195 ↗
8. Devanathan MAV, Stachurski Z, Beck W. A technique for the evaluation of hydrogen embrittlement characteristics of electroplating baths. J Electrochem Soc 1963; 110: 886–890.10.1149/1.2425894 ↗
9. Doshida T, Takai K, Ichiba M. Hydrogen absorption behavior of steel bar for prestressed concrete in a solution of ammonium thiocyanate. Zairyo-to-Kankyo 2012; 61: 249–256.10.3323/jcorr.61.249 ↗
10. Enos DG, Scully JR. A critical-strain criterion for hydrogen embrittlement of cold-drawn, ultrafine pearlitic steel. Metall Mater Trans A 2002; 33A: 1151–1166.10.1007/s11661-002-0217-z ↗
11. Fédération Internationale de la Précontrainte (FIP). Report on prestressing steel. 5. Stress corrosion cracking resistance test for prestressing tendons. Lausanne, Switzerland: FIP, 1980.
12. Finholt AE, Anderson CD, Agre CL. The reduction of isocyanates and isothiocyanates with lithium aluminum hydride. J Org Chem 1953; 18: 1338–1340.10.1021/jo50016a012 ↗
13. Frankel GS, Latanision RM. Hydrogen transport during deformation in nickel: part I. Polycrystalline nickel. Metall Mater Trans A 1986a; 17A: 861–867.10.1007/BF02643862 ↗
14. Frankel GS, Latanision RM. Hydrogen transport during deformation in nickel: part II. Single crystal nickel. Metall Mater Trans A 1986b; 17A: 869–875.10.1007/BF02643863 ↗
15. Hagihara Y, Ito C, Hisamori N, Suzuki H, Takai K, Akiyama E. Evaluation of delayed fracture characteristics of high strength steel based on CSRT method. Tetsu-to-Hagané 2008; 94: 215–221.10.2355/tetsutohagane.94.215 ↗
16. Hagihara Y, Itoh C, Kirikae D, Hisamori N, Suzuki H, Takai K. Probabilistic and statistical evaluation of delayed fracture characteristics obtained by CSRT method. Tetsu-to-Hagané 2009; 95: 489–497.10.2355/tetsutohagane.95.489 ↗
17. Hagihara Y, Shobu T, Hisamori N, Suzuki H, Takai K, Hirai K. Delayed fracture using CSRT method and hydrogen trapping characteristics of V-bearing high strength steel. Tetsu-to-Hagané 2011; 97: 143–151.10.2355/tetsutohagane.97.143 ↗
18. Hagihara Y, Shobu T, Hisamori N, Suzuki H, Takai K, Hirai K. Delayed fracture using CSRT and hydrogen trapping characteristics of V-bearing high-strength steel. ISIJ Int 2012; 52: 298–306.10.2355/isijinternational.52.298 ↗
19. Huang Y, Nakajima A, Nishikata A, Tsuru T. Effect of mechanical deformation on permeation of hydrogen in iron. ISIJ Int 2003; 43: 548–554.10.2355/isijinternational.43.548 ↗
20. Ichiba M, Niidome Y, Nakamura S, Sakai J. Corrosion behavior of prestressing steel in a solution of 20% ammonium thiocyanate. Zairyo-to-Kankyo 2010; 59: 332–334.10.3323/jcorr.59.332 ↗
21. Izutsu K, Takai K, Nagumo M. Effect of cyclic stressing on delayed fracture of high strength steel. Tetsu-to-Hagané 1997; 83: 371–376.10.2355/tetsutohagane1955.83.6_371 ↗
22. Kim SJ, Kim KY. Electrochemical hydrogen permeation measurement through high-strength steel under uniaxial tensile stress in plastic range. Scr Mater 2012; 66: 1069–1072.10.1016/j.scriptamat.2012.03.001 ↗
23. Kushida T. Hydrogen entry into steel by atmospheric corrosion. ISIJ Int 2003; 43: 470–474.10.2355/isijinternational.43.470 ↗
24. Kushida T, Matsumoto H, Kuratomi N, Tsumura T, Nakasato F, Kudo T. Delayed fracture and hydrogen absorption of 1.3GPa grade high strength bolt steel. Tetsu-to-Hagané 1996; 82: 297–302.10.2355/tetsutohagane1955.82.4_297 ↗
25. Li S, Akiyama E, Kimura Y, Tsuzaki K, Uno N, Zhang B. Hydrogen embrittlement property of a 1700 MPa class ultra-high strength tempered martensitic steel. Sci Technol Adv Mater 2010; 11: 025005.10.1088/1468-6996/11/2/025005 ↗
26. Li S, Akiyama E, Shinohara T, Matsuoka K, Oshikawa W. Hydrogen entry behavior into iron and steels under atmospheric corrosion. ISIJ Int 2013; 53: 1062–1069.10.2355/isijinternational.53.1062 ↗
27. Liu Q, Atrens AD, Shi Z, Verbeken K, Atrens A. Determination of the hydrogen fugacity during electrolytic charging of steel. Corros Sci 2014; 87: 239–258.10.1016/j.corsci.2014.06.033 ↗
28. McBreen J, Nonis L, Beck W. A method for determination of the permeation rate of hydrogen through metal membranes. J Electrochem Soc 1966; 113: 1218–1222.10.1149/1.3087209 ↗
29. Nishimura R, Shiraishi D, Maeda Y. Hydrogen permeation and corrosion behavior of high strength steel MCM 430 in cyclic wet-dry SO2 environment. Corros Sci 2004; 46: 225–243.10.1016/S0010-938X(03)00141-0 ↗
30. Nishimura R, Inoue H, Okitsu K, Latanision RM, Hubler GK. Hydrogen permeation behavior in pure nickel implanted with phosphorus, sulphur and their mixture. Corros Sci 2007; 49: 1478–1495.10.1016/j.corsci.2006.08.015 ↗
31. Omura T. Hydrogen entry and its effect on delayed fracture susceptibility of high strength steel bolts under atmospheric corrosion. ISIJ Int 2012; 52: 267–273.10.2355/isijinternational.52.267 ↗
32. Sakashita S, Akiyama E, Tsuzaki K, Takahashi T. Examination of evaluation of maximum hydrogen content in the environment for high strength bolt steel. CAMP-ISIJ 2002; 15: 576.
33. Smialowski M. Hydrogen in steel effect of hydrogen on iron and steel during production, fabrication, and use. Oxford, UK: Pergamon Press, 1962.10.1016/B978-0-08-009697-1.50017-X ↗
34. Takai K, Watanuki R. Hydrogen in trapping states innocuous to environmental degradation of high-strength steels. ISIJ Int 2003; 43: 520–526.10.2355/isijinternational.43.520 ↗
35. Takai K, Murakami K, Yabe N, Suzuki H, Hagihara Y. Properties of thermal hydrogen desorption and substitution of high-pressure gas charging by electrolysis charging for Inconel 625 and SUS 316l. J Jpn Inst Metals 2008; 72: 448–456.10.2320/jinstmet.72.448 ↗
36. Wang MQ, Akiyama E, Tsuzaki K. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel. Mater Sci Eng A 2005a; A398: 37–46.10.1016/j.msea.2005.03.008 ↗
37. Wang MQ, Akiyama E, Tsuzaki K. Hydrogen degradation of a boron-bearing steel with 1050 and 1300MPa strength levels. Scr Mater 2005b; 52: 403–408.10.1016/j.scriptamat.2004.10.023 ↗
38. Wang M, Akiyama E, Tsuzaki K. Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation. Corros Sci 2006; 48: 2189–2202.10.1016/j.corsci.2005.07.010 ↗
39. Wang M, Akiyama E, Tsuzaki K. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test. Corros Sci 2007; 49: 4081–4097.10.1016/j.corsci.2007.03.038 ↗
40. Yamasaki S, Takahashi T. Evaluation method of delayed fracture property of high strength steel. Tetsu-to-Hagané 1997; 83: 454–459.10.2355/tetsutohagane1955.83.7_454 ↗
41. Yoshizawa S, Tsuruta T, Yamakawa K. Development of nickel plating methods in electrochemical measurement of hydrogen content in steel. Corros Eng 1975; 24: 511–515.10.3323/jcorr1974.24.10_511 ↗