Abstract CO2 geological utilization and storage (CGUS) is a key technology to achieve carbon neutrality goals. To apply CGUS on a larger scale, the issue of steel corrosion during the process must be addressed to mitigate technological risks. This paper provides an overview of CO2-induced steel corrosion mechanisms and identifies factors that influence corrosion. The impact of CO2 partial pressure, temperature, salinity, pH, impurities, and fluid flow on steel corrosion behavior are also discussed. With the presence of water, the corrosive effect of supercritical CO2 on steel is stronger than that of dissolved CO2 or gaseous CO2. As the temperature increases, the corrosion rate of steel first increases and then decreases. Increasing salinity and decreasing pH lead to an accelerated corrosion rate of steel. Corrosion inhibitors, coatings, and corrosion-resistant alloys are recommended protective measures against CO2-induced corrosion. Compared with coatings, corrosion inhibitors and corrosion-resistant alloys are more commonly used in CGUS projects. Future research directions include further exploration of the mechanisms underlying CO2-induced steel corrosion, clarifying the coupled effects of various environmental factors, and developing corrosion protection technologies under high-pressure and high-concentration CO2 conditions.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · CO2 Sequestration and Geologic Interactions · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Geomechanics and Geotechnical Engineering , 74613 Institute of Rock and Soil Mechanics, Chinese Academy of Sciences , Wuhan , Hubei 430071 , China

University of Chinese Academy of Sciences , Beijing 100049 , China

Southwest Petroleum University , Chengdu , Sichuan 610500 , China

Xi’an University of Technology , Xi’an , Shanxi 710048 , China

Funding

National Natural Science Foundation of China · Key R&D Program of Inner Mongolia Autonomous Region of China · Science and Technology Plan Project of Sichuan Province

References (100+)

Show source-provided references
1. Abd El-Lateef, H.M., Abbasov, V.M., and Aliyeva, L.I. (2013). Inhibition of carbon steel corrosion in CO2-saturated brine using some newly surfactants based on palm oil: experimental and theoretical investigations. Mater. Chem. Phys. 142: 502–512, https://doi.org/10.1016/j.matchemphys.2013.07.044.10.1016/j.matchemphys.2013.07.044 ↗
2. Almeida, T.D., Bandeira, M.C.E., Moreira, R.M., and Mattos, O.R. (2017). New insights on the role of CO2 in the mechanism of carbon steel corrosion. Corros. Sci. 120: 239–250, https://doi.org/10.1016/j.corsci.2017.02.016.10.1016/j.corsci.2017.02.016 ↗
3. Bacca, K.R.G., Lopes, N.F., Santos, B.G., Santos, C.A., and Costa, E.M. (2022). Electrochemical, mechanical, and tribological properties of corrosion product scales formed on X65 steel under CO2 supercritical pressure environments. Surf. Coat. Tech. 446: 128789.10.1016/j.surfcoat.2022.128789 ↗
4. Bachu, S. (2003). Screening and ranking of sedimentary basins for sequestration of CO2 in geological media in response to climate change. Environ. Geol. 44: 277–289, https://doi.org/10.1007/s00254-003-0762-9.10.1007/s00254-003-0762-9 ↗
5. Bachu, S. (2008). CO2 storage in geological media: role, means, status and barriers to deployment. Prog. Energy Combust. Sci. 34: 254–273, https://doi.org/10.1016/j.pecs.2007.10.001.10.1016/j.pecs.2007.10.001 ↗
6. Bai, H.T., Wang, Y.Q., Ma, Y., Zhang, Q.B., and Zhang, N.S. (2018). Effect of CO2 Partial Pressure on the Corrosion Behavior of J55 Carbon Steel in 30% Crude Oil/Brine Mixture. Materials 11: 1765.10.3390/ma11091765 ↗
7. Barker, R., Hua, Y., and Neville, A. (2017). Internal corrosion of carbon steel pipelines for dense-phase CO2 transport in carbon capture and storage (CCS)–a review. Int. Mater. Rev. 62: 1–31, https://doi.org/10.1080/09506608.2016.1176306.10.1080/09506608.2016.1176306 ↗
8. Barros, A., Cruz, C., Garcia, A., and Cheung, N. (2021). Corrosion behavior of an Al–Sn–Zn alloy: Effects of solidification microstructure characteristics. J. Mater. Res. Technol. 12: 257–263.10.1016/j.jmrt.2021.02.081 ↗
9. Biswal, J., Pant, H.J., Sharma, S.C., and Gupta, A.K. (2020). Investigation of effect of an amine inhibitor on corrosion of carbon steel by using thin layer activation technique. J. Radioanal. Nucl. Chem. 323: 1229–1345.10.1007/s10967-019-06710-7 ↗
10. Bockris, J.O.M. and Drazic, D. (1962). The kinetics of deposition and dissolution of iron: effect of alloying impurities. Electrochim. Acta 7: 293–313, https://doi.org/10.1016/0013-4686(62)87007-8.10.1016/0013-4686(62)87007-8 ↗
11. Bockris, J.O.M., Drazic, D., and Despic, A.R. (1961). The electrode kinetics of the deposition and dissolution of iron. Electrochim. Acta 4: 325–361, https://doi.org/10.1016/0013-4686(61)80026-1.10.1016/0013-4686(61)80026-1 ↗
12. Brittan, A., Mahaffey, J., Adam, D., and Anderson, M. (2021). Mechanical and corrosion response of 316SS in supercritical CO2. Oxid. Met. 95: 409–425, https://doi.org/10.1007/s11085-021-10026-x.10.1007/s11085-021-10026-x ↗
13. Brown, B., Parakala, S.R., and Nesic, S. (2004). Proceedings of the CORROSION 2004, March 28–April 1, 2004: CO2 corrosion in the presence of trace amounts of H2S. NACE International, New Orleans, Louisiana.10.5006/C2004-04736 ↗
14. Chang, C.H., Huang, T.C., Peng, C.W., Yeh, T.C., Lu, H.I., Hung, W.I., Weng, C.J., Yang, T.I., and Yeh, J.M. (2012). Novel anticorrosion coatings prepared from polyaniline/graphene composites. Carbon 50: 5044–5051.10.1016/j.carbon.2012.06.043 ↗
15. Chen, C.F., Lu, M.X., Sun, D.B., Zhang, Z.H., and Chang, W. (2005). Effect of chromium on the pitting resistance of oil tube steel in a carbon dioxide corrosion system. Corrosion 61: 594–601, https://doi.org/10.5006/1.3278195.10.5006/1.3278195 ↗
16. Choi, Y.S., Hassani, S., Vu, T.N., Nesic, S., and Abas, A.Z.B. (2016). Effect of H2S on the corrosion behavior of pipeline steels in supercritical and liquid CO2 environments. Corrosion 72: 999–1009.10.5006/2026 ↗
17. Choi, Y.S. and Nesic, S. (2011). Determining the corrosive potential of CO2 transport pipeline in high pCO2-water environments. Int. J. Greenh. Gas Control 5: 788, https://doi.org/10.1016/j.ijggc.2010.11.008.10.1016/j.ijggc.2010.11.008 ↗
18. Cole, I.S., Paterson, D.A., and Corrigan, P. (2012). State of the aqueous phase in liquid and supercritical CO2 as relevant to CCS pipelines. Int. J. Greenh. Gas Control 7: 82–88, https://doi.org/10.1016/j.ijggc.2011.12.008.10.1016/j.ijggc.2011.12.008 ↗
19. Collier, J., Papavinasam, S., Li, J., Shi, C., Liu, P., and Gravel, J.P. (2013). Proceedings of the CORROSION 2013, March 17–21, 2013: effect of impurities on the corrosion performance of steels in supercritical carbon dioxide: optimization of experimental procedure. NACE International, Orlando, Florida.10.5006/C2013-02357 ↗
20. Craig, B.D. and Smith, L. (2011). Corrosion resistant alloys (CRAs) in the oil and gas industry. Nickel Inst. Tech. Ser. 1: 0073.
21. Cui, G., Bi, Z.X., Liu, J.G., Wang, S., and Li, Z.L. (2019). New method for CO2 corrosion resistance Ni-W-Y2O3-ZrO2 nanocomposite coatings. Ceram. Int. 45: 6163–6174.10.1016/j.ceramint.2018.12.093 ↗
22. Cui, L., Kang, W., You, H., Cheng, J.R., and Li, Z. (2021). Experimental study on corrosion of J55 casing steel and N80 tubing steel in high pressure and high temperature solution containing CO2 and NaCl. J. Bio- Tribo-Corrosion 7: 1–14, https://doi.org/10.1007/s40735-020-00449-5.10.1007/s40735-020-00449-5 ↗
23. Cui, G., Yang, Z., Liu, J., and Li, Z. (2019). A comprehensive review of metal corrosion in a supercritical CO2 environment. International Journal of Greenhouse Gas Control 90: 102814.10.1016/j.ijggc.2019.102814 ↗
24. Deng, S., Ling, D.K., Zhou, B.B., Gong, Y., Shen, X., Liu, L., and Zhao, H.J. (2021). pH effect of natural gas hydrate on X80 steel solid–liquid phase scouring corrosion. ACS Omega 6: 3017–3023, https://doi.org/10.1021/acsomega.0c05392.10.1021/acsomega.0c05392 ↗
25. Deng, J.G., Yan, W., Li, X.R., and Dong, X.Q. (2011). Influence of H2S content on CO2 corrosion behaviors of N80 tubing steel. Pet. Sci. Technol. 29: 1387–1396, https://doi.org/10.1080/10916466.2010.545784.10.1080/10916466.2010.545784 ↗
26. Desimone, M.P., Grundmeier, G., and Gordillo, G. (2011). Amphiphilic amido-amine as an effective corrosion inhibitor for mild steel exposed to CO2 saturated solution: polarization, EIS and PM-IRRAS studies. Electrochim. Acta 56: 2990–2998, https://doi.org/10.1016/j.electacta.2011.01.009.10.1016/j.electacta.2011.01.009 ↗
27. Dewaard, C. and Milliams, D.E. (1975). Prediction of carbonic acid corrosion in natural gas pipelines. Ind. Finish. Surf. Coating. 28: 24–26.
28. Ding, C., Gao, K.W., and Chen, C.F. (2009). Effect of Ca2+ on CO2 corrosion properties of X65 pipeline steel. Int. J. Miner. Metall. Mater. 16: 661–666.
29. Dong, B.J., Liu, W., Wu, F., Zhu, J.Q., Wongpat, B., Zhao, Y.G., Fan, Y.M., and Zhang, T.Y. (2020a). Determination of critical salinity of pitting and uniform corrosion of X60 under CO2–O2 coexistence environment. Anti-Corrosion Methods Mater. 67: 166–177, https://doi.org/10.1108/acmm-06-2019-2147.10.1108/ACMM-06-2019-2147 ↗
30. Dong, B.J., Liu, W., Zhang, Y., Banthukul, W., Zhao, Y.G., Zhang, T.Y., Fan, Y.M., and Li, X.G. (2020b). Comparison of the characteristics of corrosion scales covering 3Cr steel and X60 steel in CO2-H2S coexistence environment. J. Nat. Gas Sci. Eng. 80: 103371, https://doi.org/10.1016/j.jngse.2020.103371.10.1016/j.jngse.2020.103371 ↗
31. Dong, B.J., Zeng, D.Z., Yu, Z.M., Cai, L.L., Yu, H.Y., Shi, S.Z., Tian, G., and Yi, Y.G. (2021). Major corrosion influence factors analysis in the production well of CO2 flooding and the optimization of relative anti-corrosion measures. J. Petrol Sci. Eng. 200: 108052, https://doi.org/10.1016/j.petrol.2020.108052.10.1016/j.petrol.2020.108052 ↗
32. Dong, B.J., Zeng, D.Z., Yu, Z.M., Tan, S.Z., Jiang, J.J., Zhang, Q., Cai, S.Z., and Yuan, X. (2019). Effects of heat-stable salts on the corrosion behaviours of 20 steel in the MDEA/H2S/CO2 environment. Corrosion Eng. Sci. Technol. 54: 339–352, https://doi.org/10.1080/1478422x.2019.1591737.10.1080/1478422X.2019.1591737 ↗
33. Duan, Z. and Sun, R. (2003). An improved model calculating CO2 solubility in pure water and aqueous NaCl solutions from 273 to 533 K and from 0 to 2000 bar. Chem. Geol. 193: 257–271, https://doi.org/10.1016/s0009-2541(02)00263-2.10.1016/S0009-2541(02)00263-2 ↗
34. Dugstad, A., Halseid, M., and Morland, B. (2014). Testing of CO2 specifications with respect to corrosion and bulk phase reactions. Energy Proc. 63: 2547–2556, https://doi.org/10.1016/j.egypro.2014.11.277.10.1016/j.egypro.2014.11.277 ↗
35. Farelas, F., Choi, Y.S., and Nesic, S. (2013). Corrosion behavior of API 5L X65 carbon steel under supercritical and liquid carbon dioxide phases in the presence of water and sulfur dioxide. Corrosion 69: 243–250, https://doi.org/10.5006/0739.10.5006/0739 ↗
36. Ferreira, E.S., Giacomelli, C., Giacomelli, F.C., and Spinelli, A. (2004). Evaluation of the inhibitor effect of L-ascorbic acid on the corrosion of mild steel. Mater. Chem. Phys. 83: 129–134, https://doi.org/10.1016/j.matchemphys.2003.09.020.10.1016/j.matchemphys.2003.09.020 ↗
37. Fierro, G., Ingo, G., and Mancia, F. (1990). XPS investigation on AISI 420 stainless steel corrosion in oil and gas well environments. J. Mater. Sci. 25: 1407–1415, https://doi.org/10.1007/bf00585458.10.1007/BF00585458 ↗
38. Firouzdor, V., Sridharan, K., Cao, G., Anderson, M., and Allen, T.R. (2013). Corrosion of a stainless steel and nickel-based alloys in high temperature supercritical carbon dioxide environment. Corros. Sci. 69: 281–291, https://doi.org/10.1016/j.corsci.2012.11.041.10.1016/j.corsci.2012.11.041 ↗
39. Gao, K.W., Yu, F., Pang, X.L., Zhang, G.A., Qiao, L.J., Chu, W.Y., and Lu, M.X. (2008). Mechanical properties of CO2 corrosion product scales and their relationship to corrosion rates. Corros. Sci. 50: 2796, https://doi.org/10.1016/j.corsci.2008.07.016.10.1016/j.corsci.2008.07.016 ↗
40. Gulbrandsen, E. and Bilkova, K. (2006). Proceedings of the CORROSION 2006, March 12–16, 2006: solution chemistry effects on corrosion of carbon steels in presence of CO2 and acetic acid. NACE International, San Diego, California.10.5006/C2006-06364 ↗
41. Halseid, M., Dugstad, A., and Morland, B. (2014). Corrosion and bulk phase reactions in CO2 transport pipelines with impurities: review of recent published studies. Energy Proc. 63: 2557–2569, https://doi.org/10.1016/j.egypro.2014.11.278.10.1016/j.egypro.2014.11.278 ↗
42. Harris, M. (2017). Effects of corrosion inhibitor on the corrosion behavior of low carbon steel in CO2 environment, Ph.D. thesis. US, Ohio, The University of Akron.
43. He, W., Knudsen, O., and Diplas, S. (2009). Corrosion of stainless steel 316L in simulated formation water environment with CO2–H2S–Cl−. Corros. Sci. 51: 2811–2819, https://doi.org/10.1016/j.corsci.2009.08.010.10.1016/j.corsci.2009.08.010 ↗
44. Heusler, K.E. (1958). Der Einfluß der Wasserstoffionenkonzentration auf das elektrochemische Verhalten des aktiven Eisens in sauren Lösungen Der Mechanismus der Reaktion Fe⇌Fe+++ 2e. Zeitschrift für Elektrochemie. Ber. Bunsenges. Phys. Chem. 62: 582–587, https://doi.org/10.1002/bbpc.19580620510.10.1002/bbpc.19580620510 ↗
45. Hua, Y., Barker, R., and Neville, A. (2015a). The effect of O2 content on the corrosion behaviour of X65 and 5Cr in water-containing supercritical CO2 environments. Appl. Surf. Sci. 356: 499–511, https://doi.org/10.1016/j.apsusc.2015.08.116.10.1016/j.apsusc.2015.08.116 ↗
46. Hua, Y., Barker, R., and Neville, A. (2015b). Understanding the influence of SO2 and O2 on the corrosion of carbon steel in water-saturated supercritical CO2. Corrosion 71: 667–683, https://doi.org/10.5006/1504.10.5006/1504 ↗
47. Hua, Y., Jonnalagadda, R., and Zhang, L. (2017). Assessment of general and localized corrosion behavior of X65 and 13Cr steels in water-saturated supercritical CO2 environments with SO2/O2. Int. J. Greenh. Gas Control 64: 126–136, https://doi.org/10.1016/j.ijggc.2017.07.012.10.1016/j.ijggc.2017.07.012 ↗
48. Hua, Y., Mohammed, S., Barker, R., and Neville, A. (2020). Comparisons of corrosion behaviour for X65 and low Cr steels in high pressure CO2-saturated brine. J. Mater. Sci. Technol. 41: 21–32, https://doi.org/10.1016/j.jmst.2019.08.050.10.1016/j.jmst.2019.08.050 ↗
49. Hua, Y., Shamsa, A., and Baarker, R. (2018). Protectiveness, morphology and composition of corrosion products formed on carbon steel in the presence of Cl−, Ca2+ and Mg2+ in high pressure CO2 environments. Appl. Surf. Sci. 455: 667–682, https://doi.org/10.1016/j.apsusc.2018.05.140.10.1016/j.apsusc.2018.05.140 ↗
50. Huang, X.B., Yin, Z.F., Li, H.L., Bai, Z.Q., and Zhao, W.Z. (2012). Corrosion of N80 tubing steel in brine at 1.2 MPa CO2 containing trace amounts of H2S. Corrosion Eng. Sci. Technol. 47: 78–83, https://doi.org/10.1179/1743278211y.0000000019.10.1179/1743278211Y.0000000019 ↗
51. Ilim, I., Bahri, S., Simanjuntak, W., Syah, Y.M., Bundjali, B., and Buchari, B. (2017). Performance of oligomer 4-vinylpiperidine as a carbon dioxide corrosion inhibitor of mild steel. J. Mater. Environ. Sci. 8: 2381–2390.
52. Ingham, B., Ko, M., and Laycock, N. (2012). In situ synchrotron X-ray diffraction study of scale formation during CO2 corrosion of carbon steel in sodium and magnesium chloride solutions. Corros. Sci. 56: 96–104, https://doi.org/10.1016/j.corsci.2011.11.017.10.1016/j.corsci.2011.11.017 ↗
53. IPCC (2021). Climate change 2021: the physical science basis. Contribution of working group I to the sixth assessment report of the intergovernmental panel on climate change. Cambridge University Press, Cambridge, UK and New York, NY, USA.
54. Kahyarian, A. (2018). Mechanism and prediction of mild steel corrosion in aqueous solutions containing carboxylic acids, carbon dioxide, and hydrogen sulfide, Ph.D. thesis. US, Ohio, Ohio University.
55. Kahyarian, A., Brown, B., and Nesic, S. (2017). Electrochemistry of CO2 corrosion of mild steel: effect of CO2 on iron dissolution reaction. Corros. Sci. 129: 146–151, https://doi.org/10.1016/j.corsci.2017.10.005.10.1016/j.corsci.2017.10.005 ↗
56. Kahyarian, A., Brown, B., and Nesic, S. (2020). The unified mechanism of corrosion in aqueous weak acids solutions: a review of the recent developments in mechanistic understandings of mild steel corrosion in the presence of carboxylic acids, carbon dioxide, and hydrogen sulfide. Corrosion 76: 268–278, https://doi.org/10.5006/3474.10.5006/3474 ↗
57. Kahyarian, A. and Nesic, S. (2020). On the mechanism of carbon dioxide corrosion of mild steel: experimental investigation and mathematical modeling at elevated pressures and non-ideal solutions. Corros. Sci. 173: 108719, https://doi.org/10.1016/j.corsci.2020.108719.10.1016/j.corsci.2020.108719 ↗
58. Keddam, M., Mattos, O.R., and Takenouti, H. (1981a). Reaction model for iron dissolution studied by electrode impedance. II. Determination of the reaction model. J. Electrochem. Soc. 128: 266, https://doi.org/10.1149/1.2127402.10.1149/1.2127402 ↗
59. Keddam, M., Mottos, O.R., and Takenouti, H. (1981b). Reaction model for iron dissolution studied by electrode impedance. I. Experimental results and reaction model. J. Electrochem. Soc. 128: 257, https://doi.org/10.1149/1.2127401.10.1149/1.2127401 ↗
60. Kermani, M.B., Gonzales, J.C., and Turconi, G.L. (2003). Proceedings of the CORROSION 2003, March 16–20, 2003: development of superior corrosion resistance 3 % Cr steels for downhole applications. NACE International, San Diego, California.10.5006/C2003-03116 ↗
61. Kim, S.H., Cha, J.H., and Jang, C. (2020). Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650 °C. Corros. Sci. 174: 108843, https://doi.org/10.1016/j.corsci.2020.108843.10.1016/j.corsci.2020.108843 ↗
62. Koguma, K., Ikeda, M., and Kaku, H. (2005). Localized corrosion of MoS2-sputtered films in the atmosphere: measuring the corrosion current in deionized water. Jpn. J. Tribol. 50: 461–470.
63. Li, Z. (2022). Investigation of properties of styrene-acrylic copolymer containing imidazole for protection of HRB400 steel in atmospheric environment. Int. J. Electrochem. Sci. 17: 220419, https://doi.org/10.20964/2022.04.11.10.20964/2022.04.11 ↗
64. Li, W., Brown, B., Young, D., and Nesic, S. (2014). Investigation of pseudo-passivation of mild steel in CO2 corrosion. Corrosion 70: 294–302, https://doi.org/10.5006/0950.10.5006/0950 ↗
65. Li, D., Han, D., Zhang, L., Lu, M., Wang, L., and Ma, W. (2013). Proceeding of the CORROSION 2013, March 17–21, 2013: effects of temperature on CO2 corrosion of tubing and casing steel. NACE International, Orlando, Florida.10.5006/C2013-02426 ↗
66. Li, W., Pots, B.F.M., and Zhong, X.K. (2017). Inhibition of CO2 corrosion of mild steel – study of mechanical effects of highly turbulent disturbed flow. Corros. Sci. 126: 208–226, https://doi.org/10.1016/j.corsci.2017.07.003.10.1016/j.corsci.2017.07.003 ↗
67. Li, Y.Z., Xu, N., Guo, X.P., and Zhang, G.A. (2017). Inhibition effect of imidazoline inhibitor on the crevice corrosion of N80 carbon steel in the CO2-saturated NaCl solution containing acetic acid. Corros. Sci. 126: 127–141, https://doi.org/10.1016/j.corsci.2017.06.021.10.1016/j.corsci.2017.06.021 ↗
68. Li, D.P., Zhang, L., Shi, F.X., Wang, Z., Li, H., and Lu, M.X. (2015). Effect of temperature on the corrosion behavior of 13Cr stainless steel under a high CO2 partial pressure environment. Chinese J. Eng. 37(11): 1463–1468, https://doi.org/10.13374/j.issn2095-9389.2015.11.011.
69. Liu, W., Dou, J.J., Lu, S.L., Zhang, P., and Zhao, Q.H. (2016). Effect of silty sand in formation water on CO2 corrosion behavior of carbon steel. Appl. Surf. Sci. 367: 438–448, https://doi.org/10.1016/j.apsusc.2016.01.228.10.1016/j.apsusc.2016.01.228 ↗
70. Liu, H.W., Gu, T.Y., and Zhang, G.A. (2016a). Corrosion inhibition of carbon steel in CO2-containing oilfield produced water in the presence of iron-oxidizing bacteria and inhibitors. Corros. Sci. 105: 149–160, https://doi.org/10.1016/j.corsci.2016.01.012.10.1016/j.corsci.2016.01.012 ↗
71. Liu, Q.Y., Mao, L.J., and Zhou, S.W. (2014). Effects of chloride content on CO2 corrosion of carbon steel in simulated oil and gas well environments. Corros. Sci. 84: 165, https://doi.org/10.1016/j.corsci.2014.03.025.10.1016/j.corsci.2014.03.025 ↗
72. Liu, Y.C., Zhang, Y.L., Yuan, J.M., Ye, M.J., and Xu, J.Z. (2013). Research on corrosion perforation on pipeline by media of high salinity acidic oil–water mixture. Eng. Fail. Anal. 34: 35–40, https://doi.org/10.1016/j.engfailanal.2013.07.012.10.1016/j.engfailanal.2013.07.012 ↗
73. Lu, Y., Zhang, C., Wang, W., and Zhao, J. (2019). Study of the synergistic effect between corrosion inhibitors by using fractional free volume. Chem. Res. Chin. Univ. 35: 1046–1051.10.1007/s40242-019-9171-9 ↗
74. Muraki, T., Hara, T., and Nose, K. (2002). Proceedings of the CORROSION 2002, April 7–11, 2002: effects of chromium content up to 5 % and dissolved oxygen on CO2 corrosion. NACE International, Denver, Colorado.
75. Muraki, T., Nose, K., and Asahi, H. (2003). Proceedings of the CORROSION 2003, March 16–20, 2003: development of 3 % chromium line pipe steel. San Diego, California.10.5006/C2003-03117 ↗
76. Nesic, S., Postlethwaite, J., and Olsen, S. (1996a). An electrochemical model for prediction of corrosion of mild steel in aqueous carbon dioxide solutions. Corrosion 52: 280–294, https://doi.org/10.5006/1.3293640.10.5006/1.3293640 ↗
77. Nesic, S., Thevenot, N., and Crolet, J.L. (1996b). Proceedings of the CORROSION 96, March 24–29, 1996: electrochemical properties of iron dissolution in the presence of CO2-basics revisited. Denver, Colorado: NACE International.10.5006/C1996-96003 ↗
78. Nesic, S., Wang, S.H., and Cai, J.Y. (2004). Proceedings of the SPE international symposium on oilfield corrosion, May 28, 2004: integrated CO2 corrosion multiphase flow model. Society of Petroleum Engineers, Aberdeen, UK.10.2118/87555-MS ↗
79. Niu, Q.W., Li, Z.L., Cui, G., and Wang, B.Y. (2017). Effect of flow rate on the corrosion behavior of N80 steel in simulated oil field environment containing CO2 and HAc. Int. J. Electrochem. Sci. 12(11): 10279–10290.10.20964/2017.11.23 ↗
80. Olvera-Martinez, M.E., Mendoza-Flores, J., and Genesca, J. (2015). CO2 corrosion control in steel pipelines. Influence of turbulent flow on the performance of corrosion inhibitors. J. Loss Prev. Process Ind. 35: 19–28, https://doi.org/10.1016/j.jlp.2015.03.006.10.1016/j.jlp.2015.03.006 ↗
81. Pal, S., Bhadauria, S.S., and Kumar, P. (2019). Pitting corrosion behavior of F304 stainless steel under the exposure of ferric chloride solution. J. Bio- Tribo-Corrosion 5: 1–13, https://doi.org/10.1007/s40735-019-0283-z.10.1007/s40735-019-0283-z ↗
82. Pessu, F., Barker, R., and Neville, A. (2015). The influence of pH on localized corrosion behavior of X65 carbon steel in CO2-saturated brines. Corrosion 71: 1452–1466, https://doi.org/10.5006/1770.10.5006/1770 ↗
83. Pots, B.F.M. and John, R.C. (2002). Improvement on De Waard-Milliams corrosion prediction and application to corrosion management. NACE International, Houston, US.10.5006/C2002-02235 ↗
84. Qian, S. and Cheng, Y.F. (2019). Synergism of imidazoline and sodium dodecylbenzenesulphonate inhibitors on corrosion inhibition of X52 carbon steel in CO2-saturated chloride solutions. J. Mol. Liq. 294: 111674.10.1016/j.molliq.2019.111674 ↗
85. Remita, E., Tribollet, B., Sutter, E., Vivier, V., Ropital, F., and Kittel, J. (2008). Hydrogen evolution in aqueous solutions containing dissolved CO2: quantitative contribution of the buffering effect. Corros. Sci. 50: 1433–1440, https://doi.org/10.1016/j.corsci.2007.12.007.10.1016/j.corsci.2007.12.007 ↗
86. Ren, X.D., Wang, H., Wei, Q., Lu, Y., Xiao, B.W., and Xie, J. (2021). Electrochemical behaviour of N80 steel in CO2 environment at high temperature and pressure conditions. Corros. Sci. 189: 109619.10.1016/j.corsci.2021.109619 ↗
87. Reyes-Dorantes, E., Zuniga-Diaz, J., and Quinto-Hernandez, A. (2017). Fatty amides from crude rice bran oil as green corrosion inhibitors. J. Chem. 2017: 2871034, https://doi.org/10.1155/2017/2871034.10.1155/2017/2871034 ↗
88. Ruhl, A.S. and Kranzmann, A. (2012). Corrosion behavior of various steels in a continuous flow of carbon dioxide containing impurities. Int. J. Greenh. Gas Control 9: 85–90, https://doi.org/10.1016/j.ijggc.2012.03.005.10.1016/j.ijggc.2012.03.005 ↗
89. Ruhl, A.S. and Kranzmann, A. (2013). Investigation of corrosive effects of sulphur dioxide, oxygen and water vapour on pipeline steels. Int. J. Greenh. Gas Control 13: 9–16, https://doi.org/10.1016/j.ijggc.2012.12.007.10.1016/j.ijggc.2012.12.007 ↗
90. Russick, E.M., Poulter, G.A., Adkins, C.L.J., and Sorensen, N.R. (1996). Corrosive effects of supercritical carbon dioxide and cosolvents on metals. J. Supercrit. Fluids 9: 43, https://doi.org/10.1016/s0896-8446(96)90043-1.10.1016/S0896-8446(96)90043-1 ↗
91. Sæle, A., Graue, A., and Alcorn, Z.P. (2022). Unsteady-state CO2 foam injection for increasing enhanced oil recovery and carbon storage potential. AGER 6: 472–481, https://doi.org/10.46690/ager.2022.06.04.10.46690/ager.2022.06.04 ↗
92. Schmitt, G.A. and Mueller, M. (1999). Proceedings of the CORROSION 99, April 25–30, 1999: critical wall shear stresses in CO2 corrosion of carbon steel. San Antonio, Texas.10.5006/C1999-99044 ↗
93. Schmitt, G.A., Mueller, M., Papenfuss, M., and Strobel-Effertz, E. (1999). Understanding localized corrosion of carbon steel from physical properties of iron carbonate scales. In: Corrosion 99, NACE-99038. NACE International, San Antonio, Texas. https://onepetro.org/NACECORR/proceedings-abstract/CORR99/All-CORR99/NACE-99038/128098.
94. Shi, B.C., Wang, X.W., Zhou, K.L., Xue, K., Liu, K., Zhang, X.K., and Qiu, Y.J. (2023). Study on the corrosion mechanism of N80 steel in simulated oxygen-reduced air drive production wellbores. ACS Omega 8(26): 24016–24022.10.1021/acsomega.3c02869 ↗
95. Singh, A., Ansari, K.R., and Xu, X.H. (2017). An impending inhibitor useful for the oil and gas production industry: weight loss, electrochemical, surface and quantum chemical calculation. Sci. Rep. 7: 1–17, https://doi.org/10.1038/s41598-017-13877-0.10.1038/s41598-017-13877-0 ↗
96. Soeder, D.J. (2021). Greenhouse gas sources and mitigation strategies from a geosciences perspective. Adv. Geo-energy Res. 5: 274–285, https://doi.org/10.46690/ager.2021.03.04.10.46690/ager.2021.03.04 ↗
97. Sridhar, S. and Saadedine, T. (1998). Critical factors in predicting CO2/H2S corrosion in multiphase systems. NACE International, US, Houston.
98. Sun, C., Ding, T.C., Sun, J.B., Lin, X.Q., Zhao, W.M., and Chen, H. (2023). Insights into the effect of H2S on the corrosion behavior of N80 steel in supercritical CO2 environment. J. Mater. Res. Technol. 26: 5462–5477, https://doi.org/10.1016/j.jmrt.2023.08.277.10.1016/j.jmrt.2023.08.277 ↗
99. Sun, C., Sun, J.B., and Wang, Y. (2017). Effect of impurity interaction on the corrosion film characteristics and corrosion morphology evolution of X65 steel in water-saturated supercritical CO2 system. Int. J. Greenh. Gas Control 65: 117–127, https://doi.org/10.1016/j.ijggc.2017.09.002.10.1016/j.ijggc.2017.09.002 ↗
100. Sun, C., Sun, J.B., Wang, Y., Lin, X., Li, X., Cheng, X., and Liu, H. (2016a). Synergistic effect of O2, H2S and SO2 impurities on the corrosion behavior of X65 steel in water-saturated supercritical CO2 system. Corros. Sci. 107: 193–203, https://doi.org/10.1016/j.corsci.2016.02.032.10.1016/j.corsci.2016.02.032 ↗