Selected Cr(VI) replacement options for aluminum alloys: a literature survey
Source abstract
Abstract
Abstract There is a significant move away from the use of hexavalent chromium, Cr(VI), which is a mature, trusted, and relatively inexpensive treatment that has been used for many years by industry to reduce corrosion. Although Cr(VI) is effective at reducing corrosion, it poses a substantial health hazard. While there is a need to define a process that will be able to replace Cr(VI), the process must be able to provide the same level of corrosion protection currently provided by hexavalent treatments. In addition, it needs to do this without the associated environmental problems. This paper focuses mainly, but not exclusively, on the trivalent chromium pretreatment (TCP) and its commercially available variants. The TCP was developed by the Naval Air Systems Command (NAVAIR) and is used by the US military. The rationale for the focus of this paper is that in the near term, the aeronautics industry needs to move away from Cr(VI) towards a more benign commercially available chemical treatment that can help protect the aluminum alloys used by that industry. TCPs are currently available commercially and have undergone numerous tests by multiple organizations to establish their effectiveness in reducing corrosion of both bare and painted aluminum alloys.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Aluminum Alloy Microstructure Properties · Bauxite Residue and Utilization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Gold Standard Corrosion Science Group, LLC , Greater Boston, MA , USA
Department of Chemical Engineering , Materials and Industrial Production, University of Naples Federico II , Piazzale Tecchio, 80 , 80125 Naples , Italy
Corrosion and Protection Centre, School of Materials , The University of Manchester , Manchester, M139PL , UK
References (61)
Show source-provided references
1. ASTM B117. Standard Practice for Operating Salt Spray (Fog) Apparatus, 2011.
2. ASTM D 1654. Standard Test Method for Evaluation of Painted or Coated Specimens Subjected to Corrosive Environments, 2008.
3. ASTM G85-11. Standard Practice for Modified Salt Spray (Fog) Testing, 2011.
4. Belsanti L, Forchin E, Stifanese R, Toselli M, Traverso P. Characterization of corrosion resistance of chromium-free conversion coatings for aeronautical application. Metall Ital 2016; 108: 37–44.
5. Chen WK, Lee JL, Bai CY, Hou KH, Ger MD. Growth and characteristics of Cr(III)-based conversion coating on aluminum alloy. J Taiwan Inst Chem E 2012; 43: 989–995.10.1016/j.jtice.2012.05.007 ↗
6. Concurrent Technologies Corporation. Chromium alternatives qualification testing. Final, US Air Force Plant (AFP) 44. 2007.
7. Dardona S, Jaworowski M. In situ spectroscopic ellipsometry studies of trivalent chromium coating on aluminum. Appl Phys Lett 2010; 97: 181908.10.1063/1.3511472 ↗
8. Dong X, Wang P, Argekar S, Schaefer DW. Structure and composition of trivalent chromium process (TCP) films on Al alloy. Langmuir 2010; 26: 10833–10841.10.1021/la100699u ↗
9. Dong X, Argekar S, Wang P, Schaefer DW. In situ evolution of trivalent chromium process passive film on Al in a corrosive aqueous environment. ACS Appl Mater Interfaces 2011; 3: 4206–4214.10.1021/am200845v ↗
10. Federal Registry 2006; 71, Number 39: 10099–10385.10.1353/slj.2007.0002 ↗
11. Gaydos S. Evaluation of alternative Cr(VI) surface treatments. SERDP/ESTCP Workshop, 2008.
12. Grilli R, Baker MA, Castle JE, Dunn B, Watts JF. Corrosion behaviour of a 2219 aluminium alloy treated with a chromate conversion coating exposed to a 3.5% NaCl solution. Corros Sci 2011; 53: 1214–1223.10.1016/j.corsci.2010.12.006 ↗
13. Guo Y, Frankel G. Characterization of trivalent chromium process coating on AA2024-T3. Surf Coat Technol 2012a; 206: 3895–3902.10.1016/j.surfcoat.2012.03.046 ↗
14. Guo Y, Frankel GS. Active corrosion inhibition of AA2024-T3 by trivalent chrome process treatment. Corrosion 2012b; 68: 045002-1-045002-10.10.5006/0010-9312-68-4-3 ↗
15. Henkel Surface Technologies Technical Process Bulletin No. 1722 2001.
16. Iyer A, Willis W, Frueh S, Nickerson W, Fowler A, Barnes J, Hagos L, Escarsega J, Scala JL, Suib SL. Characterization of NAVAIR trivalent chromium process (TCP) coatings and solutions. Plat Surf Finish 2010; 5: 32–42.
17. Lane RA, Fink C, Grethlein C. Analysis of alternatives to hexavalent chromium: a program management guide to minimize the use of CrVI in military systems. Rome, NY: Advanced Materials, Manufacturing and Testing Information Analysis Center (AMMTIAC), 2012.
18. Li L, Swain GM. Effects of aging temperature and time on the corrosion protection provided by trivalent chromium process coatings on AA2024-T3. ACS Appl Mater Interfaces 2013; 5: 7923–7930.10.1021/am4020023 ↗
19. Li L, Swain G, Howell A, Woodbury D, Swain G. The formation, structure, electrochemical properties and stability of trivalent chrome process (TCP) coatings on AA2024. J Electrochem Soc 2011; 158: C274–C283.10.1149/1.3607980 ↗
20. Li L, Kim DY, Swain GM. Transient formation of chromate in trivalent chromium process (TCP) coatings on AA2024 as probed by raman spectroscopy. J Electrochem Soc 2012a; 159: C326–C333.10.1149/2.019208jes ↗
21. Li J, Yao C, Liu Y, Li D, Zhou B, Cai W. The hazardous hexavalent chromium formed on trivalent chromium conversion coating: the origin, influence factors and control measures. J Hazard Mater 2012b; 221–222: 56–61.10.1016/j.jhazmat.2012.04.004 ↗
22. Li L, Desouza AL, Swain GM. In situ pH measurement during the formation of conversion coatings on an aluminum alloy AA2024. Analyst 2013a; 138: 4398–4402.10.1039/c3an00663h ↗
23. Li L, Doran KP, Swain GM. Electrochemical characterization of trivalent chromium process (TCP) coatings on aluminum alloys 6061 and 7075. J Electrochem Soc 2013b; 160: C396–401.10.1149/2.117308jes ↗
24. Li L, Whitman BW, Munson CA, Estrda R, Matzdorf CA, Swain GM. Structure and corrosion performance of a non-chromium process (NCP) Zr/Zn pretreatment conversion coating on aluminum alloys. J Electrochem Soc 2016; 163: C718–C728.10.1149/2.0451613jes ↗
25. Material Safety Data Sheet (MSDS) SurTec650. 2007.
26. Matzdorf CA. Risk management approach and progress in Cd and Cr(VI) elimination. ASETS Defense 2014.
27. Matzdorf CA, Nickerson WC. Patent No. 0230215. USA. 2003.
28. Matzdorf C, Kane MJ, Green JL. Patent No. 6375726. USA. 2002.
29. Matzdorf CA, Nickerson WC, Lipnickas E. Evaluation of modified zirconium/trivalent chromium conversion coatings by accelerated corrosion and electrochemical techniques. Tri-Service Corrosion Conference 2005.
30. MIL-DTL-53022. Detail specification primer, epoxy coating, corrosion inhibiting, lead and chromate free. 2010.
31. MIL-DTL-53039. Detail specification – coating, aliphatic polyurethane, single component, chemical agent resistant. 2013.
32. MIL-DTL-5541F. Chemical conversion coatings on aluminum and aluminum alloys. 2006.
33. MIL-DTL-81706. Chemical conversion materials for coating aluminum and aluminum alloys. 2004.
34. MIL-P-53030. Military specification – primer coating, epoxy, water reducible, lead and chromate free. 1992.
35. MIL-PRF-23377J. Performance specification primer coatings: epoxy, high-solids. 2006.
36. MIL-PRF-85285E. Performance specification coating: polyurethane, aircraft and support equipment. 2012.
37. MIL-PRF-85582C. Performance specification – primer coatings: epoxy, waterborne. 1997.
38. MIL-PRF-85582C. Performance specification primer coatings: epoxy, waterborne. 2012.
39. MIL-PRF-85582N. Performance specification – primer coatings: epoxy, waterborne. 2012.
40. Mirovsky Y, Bendov A, Leibovich H, Gerhard M, Rubinstein D. Clean sky: the future of the aviation industry – developments at Israel aerospace industries; 54th Israel Annual Conference on Aerospace Sciences 2014; 3: 1715–1723.
41. Monetta T, Acquesta A, Maresca V, Di Petta P, Lo Masti M. Characterization of aluminum alloys environmentally friendly surface treatments for aircraft and aerospace industry. Surf Interface Anal 2013; 45: 1552–1529.10.1002/sia.5280 ↗
42. Nickerson WC, Lipnickas E. Characterization of a viable non-chromated conversion coating for aluminum and its alloys by electrochemical and other methods. Tri-Service Corrosion Conference 2003.
43. Nickerson W, Matzdorf C. Non-chromate aluminum pretreatments. Final, naval aviation systems command. NAVAIR 2012.10.21236/ADA582070 ↗
44. Official Journal of the European Union, L396/1 30.12.2006 Concerning the Registration, Evaluation, Authorisation and Restriction of Chemicals (REACH).
45. Official Journal of the European Union, L37/19 13.2.2003 On the restriction of the use of certain hazardous substances in electrical and electronic equipment (RoHS).
46. Official Journal of the European Union, L197/38 24.7.2012 on waste electrical and electronic equipment (WEEE).
47. Official Journal of the European Union, L269/34 13.2.2003 On end-of life vehicles (ELV).
48. Palomino LEM, Aoki IV, de Melo HG. Microstructural and electrochemical characterization of Ce conversion layers formed on Al alloy 2024-T3 covered with Cu-rich smut. Electrochim Acta 2006; 51: 5943–5954.10.1016/j.electacta.2006.03.036 ↗
49. Pearlstein F, Agarwala VS. Patent No. 5304257. USA. 1994a.
50. Pearlstein F, Agarwala VS. Trivalent chromium solutions for applying chemical conversion coatings to aluminum alloys or for sealing anodized aluminum. Plat Surf Finish 1994b; 81: 50–55.
51. Pearlstein F, Agarwala VS. Trivalent chromium treatment for aluminum corrosion resistance and paint adhesion. Paper 546 Corrosion 97. NACE. 1997.10.5006/C1997-97546 ↗
52. Placzankis BE, Miller CE, Matzdorf CA. Screening of non chromate conversion coatings on aluminium alloys 2024, 2219, 5083, and 7075. Army Research Laboratory 2003. ARL-TR-2907.
53. Powers M. An investigation of hexavalent-free chromate conversion coatings for test and measurement instrumentation. TMS Suppl Proc 2008; 3: 295–300.
54. Price K. An environmentally friendly chemfilms. Finishing Today 2007; 83: 18–19.
55. Qi J, Thompson GE. Comparative studies of thin film growth on aluminium by AFM, TEM and GDOES characterization. Appl Surf Sci 2016; 377: 109–120.10.1016/j.apsusc.2016.03.115 ↗
56. Qi JT, Hashimoto T, Walton J, Zhou X, Skeldon P, Thompson G. Trivalent chromium conversion coating formation on aluminium. Surf Coat Technol 2015; 280: 317–329.10.1016/j.surfcoat.2015.09.024 ↗
57. Qi J, Hashimoto T, Thompson GE, Carr J. Influence of water immersion post-treatment parameters on trivalent chromium conversion coatings formed on AA2024-T351 alloy. J Electrochem Soc 2016a; 163: C131–C138.10.1149/2.0221605jes ↗
58. Qi J, Hashimoto T, Walton JR, Zhou X, Skeldon P, Thompson GE. Formation of a trivalent chromium conversion coating on AA2024-T351. J Electrochem Soc 2016b; 163: C25–C35.10.1149/2.0771602jes ↗
59. Rochester T, Kennedy ZW. Unexpected results from corrosion testing of trivalent passivates. Plat Surf Finish 2007; 94: 14–18.
60. Safety Data Sheet (SDS) Chemeon TCP-HF. 2016.
61. Suib S, La Scala J, Nickerson W, Fowler A, Zaki N. Determination of hexavalent chromium in NAVAIR trivalent chromium process (TCP) coatings and process solutions. Met Finish 2009; 28–34.10.1016/S0026-0576(09)80028-7 ↗