Abstract In this work, the corrosion-wear synergistic effect for nanocrystalline Fe(Al), 20 wt.% Al 2 O 3 /Fe(Al) composites with and without 4 wt.% Cr in artificial seawater (3.5% NaCl aqueous solution with 60 kg/m 3 quartz sand) was investigated. The results showed that the main damage behavior of Al 2 O 3 /Fe(Al) composites was a corrosive effect because of its poor corrosion resistance and high hardness, whereas for Fe(Al) material, the main damage mode was a chiseling action by solid particles, due to its relatively low hardness. With 4 wt.% Cr addition, the erosion weight loss at different erosion rates decreased by more than 30%. The Al 2 O 3 /Fe(Al) composites had good pure wear resistance, while poor corrosion resistance resulted in an increase in the interaction of corrosion and wear (about 70% of the total damage amount).
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials and Chemical Engineering, Xi’an Technological University, Xi’an 710021, Shaanxi Province, P.R. China

State Key Laboratory for Mechanical Behavior of Materials, School of Materials Science and Engineering, Xi’an Jiaotong University, Xi’an 710049, Shaanxi Province, P.R. China

References (26)

Show source-provided references
1. Andrews P, Illson TF. Erosion-corrosion studies on 13Cr steel in gas well environments by liquid jet impingement. Wear 2000; 233–235: 568–574.10.1016/S0043-1648(99)00228-8 ↗
2. Bai Y, Xing J, Wu H, Liu Z, Gao Y, Ma S. Study on preparation and mechanical properties of Fe3Al–20 wt.%Al2O3 composites. Mater Design 2012; 39: 211–219.10.1016/j.matdes.2012.02.044 ↗
3. Bai Y, Xing J, Liu Z, Gao Y. The microstructure and tribological property of in-situ Fe3Al-Al2O3 composites in argon atmosphere. Intermetallics 2013a; 38: 107–115.10.1016/j.intermet.2013.03.003 ↗
4. Bai Y, Xing J, Wu H, Liu Z, Huang Q, Ma S, Gao Y. The mechanical alloying mechanism of various Fe2O3–Al–Fe systems. Adv Powder Technol 2013b; 24: 373–381.10.1016/j.apt.2012.08.011 ↗
5. Balasubramaniam R. On the role of chromium in minimizing room temperature hydrogen embrittlement in iron aluminides. Scripta Mater 1996; 34: 127–133.10.1016/1359-6462(95)00495-5 ↗
6. Baligidad RG, Radhakrishna A. Effect of alloying additions on structure and mechanical properties of high carbon Fe-16 wt.% Al alloy. Mater Sci Eng A 2000; 287: 17–24.10.1016/S0921-5093(00)00832-7 ↗
7. Barker KC, Ball A. Synergistic abrasive corrosion wear of chromium-containing steels. Brit Corros J 1989; 24: 222–228.10.1179/000705989798270036 ↗
8. Butterfield GR. Transition behavior of saltation: wind tunnel observation of unsteady winds. J Arid Environ 1998; 39: 377–394.10.1006/jare.1997.0367 ↗
9. Huang YD, Yang WY, Chen GL, Sun ZQ. On the effect of the B2 thermomechanical treatment in improving the room temperature ductility of Fe3Al-based alloys. Intermetallics 2001; 9: 331–340.10.1016/S0966-9795(01)00007-3 ↗
10. Kai W, Chang MT, Liu CD, Chiang DL, Chu JP. The high-temperature corrosion of Fe–28Al base alloys containing Cr and Y additions in H2/H2S/H2O mixed gases. Mater Sci Eng A 2002; 329–331: 734–744.10.1016/S0921-5093(01)01519-2 ↗
11. Landolt D, Mischler S, Stemp M. Electrochemical methods in tribocorrosion: a critical appraisal. Electrochim Acta 2001; 46: 3913–3929.10.1016/S0013-4686(01)00679-X ↗
12. Lee D, Kim G, Kim J. The oxidation of Fe3Al-(0, 2, 4, 6%) Cr alloys at 1000°C. Mater Sci Eng A 2003; 339: 109–114.10.1016/S0921-5093(02)00112-0 ↗
13. McKamey CG, Liu CT. Environmental effects on room-temperature ductility and fracture in Fe3Al. Scr Metall Mater 1990; 24: 2119–2122.10.1016/0956-716X(90)90496-4 ↗
14. McKamey CG, DeVan JH, Tortorelli PF, Sikka VK. A review of recent developments in Fe 3 Al-based alloys. J Mater Res 1991; 6: 1779–1805.10.1557/JMR.1991.1779 ↗
15. Palm M, Inden G. Experimental determination of phase equilibria in the Fe-Al-C system. Intermetallics 1995; 3: 443–454.10.1016/0966-9795(95)00003-H ↗
16. Parionaa MM, Teleginskia V, Santosa K,de Lima AAOC, Zara AJ, Micene KT, Riva R. Influence of laser surface treated on the characterization and corrosion behavior of Al–Fe aerospace alloys. Appl Sure S 2013; 276: 76–85.10.1016/j.apsusc.2013.03.025 ↗
17. Peng FQ. Practical handbook of metallic materials. Beijing: China Machine Press, 1987: 128–132 (in Chinese).
18. Qian DS, Zhong XL, Hashimoto T, Yan YZ, Liu Z. Effect of excimer laser surface melting on the corrosion performance of a SiCp/Al metal matrix composite. Appl Sure S 2015; 330: 280–291.10.1016/j.apsusc.2014.12.132 ↗
19. Schonfeldt HJ, Lowis S. Turbulence driven saltation in the atmospheric surface layer. Meteorol Z 2003; 12: 257–268.10.1127/0941-2948/2003/0012-0257 ↗
20. Sharma G, Sundararaman M, Prabhu N, Goswami GL. Sliding wear resistance of iron aluminides. Bull Mater Sci 2003; 26: 311–314.10.1007/BF02707452 ↗
21. Sterk G, Jacob AFG, Van JH. Effect of turbulent flow structures on saltation sand transport in the atmospheric boundary layer. Earth Surf Proc Land 1998; 23: 877–887.10.1002/(SICI)1096-9837(199810)23:10<877::AID-ESP905>3.3.CO;2-I ↗
22. Tao S, Li DY. Investigation of corrosion–wear synergistic attack on nanocrystalline Cu deposits. Wear 2007; 263: 363–370.10.1016/j.wear.2007.01.056 ↗
23. Yang J, La PQ, Liu WM, Hao Y. Microstructure and properties of Fe3Al–Fe3AlC0.5 composites prepared by self-propagating high temperature synthesis casting. Mater Sci Eng A 2004; 382: 8–14.10.1016/j.msea.2004.03.095 ↗
24. Zhang XH, Yang J, Ma JQ, Bi Q, Cheng J, Liang Y, Liu W. Microstructures and mechanical properties of Fe28Al5Cr/TiC composites produced by hot-pressing sintering. Mater Sci Eng A 2011; 528: 6819–6824.10.1016/j.msea.2011.05.063 ↗
25. Zhu SY, Bi QL, Yang J, Liu W. Influence of Cr content on tribological properties of Ni3Al matrix high temperature self-lubricating composites. Tribol Int 2011; 44: 1182–1187.10.1016/j.triboint.2011.05.014 ↗
26. Ziomek-Moroz M, Miller A, Hawk J, Cadien K, Li DY. An overview of corrosion–wear interaction for planarizing metallic thin films. Wear 2003; 255: 869–874.10.1016/S0043-1648(03)00225-4 ↗