journal article·2001-03

The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions

Geneviève Baril, Nadine Pébère

Corrosion Science· Volume 43· Issue 3
Publisher page

Abstract

Abstract The corrosion behaviour of pure magnesium in aerated and deaerated Na 2 SO 4 solutions (0.01 and 0.1 M) was investigated by steady-state current–voltage curves and electrochemical impedance measurements with a rotating disc electrode. It was shown that the anodic current densities were lower and the resistance values higher in deaerated media. It was demonstrated that the absence of HCO 3 − due to the absence of CO 2 , which is always present in the natural environment was responsible for the results observed. The magnesium surface was covered with a porous film (MgO, Mg(OH) 2 ) which became thicker with time. The protection afforded by the layer was low and the corrosion rate remained constant as the immersion time increased. In addition, experiments carried out at different NaHCO 3 concentrations in deaerated media revealed that the corrosion rate of magnesium was accelerated when the NaHCO 3 concentration increased due to dissolution of the film (MgO, Mg(OH) 2 ). It was concluded that O 2 did not influence magnesium corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Magnesium Alloys: Properties and Applications · Magnesium Oxide Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Dolet · Matériaux et Techniques · 1997 · 7–8 · 310.1051/mattech/199785070003 ↗
2. Gulbrandsen · Electrochim. Acta · 1992 · 37 · 140310.1016/0013-4686(92)87014-Q ↗
3. Gulbrandsen · Corros. Sci. · 1993 · 34 · 142310.1016/0010-938X(93)90238-C ↗
4. Udhayan · J. Power Sources · 1996 · 63 · 10310.1016/S0378-7753(96)02456-1 ↗
5. Song · Corros. Sci. · 1997 · 39 · 85510.1016/S0010-938X(96)00172-2 ↗
6. Song · Corros. Sci. · 1997 · 39 · 198110.1016/S0010-938X(97)00090-5 ↗
7. Nordlien · J. Electrochem. Soc. · 1995 · 142 · 332010.1149/1.2049981 ↗
8. Hallopeau · Corros. Rev. · 1998 · 16 · 2710.1515/CORRREV.1998.16.1-2.27 ↗
9. Bedjoudi · Corrosion · 1993 · 49 · 73810.5006/1.3316126 ↗
10. Pébère · Electrochim. Acta · 1990 · 35 · 55510.1016/0013-4686(90)87043-2 ↗
11. Perrault · J. Electroanal. Chem. · 1974 · 51 · 10710.1016/S0022-0728(74)80298-6 ↗
12. Petty · J. Am. Chem. Soc. · 1954 · 76 · 36310.1021/ja01631a013 ↗
13. Robinson · J. Electrochem. Soc. · 1954 · 108 · 3610.1149/1.2428007 ↗
14. Thoma · Metalloberfläche · 1984 · 38 · 393
15. Ch. Brun, J. Pagetti, J. Talbot, Mémoires Scientifiques Revue Métallurgie 10 (1976) 659
16. W.L. Loose, in: H.H. Uhlig (Ed.), The Corrosion Handbook, John Wiley & Sons Inc., New York, 1966, p. 218
17. G. Baril, N. Pébère, in: M. Elboujdaini, E. Ghali (Eds.), Proceedings of the International Symposium on Environmental Degradation of Materials and Corrosion Control in Metals, 1999, p. 55
18. Gabrielli · Electrochim. Acta · 1974 · 19 · 35510.1016/0013-4686(74)87009-X ↗
19. You · Corros. Sci. · 1993 · 34 · 510.1016/0010-938X(93)90254-E ↗
20. Deslouis · J. Electroanal. Chem. · 1984 · 181 · 11910.1016/0368-1874(84)83624-2 ↗
21. Levich · 1962
22. Epelboin · Electrochim. Acta · 1975 · 22 · 91310.1016/0013-4686(75)87017-4 ↗
23. Vermilyea · J. Electrochem. Soc. · 1969 · 116 · 148710.1149/1.2411579 ↗
24. Gabrielli · Corros. Sci. · 1996 · 26 · 1125
25. M. Pourbaix, Atlas d’équilibres électrochimiques, Ed. Gauthier-Villas, Paris, 1963, p. 449
26. F.J. Dougherty, A.A. Gallaccio, US Air Force Syst. Command, Air Force Mater. Lab., Techn. Rep., AFML (1975), AFML-TR-75-42, Proc. Triservice Corros. Mil. Equip. Conf., vol. 1, ADA021053, 1974, pp. 211–235