Pitting initiation on 304 stainless steel in a chloride-contaminated pore solution under alternating temperature conditions
Source abstract
Abstract
Abstract Pitting initiation on 304 stainless steel grades was investigated in alternating temperature pore solutions to simulate pitting on stainless steel rebar in a tropical marine environment. The results suggested that a larger amplitude of alternating temperature heavily doped the passive film, reduced the film’s thickness and increased the (Fe 3+ ox + Fe 3+ hy)/Fe 2+ ox and Cr 3+ hy/Cr 3+ ox ratios in the film. Alternating temperatures more significantly degraded the passive film and intensified the pitting sensitivity on the stainless steel when compared with the average temperatures of the alternating temperature cycles. More pitting initiation sites were observed on the samples that experienced the 22–60 °C and 22–70 °C alternating temperature cycles than their counterparts in 50 °C and 60 °C solutions, respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.